Stainless hlau 316L: Tsawg-Carbon Qib nrog Superior Corrosion Resistance

Dec 02, 2025

Tso lus

316L Stainless hlau yog dab tsi?

316L yog molybdenum{1}}cov kabmob austenitic stainless hlau nrog cov ntsiab lus carbon txwv rau 0.030% siab tshaj plaws. L lub npe sawv cev rau cov pa roj carbon tsawg. Qhov sib ntxiv ntawm molybdenum ntawm 2.0-3.0% muab cov qib zoo dua rau pitting thiab crevice corrosion nyob rau hauv chloride ib puag ncig tshaj 304 tsev neeg, thaum cov ntsiab lus tsis tshua muaj carbon khaws cia qhov kev tiv thaiv tom qab vuam los ntawm kev tiv thaiv chromium carbide nag lossis daus ntawm cov ciam teb.

Qib tau raug xaiv UNS S31603 hauv Asmeskas system, 1.4404 (X2CrNiMo17-12-2) hauv EN 10088, SUS316L hauv JIS, thiab 022Cr17Ni12Mo2 hauv Suav GB system. Nws yog them los ntawm ASTM A240 rau phaj, ntawv thiab sawb, A312 / A213 / A269 rau yeeb nkab thiab raj, thiab A276 rau bar.

Tshuaj muaj pes tsawg leeg (ASTM A240)

Element C Mn P S Si Cr Ni Mo N
Cov ntsiab lus,% 0.030 max max 2.00 Nws 0.045 max 0.030 max 0.75 max 16.0-18.0 10.0-14.0 2.00-3.00 0.10 max

Mechanical Properties (ASTM A240, Annealed)

Khoom Kev xav tau
Tensile zog Rm 485 MPa min
0.2% yield zog Rp0.2 170 MPa min
Elongation nyob rau hauv 50 mm 40% min
Hardness 217 HB / 95 HRB max

Corrosion Resistance

316L muaj kev tiv thaiv zoo heev rau ntau yam ntawm corrosive media:

Chloride-cov kabmob ib puag ncig, qhov twg cov ntsiab lus molybdenum nce pitting kuj sib npaug tus lej (PREN) txog li 24, piv rau 18-19 rau 304L.

Intergranular corrosion tom qab vuam, tshem tawm los ntawm 0.030% siab tshaj cov ntsiab lus carbon.

Organic acids, khoom noj khoom haus, tshuaj, thiab ntau dilute mineral acids nyob rau hauv nruab nrab kub.

Kev ntxhov siab corrosion tawg hauv kev pabcuam chloride, zoo dua li 304 tab sis tsis tiv thaiv kab mob; rau kev nkag mus rau hauv dej hiav txwv loj, siab dua - qib alloy raug pom zoo.

Weldability thiab Fabrication

316L welds tau yooj yim los ntawm tag nrho cov txheej txheem ib txwm siv, suav nrog GTAW, GMAW, SMAW thiab SAW, siv cov hlau sib txuam xws li ER316L. Vim tias cov ntsiab lus tsis tshua muaj carbon tsawg, cov pob qij txha welded khaws tag nrho cov kev tiv thaiv corrosion yam tsis muaj kev tshaj tawm -weld kho cua sov, uas yog qhov kev txiav txim siab zoo hauv cov ntaub ntawv loj xws li cov tso tsheb hlau luam, cov kav dej thiab cov txheej txheem nkoj. Cov qib kuj tseem tsim tau zoo, nrog rau kev ua kom zoo rau kev sib sib zog nqus nqus, khoov thiab dov, thiab nws tuaj yeem ua haujlwm, txawm tias nws ua haujlwm - hardens sai dua carbon steel.

Kev kho mob thiab siab -Purity Applications

Rau cov khoom siv kho mob cog tau, lub tshuab nqus tsev tshwj xeeb-melted version hu ua 316LVM (lub tshuab nqus tsev qis) yog siv, teev nyob rau hauv ASTM F138 thiab ISO 5832-1. Cov khoom siv no muaj qhov huv huv microstructure thiab kev txwv nruj dua li tus qauv 316L, thiab cov khoom tsim los ntawm nws raug soj ntsuam rau biocompatibility raws li ISO 10993 series. Hauv cov chaw muag tshuaj thiab cov khoom siv semiconductor, 316L nrog electropolished lossis mechanically polished nto yog cov khoom siv rau cov kav dej siab huv vim tias nws yooj yim los ntxuav, tsis nqus cov pa paug, thiab tsis ua rau cov hlau ions nkag mus rau hauv cov khoom ntws.

Tej kev siv

Cov khoom siv tshuaj thiab petrochemical txheej txheem thiab kav dej.

Pharmaceutical, biotechnology thiab khoom noj khoom haus.

Marine structures, ntug hiav txwv architecture thiab nkoj fittings.

Thaum tshav kub kub exchangers, condensers thiab dej txias tshuab.

Medical implants (316LVM) thiab cov cuab yeej phais.

Semiconductor thiab ultra{0}} cov dej ntshiab huv.

Cryogenic cia thiab thauj cov roj liquefied.

Cov lus nug nquag

Q1. Dab tsi yog intergranular corrosion thiab yog vim li cas 316L tiv nws?

Intergranular corrosion tawm tsam cov ciaj ciam ntawm cov hlau tsis muaj steel tom qab vuam lossis siab - qhov kub thiab txias, tshwm sim los ntawm chromium carbides precipitating ntawm ciam teb thiab depleting chromium nyob ib sab. Cov ntsiab lus carbon tsawg ntawm 316L (0.030% siab tshaj) txo qis kev tsim cov carbide, khaws cia cov zaj duab xis passive thoob plaws tag nrho cov qauv, yog li cov pob qij txha welded khaws lawv cov corrosion tsis kam tom qab-weld annealing.

Q2. 316L puas tuaj yeem siv rau kev cog ntoo?

Yog lawm. Implant-qib 316L, hu ua 316LVM, tau teev nyob rau hauv ASTM F138 thiab ISO 5832-1 thiab yog siv rau orthopedic screws, phaj thiab lwm yam khoom siv. Nws cov kev tiv thaiv corrosion, biocompatibility thiab ductility raug txheeb xyuas rau kev cog qoob loo mus sij hawm ntev, thiab cov cuab yeej raug soj ntsuam raws li ISO 10993 kev ntsuam xyuas kab mob lom.

Q3. 316L coj li cas ntawm qhov kub thiab txias?

316L khaws nws cov ductility thiab toughness mus txog -196 degrees Celsius vim nws ruaj khov austenitic qauv. Nws yog cov khoom siv txheem rau LNG cia tso tsheb hlau luam, cov kav dej cryogenic thiab cov khoom siv hauv aerospace, thiab tsis raug kev puas tsuaj uas cuam tshuam rau ferritic lossis martensitic steels ntawm qhov kub thiab txias.

Q4. Qhov txawv ntawm 316 thiab 316L yog dab tsi?

Cov ntsiab lus carbon: 316 tso cai rau 0.08%, thaum 316L txwv rau 0.030%. Nyob rau hauv lub annealed mob, mechanical zog yuav luag zoo tib yam. Qhov txawv tshwm sim tom qab welding, qhov twg 316L zam rhiab heev thiab intergranular corrosion yam tsis muaj post-weld heat treatment.

Q5. Puas yog 316L haum rau dej hiav txwv?

316L yog qhov tsim nyog rau cov huab cua me me hauv hiav txwv, thaj chaw txaws thiab qis - dej hiav txwv nrawm ntawm qhov kub thiab txias. Rau immersion mus tas li, creviced lossis stagnant, los yog dej hiav txwv sov, pitting thiab crevice corrosion tuaj yeem tshwm sim, thiab 6% molybdenum super- qib austenitic lossis duplex yog ib txwm teev.

Q6. Vim li cas molybdenum ntxiv rau 316L?

Molybdenum txhim khu kev tiv thaiv rau pitting thiab crevice corrosion nyob rau hauv chloride media thiab tsub kom lub zog ntawm siab kub. 2.0-3.0% molybdenum cov ntsiab lus yog lub ntsiab yog vim li cas 316L outperforms 304L nyob rau hauv marine, tshuaj thiab kws tshuaj.

Xa kev nug