EN 10216-5 1.4841 Stainless Hlau Seamless Boiler Tube
Nov 06, 2025
Tso lus
TS EN 10216-5 siv rau cov kav dej seamless uas ua los ntawm austenitic stainless hlau (xws li creep-cov hlau tsis muaj zog) thiab duplex stainless hlau. Cov kav dej no feem ntau yog siv rau hauv cov hlab ntsha siab thiab cov ntawv thov uas xav tau kev tiv thaiv corrosion siab. 1.4841 stainless hlau seamless yeeb nkab (tso ntawv pov thawj rau CE, DNV, PED, TÜV, thiab EN 10216-5) yog qhov kub-kub austenitic stainless hlau ua raws li European tus qauv EN 10216-5, siv rau kev tsim seamless kav.
GNEE cov1.4841 seamless stainless hlau yeeb nkabs yog cov cua sov- thiab siab-kub{2}} cov kav dej tiv taus ua los ntawm EN 310 qib stainless hlau (tseem hu ua AISI 310 lossis UNS S31000). Lawv tau tsim los siv cov txheej txheem kub thiab txias, nrog rau kev kho cua sov rau descaling thiab ci annealing. Sab hauv thiab sab nrauv tiav ntawm cov kav dej ua tau raws li qhov yuav tsum tau ua ntawm cov txheej txheem tsim khoom. Nrog siab chromium thiab npib tsib xee cov ntsiab lus, lawv pom zoo oxidation tsis kam, sulfur kuj, thiab corrosion kuj ntawm kub kub. Sab nraud txoj kab uas hla yog categorized rau plaub qib (D1, D2, D3, thiab D4), thiab phab ntsa thickness muab faib ua plaub qib (T1, T2, T3, thiab T4). Cov kav dej nrog nruj dua tuaj yeem muab tau raws li qhov kev thov. Peb lub Hoobkas ua tau raws li TC1 thiab TC2 qhov kev xeem yuav tsum tau ua, ua cov kav dej no tsim nyog rau cov ntawv thov uas xav tau lub zog siab thiab tawv nyob rau hauv cov xwm txheej tsis zoo, xws li cov khoom siv rauv, lub taub hau, thiab cov khoom siv hluav taws xob.

Sib npaug ntawm 1.4841
|
STANDARD |
WERKSTOFF NR. |
UNS |
|---|---|---|
|
SIB 310 |
1.4841 |
S31000 |
EN 10216-5 Stainless Hlau Tube Specifications
| Txuj | TS EN 10216-5 |
|---|---|
| Tube Hom | Seamless Tube |
| Hlau No. | 1.4301, 1.4307, 1.4401, 1.4404, 1.4841, 1.4571, 1.4462 |
| ASTM Qib | 304/304L, 316/316L, 321, 316Ti, 2205 TSI |
| Ua tiav | Annealing Pickling Bright Annealing Polished |
| Sab nraud txoj kab uas hla | 6 mus 711mm |
| Thickness | 0.8 mus rau 30 mm |
| Kev sim | TC1 thiab TC2 |
| Daim ntawv thov | Lub Hom Phiaj Siab |
Tshuaj muaj pes tsawg leeg ntawm 1.4841 stainless hlau yeeb nkab
| C, % | Si,% | Mn,% | P, % | S, % | Cr,% | Tsis yog,% | Ti, % |
| 0.08 max | max 1.00 Nws | max 2.00 Nws | 0.04 max | 0.015 max | 17.0-19.0 | 9.0-12.0 | 5*C-0.7 |
TS EN 1.4841 Stainless hlau round yeeb nkab Mechanical Properties
| Tensile zog, MPa | Yield zog, MPa | Elongation,% |
| 500-730 | 200 feeb | 35 feeb |
TS EN 10216-5 Stainless Hlau Seamless Yeeb Nkab Sab Nraud Sab Nrauv
| Kub dov | Sab nraud txoj kab uas hla, mm | Ua siab ntev |
| 30 Tsawg dua lossis sib npaug rau OD Tsawg dua lossis sib npaug rau 219.1 | D2, ± 1% lossis ± 0.5mm | |
| 219.1<OD Tsawg dua lossis sib npaug rau 610 | D1, ± 1.5% lossis ± 0.75mm | |
| Txias Drawn | Sab nraud txoj kab uas hla, mm | Ua siab ntev |
| OD Tsawg dua lossis sib npaug rau 219.1 | D3, ± 0.75% lossis ± 0.3mm | |
| OD Tsawg dua lossis sib npaug rau 219.1 | D4, ± 0.5% lossis ± 0.1mm |
Phab ntsa Thickness thiab kam rau ua
| Kub dov | Phab ntsa Thickness, mm | Ua siab ntev |
| 30 Tsawg dua lossis sib npaug rau OD Tsawg dua lossis sib npaug rau 219.1, WT Tsawg dua lossis sib npaug rau 0.01 * OD thiab WT Tsawg dua lossis sib npaug rau 4 | T1, ± 15% lossis ± 0.6mm | |
| 30 Tsawg dua lossis sib npaug rau OD Tsawg dua lossis sib npaug rau 219.1 | T2, ± 12.5% lossis ± 0.4mm | |
| 219.1<OD Tsawg dua lossis sib npaug rau 610, WT Tsawg dua lossis sib npaug rau 0.05 * OD | -1.5 | |
| 219.1<OD Tsawg dua lossis sib npaug rau 610, 0.05 * OD<WT Tsawg dua lossis sib npaug rau 0.09 * OD | T1, ± 15% lossis ± 0.6mm | |
| 219.1<OD≤610, WT>0.09 * OD | T2, ± 12.5% lossis ± 0.4mm | |
| Txias Drawn | Phab ntsa Thickness, mm | Ua siab ntev |
| OD Tsawg dua lossis sib npaug rau 219.1 | T3, ± 10% lossis ± 0.2mm | |
| OD Tsawg dua lossis sib npaug rau 219.1 | T4, ± 7.5% lossis ± 0.15mm |
GNEE muaj ze li ntawm 18 xyoo ntawm kev paub hauv seamless stainless hlau yeeb nkab ntau lawm. Txhua cov yeeb nkab tau dhau qhov loj me, qhov chaw, PMI, eddy tam sim no, thiab kev ntsuas hydrostatic. Tsuas yog siab - cov yeeb nkab zoo yog ntim thiab xa mus rau cov neeg siv khoom thoob ntiaj teb. Peb cov yeeb nkab muab npog ob qho tib si imperial thiab metric qhov ntau thiab tsawg, nrog rau sab nraud diameters li ntawm 1.58 hli mus rau 108 hli. Qhov loj me tshwj xeeb muaj nyob rau ntawm kev thov. Peb kuj muab cov kav dej ncaj thiab U- khoov mus txog 30 meters ntev. Qib: 304/304L, 304H, 316/316L, 316H, 317L, 321, 310S (2520), 347H, S31803/S32205, S32750, S32760, S390304,
Cov Lus Qhia Tshwj Xeeb: ASTM A213, A270, A789, A790, GB / T13296, DIN17458, EN10216-5
Sab nraud txoj kab uas hla: 1.58mm - 108mm
Thickness: 0.38mm-5.18mm
Ntev: Ntau tshaj 25mm (U-khoov tau tshaj)
Kev Kho Hniav: A&P, BA, EP

Xa kev nug