Stainless hlau phaj: txhais, qauv thiab qib xaiv
Feb 01, 2025
Tso lus
Stainless hlau phaj yog lub tiaj tiaj dov stainless cov khoom uas tau muab los saum toj ntawm ib thaj tsam uas tau hais tseg, sib txuas cov kev tiv thaiv corrosion nrog lub zog siab thiab zoo toughness. Nws tiv thaiv kev tawm tsam los ntawm huab cua, chav dej thiab dej nrog rau cov kua qaub, alkalis thiab ntsev, thiab nws yog cov khoom siv ua ntej rau cov hlab ntsha, cov khoom siv hluav taws xob, cov kav dej thiab cov khoom thauj -cov kabmob hauv cov khoom ntub dej lossis tshuaj lom neeg ua haujlwm.
Dab tsi suav ua Stainless Hlau Phaj
Qhov sib txawv ntawm cov phaj thiab daim ntawv yog txhais los ntawm thickness, tsis yog los ntawm qhov dav, thiab tus ciam teb los ntawm kev tswj hwm tus qauv - yuav tsum tau ua. Raws li ASTM A480 / A480M cov khoom raug suav tias yog phaj ntawm 4.76 hli thiab siab dua, uas yog 3/16 hauv, thiab daim ntawv hauv qab ntawd. European xyaum ua raws li EN 10088-2 nrog thickness txwv teem los ntawm qhov ntev raws li cov qauv xws li EN 10029, thiab kub-kuav los tiag phaj yog feem ntau txiav txim los ntawm txog 3 mm upwards.
Kev xyaum ua mills muaj kub- dov phaj los ntawm kwv yees li 3–4.76 mm mus txog li 200 mm, nrog dav txog li 3 000 mm thiab ntev txog li 12 000 mm rau cov txheej txheem txheej txheem. Cov ntu hnyav dua thiab cov qauv dav dua yog ua kom xaj.
Phaj thiab Sheet: Thickness Ciam Teb
| Yam khoom | Daim ntawv | Phaj |
|---|---|---|
| Thickness ciam teb, ASTM A480 / A480M | Hauv qab 4.76 mm | 4.76mm thiab siab dua |
| Hom kev tsim khoom | Cold dov, ces annealed thiab pickled los yog ci annealed | Kub dov, ces annealed thiab pickled |
| Kev ua tiav | 2B, IB, 2D | Tsis yog . 1, kub dov annealed thiab pickled |
| Hom thickness muaj | 0.3-4.76 hli | 3-200 mm nyob ntawm zeb |
| Hom kev siv | Cov khoom siv, cladding, light fabrication | Cov nkoj, cov khoom siv hluav taws xob, cov khoom siv thiab cov khoom hnyav |
Kev faib tawm los ntawm Cov Qauv, Cov Qauv thiab Kev Pabcuam
Los ntawm metallurgical qauv: austenitic, ferritic, martensitic nrog rau nag lossis daus hardening, thiab austenitic -ferritic duplex.
Los ntawm cov tshuaj muaj pes tsawg leeg: chromium qib, chromium- qib nickel thiab chromium-nickel- qib molybdenum, nrog qis- carbon, siab- molybdenum thiab siab - purity variants ntawm txhua qib.
Los ntawm kev ua haujlwm corrosion: nitric acid resistant, sulfuric acid resistant, pitting resistant thiab kev nyuaj siab corrosion resistant qib.
Los ntawm qhov yuav tsum tau ua haujlwm: qis- qib kub, tsis yog- qib sib nqus, dawb- qib machining thiab qib superplastic.
Qib thiab cov qauv feem ntau qhia
| Qib | Qauv | Hom muaj pes tsawg leeg | Kev pabcuam phaj |
|---|---|---|---|
| 304 / 304L | Austenitic | 18% Cr, 8 % Ni; Cov pa roj carbon tsawg hauv 304L | Tank, dav fabrication, khoom noj khoom haus thiab khoom siv mis nyuj |
| 316 / 316L | Austenitic, molybdenum bearing | 16-18% Cr, 10-14% Ni, 2-3% Mo | Cov nroj tsuag tshuaj, marine thiab ntug hiav txwv kev pab cuam, tshav kub exchangers |
| 321 | Austenitic, titanium stabilized | 18% Cr, 8% Ni nrog Ti | Ua kom siab - qhov kev pabcuam kub uas yuav tsum zam kom tsis txhob hnov qab |
| 310S | Austenitic, siab alloy | 25% Cr, 20% yog ' | Rauv qhov chaw, siab -kub oxidation kuj |
| 2205 | Duplex | 22% Cr, 5% Ni, 3% Mo, N | Siab -kev pabcuam chloride, desalination, cia tank |
| 430 | Ferritic | 16-18% yog ' | Architectural cladding, khoom siv, tsis yog -cov dej num tshuaj |
| 410 / 420 | Martensitic | 12-13% Cr, siab dua carbon hauv 420 | Hnav cov khoom, shafts, cutlery, hardened Cheebtsam |
Phaj feem ntau raug txiav txim rau ASTM A240 / A240M rau chromium thiab chromium-nickel tiaj cov khoom, nrog ASTM A480 / A480M npog cov kev cai dav dav, kam rau ua thiab ua tiav cov ntsiab lus. Cov cuab yeej siv siab ua raws li cov lus qhia tshwj xeeb hauv cov cai uas cuam tshuam, thiab cov ntawv xaj European tau muab tso rau EN 10088-2 lossis rau EN 10028-7 rau kev siv siab.
Ua tiav, Kev Ua Siab ntev thiab Fabrication
Tsis yog . 1 tiav yog tus qauv kub- dov, annealed thiab pickled phaj nto. Nws yog tsim rau kev lag luam thiab cov qauv siv thiab feem ntau ua tiav los ntawm tus fabricator.
Thickness, flatness thiab dav tolerances yog teev nyob rau hauv tus txheej txheem tswj dimension. Tightening no tolerances nce nqi ntau dua li hloov qib hauv ntau zaus.
Ntug yog muab los ua zeb ntug, sheared los yog txiav kom loj los ntawm plasma, waterjet los yog laser. Txiav ntug yuav tsum tau hnav ua ntej vuam.
Vuam siv cov khoom sib txuam hlau xws li 308L rau 304 thiab 316L rau 316, nrog rau kev sib tw thiab kev ua haujlwm tom qab los kho cov zaj duab xis passive.
Cold forming suits austenitic qib, thaum qib martensitic feem ntau tsim nyob rau hauv cov mob annealed thiab hardened tom qab ntawd.
Zam tsis txhob muaj cov tshuaj chloride-cov kabmob cim cov kua thiab cov tshuaj ntxuav ntawm austenitic phaj destined rau kev pabcuam tshuaj lom neeg lossis cov ntug dej hiav txwv.
Tej kev siv
Pulp thiab ntawv cov khoom siv, digesters thiab Tshuag npaj cov nkoj.
Kub exchangers, condensers thiab phaj-thiab-frame units.
Tshuaj thiab tshuaj txheej txheem cov hlab ntsha, kab thiab kav.
Dyeing, film processing thiab khoom noj khoom haus.
Ntug hiav txwv thiab marine architectural cladding, canopies thiab fascias.
Pipelines, cia tanks, desalination cog thiab dej kho cov qauv.
Cov lus nug nquag
Q: Lub thickness ntawm stainless hlau ua phaj es tsis yog daim ntawv?
Nyob rau hauv ASTM A480 / A480M tus ciam teb yog 4.76 hli, sib npaug rau 3/16 nyob rau hauv.
Q: Puas yog 304 lossis 316 zoo dua rau kev ua haujlwm ntawm ntug dej hiav txwv?
316 lossis 316L yog qhov kev xaiv muaj kev nyab xeeb dua vim tias nws cov ntsiab lus molybdenum tiv taus cov tshuaj chloride pitting, thaum 304 txaus tsuas yog qhov tsis muaj chlorides thiab crevices.
Q: Qhov txawv ntawm 304 thiab 304L yog dab tsi?
304L muaj cov pa roj carbon tsawg tshaj plaws, uas txo qhov kev hnov mob thaum vuam thiab txo qhov kev pheej hmoo ntawm kev sib tsoo ntawm cov cua sov- thaj tsam cuam tshuam.
Q: Tus txheej txheem twg teev qhov kam rau ua?
Kev kam rau siab thiab ua tiav cov ntsiab lus yog los ntawm qhov dav dav - cov qauv yuav tsum tau muaj, ASTM A480 / A480M, thaum cov alloy muaj pes tsawg leeg thiab cov khoom siv tshuab tau teev tseg hauv ASTM A240 / A240M lossis sib npaug EN specification.
Q: Cov phaj puas tuaj yeem welded tom qab fabrication?
Yog lawm, tab sis welds nyob rau hauv austenitic phaj yuav tsum tau pickled thiab passivated, thiab stabilized los yog qis - carbon qib yuav tsum tau siv nyob rau hauv qhov sib koom ua ke yuav pom kub los yog corrosive kev pab cuam.
Q: Lub phaj txawv li cas ntawm cov khoom coil hauv tib qib?
Lub alloy tej zaum yuav zoo tib yam, tab sis txoj kev ua txawv. Phaj yog kub dov thiab ib txwm muab nkag rau hauv qhov annealed thiab pickled Tsis yog . 1 tag, uas cuam tshuam rau saum npoo thiab thickness kam rau ua.
Q: Puas yog lub phaj tuab txhais tau tias zoo dua corrosion tsis kam?
Tsis yog. Corrosion kuj nyob ntawm qhov muaj pes tsawg leeg thiab qhov chaw saum npoo, tsis yog nyob ntawm ntu tuab. Thickness yog xaiv rau lub zog, nruj thiab corrosion pub.
Xa kev nug