Puas yog Stainless Hlau 304 lossis 316 rau zaub mov?

Dec 17, 2025

Tso lus

 
Puas yog Stainless Hlau 304 lossis 316 rau zaub mov?
Is Stainless Steel 304 or 316 for food
01

Puas yog Stainless Hlau 304 lossis 316 rau zaub mov?

Ob leeg 304 thiab 316 stainless hlau yog cov khoom noj- qib cov ntaub ntawv thiab muaj kev nyab xeeb rau kev sib cuag nrog zaub mov. 304 stainless hlau yog cov qauv kev lag luam rau feem ntau cov khoom noj txhua hnub, xws li cookware thiab zaub mov npaj nto, muab kev tiv thaiv corrosion zoo heev thiab tus nqi -effectiveness. 316 stainless hlau, vim qhov sib ntxiv ntawm molybdenum, ua tau zoo dua hauv sh ib puag ncig, tshwj xeeb tshaj yog cov uas muaj chlorides (ntsev) los yog cov tshuaj muaj zog, ua rau nws zoo tagnrho rau kev siv cov khoom siv marine lossis tshuaj lom neeg. Feem ntau, 304 stainless hlau yog ib qho kev xaiv tsim nyog, tab sis rau cov kev xav tau uas xav tau ntau dua corrosion kuj, 316 stainless hlau yuav tsum tau xaiv.

02

Dab tsi yog qhov tsis zoo ntawm 316 stainless hlau?

Lub ntsiab qhov tsis zoo ntawm 316 stainless hlau suav nrog nws cov nqi siab dua (vim muaj molybdenum thiab npib tsib xee), siab toughness thiab susceptibility mus ua hauj lwm hardening, uas ua rau machining nyuaj, nce susceptibility rau hnav thiab galling, thiab lub peev xwm rau weld corrosion (sensitization) yog welded tsis raug. Nws tsis yog- cov khoom sib nqus kuj txwv nws txoj kev siv hauv kev siv hlau nplaum. Zuag qhia tag nrho, 316 stainless hlau yog cov khoom siv siab- zoo, yog li nws qhov tsis zoo feem ntau yog nyob rau hauv cov nqi thiab kev ua haujlwm nyuaj piv rau qib zoo li 304 stainless hlau.

316 Stainless Steel
 

304 Stainless hlau (Standard Qib)
Cov txiaj ntsig zoo: Kev tiv thaiv corrosion zoo heev rau oxidizing acids, yooj yim los ntxuav, zoo formability, thiab nqi - zoo.
Kev siv zoo tshaj plaws: Cov khoom siv hauv chav ua noj, rooj ua zaub mov, cookware, ntim dej haus, thiab khoom siv hauv tsev noj mov.

 

316 Stainless hlau (qib kho dua tshiab)
Qhov zoo: Vim muaj qhov sib ntxiv ntawm molybdenum, nws muaj kev tiv thaiv corrosion zoo tshaj rau chlorides (ntsev), alkalis, thiab acids.
Kev siv zoo tshaj plaws: Ib puag ncig hnyav, kev siv dej hiav txwv, chav ua noj ua haus raug ntsev, siab -kev ua kom huv, thiab kev ua tshuaj lom neeg.

 

Cov tshuaj muaj pes tsawg leeg ntawm 304 stainless hlau thiab 316 stainless hlau

Element Khoom noj khoom haus-Qib Stainless Hlau 304 Khoom noj khoom haus-Qib Stainless Hlau 316
Chromium (Cr) 18.0 – 20.0 % 16.0 – 18.0 %
Nickel (Ni) 8.0 – 10.5 % 10.0 – 14.0 %
Molybdenum (hli) Tsawg dua lossis sib npaug li 0.75% (tsis txhob txwm ntxiv) 2.0 – 3.0 %
Cov pa roj carbon (C) Tsawg dua lossis sib npaug li 0.08% Tsawg dua lossis sib npaug li 0.08%
Manganese (Mn) Tsawg dua lossis sib npaug li 2.0% Tsawg dua lossis sib npaug li 2.0%
Silicon (Si) Tsawg dua lossis sib npaug li 1.0% Tsawg dua lossis sib npaug li 1.0%
Phosphorus (P) Tsawg dua lossis sib npaug li 0.045% Tsawg dua lossis sib npaug li 0.045%
Sulfur (S) Tsawg dua lossis sib npaug li 0.030% Tsawg dua lossis sib npaug li 0.030%
Nitrogen (N) Tsawg dua lossis sib npaug li 0.10% Tsawg dua lossis sib npaug li 0.10%
Hlau (Fe) Tshuav Tshuav

 

316 vs 304 Stainless Hlau Mechanical Properties

Mechanical Property 304 Stainless hlau 316 Stainless hlau
Tensile zog (MPa) 500-700 MPa 400-620 MPa
Elongation A50 hli (%) 45% min 45% min
Hardness (Brinell, HB) 215 Max HB 149 Max HB

 

Yuav xaiv li cas
Rau feem ntau cov chav ua noj hauv tsev thiab cov qauv kev lag luam siv: 304 stainless hlau yog zoo kawg nkaus txaus thiab pheej yig dua.
Rau cov ntug hiav txwv dej, ib puag ncig marine, los yog cov chaw ua khoom noj khoom haus uas siv cov ntsev / tshuaj ntau ntau: 316 stainless hlau muab lub neej ua haujlwm ntev thiab tiv thaiv pitting corrosion.

 

Corrosion Resistance ntawm 304 Stainless Hlau vs . 316 Stainless Hlau
304 qib stainless hlau yog feem ntau siv hom stainless hlau thoob ntiaj teb.
Nws muaj qhov zoo ntawm cov hlau tsis muaj steel, nrog rau kev tiv thaiv corrosion, formability, lub zog, thiab yooj yim ntawm kev txij nkawm.
Ntawm qhov tod tes, thaum 316 qib stainless hlau tsis yog feem ntau siv raws li 304 stainless hlau, nws cov corrosion kuj yog qhov zoo tshaj rau 304 stainless hlau, tshwj xeeb tshaj yog nyob rau hauv chlorides thiab acids. Yog li, 316 stainless hlau yog qhov kev xaiv zoo tshaj plaws rau cov ntawv thov uas xav tau kev sib cuag nrog cov tshuaj corrosive lossis ib puag ncig hnyav xws li dej hiav txwv.

 

Thaum tshav kub kub Resistance ntawm 304 Stainless hlau vs . 316 Stainless hlau
Thaum muab piv rau cov cua sov ntawm 304 thiab 316 stainless hlau, nws yog ib qho tseem ceeb kom nco ntsoov tias ob hom stainless hlau muaj oxidation zoo nyob rau hauv tej yam kev mob kub.
304 stainless hlau: Muaj qhov zoo siab - kub tsis kam, tab sis kev siv txuas ntxiv hauv qhov kub ntawm 425-860℃(797-1580℃F) tuaj yeem ua rau corrosion.
316 stainless hlau: Ua tau zoo tshaj plaws ntawm qhov kub siab tshaj 843℃(1550℃F) thiab qis dua 454℃(850℃F). Muab piv rau 304 stainless hlau, nws pom zoo corrosion kuj nyob rau hauv siab - kub ib puag ncig.

 

Vim li cas thiaj xaiv Gnee Stainless Hlau (Siv tus qauv piv txwv)?

✅ Cov khoom loj ntawm stainless hlau kav / tuav / phaj / fittings / coils muaj rau xa khoom sai.

✅ Hoobkas ncaj muag khoom, tus nqi sib tw heev, tus nqi zoo rau cov nyiaj.

✅ Kev lees paub zoo: Cov Khoom Siv Xeem Ntawv Pov Thawj (MTC), cov ntawv pov thawj tshuaj muaj pes tsawg leeg, thiab daim ntawv pov thawj khoom vaj khoom tsev muab.

✅ Tus nqi - ntxiv cov kev pabcuam: Slitting, txiav, polishing, thiab kho qhov chaw.

✅ Kev xa khoom thoob ntiaj teb nrog kev ntim khoom nyab xeeb thiab txhim khu kev qha, thiab tag nrho cov ntaub ntawv xa tawm tsim nyog tau muab.

Email:sales@gneestainless.com

Xa kev nug