Puas yog 316L stainless hlau austenitic lossis martensitic?

Dec 10, 2025

Tso lus

What is stainless steel metal?410vs420 stainless steel316Ti vs 316L Stainless Steel: Choosing Between Stabilization and Low Carbon

316L stainless hlau yog ib qho tseem ceebausteniticstainless hlau, paub txog nws lub ntsej muag -centered cubic qauv, tsis yog- cov khoom sib nqus (hauv lub xeev annealed), zoo heev corrosion kuj (vim Molybdenum), thiab zoo formability, tab sis nws muaj peev xwm hloov mus rau hauv martensite nyob rau hauv mob khaub thuas ua hauj lwm, nce magnetism thiab hardness.

 

Austenitic:Nws cov qauv tseem ceeb yog austenite, ua rau nws ductile thiab tsis yog -magnetic.

Cov pa roj carbon tsawg (L):'L' qhia txog cov ntsiab lus ntawm cov pa roj carbon tsawg, txhim kho weldability thiab tiv thaiv rhiab heev (carbide nag lossis daus).

Molybdenum Cov ntsiab lus:Ntxiv rau kev tiv thaiv zoo tshaj rau cov tshuaj chlorides thiab pitting corrosion, ua rau nws "qib marine".