Dec 25, 2025
Tso lus
Taw qhia: Ob lub Titanium-Stabilized Qib, Ib Qhov Sib Txawv Carbon
Qib 321 (UNS S32100) thiab 321H (UNS S32109) yog titanium-stabilized austenitic stainless hlau tsim los rau siab - kev pab kub. Ob leeg siv titanium los ua ke nrog cov pa roj carbon thiab tiv thaiv chromium carbide nag lossis daus, yog li ob leeg tiv thaiv intergranular corrosion tom qab vuam. Cov ntsiab lus sib txawv yog cov ntsiab lus carbon: 321H nqa ntau yam tswj ntawm 0.04 mus rau 0.10 feem pua, uas nce creep zog ntawm qhov kub thiab txias, thaum 321, nrog 0.08 feem pua siab tshaj cov pa roj carbon, muab zoo toughness thiab marginally zoo intergranular corrosion kuj.
Chemical Composition piv
| Element (wt%) | 321 (ASTM A240) | 321H (ASTM A240 / A213) |
|---|---|---|
| Cov pa roj carbon (C) | 0.08 max | 0.04 - 0.10 |
| Manganese (Mn) | max 2.00 Nws | max 2.00 Nws |
| Phosphorus (P) | 0.045 max | 0.045 max |
| Sulfur (S) | 0.030 max | 0.030 max |
| Silicon (Si) | 0.75 max | 0.75 max |
| Chromium (Cr) | 17.00 - 19.00 | 17.00 - 19.00 |
| Nickel (Ni) | 9.00 - 12.00 | 9.00 - 12.00 |
| Titanium (Ti) | 5 x (C+N) min, 0.70 max | 4 x C min, 0.60 max |
| Hlau (Fe) | Tshuav | Tshuav |
Mechanical Properties Muab piv (Annealed)
| Khoom | 321 | 321H |
|---|---|---|
| Lub zog tensile | 515 MPa min | 515 MPa min |
| Yield zog (0.2% offset) | 205 MPa min | 205 MPa min |
| Elongation | 40% min | 40% min |
| Hardness | 201 HB max | 201 HB max |
Carbon, Creep Strength thiab Tsim Tso Cai
H suffix muaj nyob rau ib qho laj thawj: ntev - lub sij hawm nkag siab zog. Ntawm qhov kub siab tshaj li 540 C, cov pa roj carbon ntau dua ntawm 321H ntxiv dag zog rau cov matrix thiab stabilizes cov qauv carbide, muab cov qauv tsim kom muaj kev ntxhov siab ntau dua li 321 hauv boiler thiab siab - cov lej ntawm cov nkoj . 321H yog li teev rau superheater thiab reheater raj, kub chav piping thiab furnace 5 qhov sib xyaw ua ke ntawm qhov kub thiab txias. 900C ntau.
Toughness thiab Corrosion Resistance
321 khaws cov pa roj carbon tsawg, yog li nws khaws cov kev cuam tshuam zoo dua, suav nrog hauv qis - qhov kev pabcuam kub mus txog -196 C, thiab me ntsis zoo dua intergranular corrosion tsis kam tshaj 321H. Rau cov khoom sib hloov ntawm qhov kub thiab txias, los yog qhov twg toughness dominates tus tsim, 321 yog qib nyiam.
Hla -Standard Equivalents
| Txuj | 321 | 321H |
|---|---|---|
| UNS | S32100 | S32109 |
| JIS | SUS 321 | SUS 321 H |
| TS EN 10088 | 1.4541 (X6CrNiTi18-10) | - |
| TS EN 10028-7 | - | 1.4940 (X6CrNiTi18-10 H) |
Daim ntawv thov
321: automotive tso manifolds, tshuaj tua hluav taws kub exchanger raj, Cheebtsam alternating ntawm qis thiab siab kub
321H: boiler superheater thiab reheater raj, cov kav dej kub, petrochemical rauv sab hauv, nuclear theem nrab- cov kav dej hauv Circuit Court
FAQ
1. Lub luag haujlwm ntawm titanium hauv 321 thiab 321H yog dab tsi?
Titanium sib xyaw ua ke nyiam nrog cov pa roj carbon monoxide los tsim cov titanium carbides ruaj khov, tiv thaiv chromium carbide nag lossis daus ntawm cov ciam teb. Qhov no yog cov txheej txheem uas muab ob qib tsis kam rau intergranular corrosion tom qab vuam.
2. 321H puas tuaj yeem siv rau hauv qhov qis-kev pabcuam kub?
Nws tuaj yeem siv tau mus txog li ntawm -196 C, tab sis nws qhov qis - qhov kub thiab txias yog qis dua li ntawm 321. Rau kev hloov qis qis - thiab cov dej kub kub, 321 tau pom zoo.
3. Dab tsi muab cov hlau siv rau 321 thiab 321H?
ER321 hlau tuav titanium nyob rau hauv cov hlau weld thiab yog qhov sib txuam muab tub lim rau ob qib. ER347 yog lwm txoj hauv kev thaum titanium hloov mus hla lub arc yog ib qho kev txhawj xeeb.
4. Tus nqi sib txawv ntawm 321 thiab 321H yog dab tsi?
321H yog me ntsis kim dua 321 vim tias cov pa roj carbon nruj dua thiab cov kev sim ntxiv rau siab - qhov kev pabcuam kub. Tus nqi them yog feem ntau nyob rau hauv ib tus lej - tus lej rau qis -ob npaug - tus lej feem pua nyob ntawm daim ntawv khoom.
5. Qhov tseeb EN sib npaug ntawm 321H yog dab tsi?
Rau phaj thiab sawb, EN 10028-7 cov npe 1.4940 (X6CrNiTi18-10 H). Nco ntsoov tias 1.4542 yog EN tus lej rau 17-4 PH nag lossis daus-hardening hlau, tsis yog rau 321H.
6. 321 thiab 321H siab li -cov khoom kub tswj tau li cas?
Tshem tawm cov nplais oxide ib ntus los ntawm kev siv tshuab lossis tshuaj, tsis txhob ua kom txias sai tom qab siab - qhov kev pabcuam kub los tiv thaiv thermal shock, thiab ua raws li cov sijhawm teem tseg uas tsis yog - kev kuaj xyuas ntawm welds.