Tshuaj lom neeg muaj pes tsawg leeg ntawm steel hlau 1.4401 (En cov qauv)
Apr 30, 2025
Tso lus
1.4401 Stainless hlau,Kuj hu uaX5cnimo 17-12-2, yog European cov qauv kev tsim qauv sib npaugAISI 316Stainless hlau. Nws yog dav siv hauv kev ua yeeb yam, khoom siv marine, kev tsim khoom lag luam, thiab kev siv khoom noj khoom haus vim nws txoj kev lag luam corrosion zoo tshaj plaws thiab tshuab zog.
Txhawm rau pab cov kws saib xyuas engers, thiab cov kws tshaj lij cov kws tshaj lij kev txiav txim siab ntawm EN 1.4401 stainless hlau raws li European (en 10088-1) tus qauv.
1.4401 Stainless hlauCov qhab nia sib npaug
| Lub hom phiaj | Xws li qib |
|---|---|
| AISI \/ ASTM | 316 |
| Din | X5cnimo 17-12-2 |
| Tsis yog | S31600 |
| JIS | Sus316 |
Tshuaj lom neeg muaj pes tsawg leeg ntawm 1.4401 stainless hlau (thiab qauv)
| Lub ntsiab | Lub cim | Cov ntsiab lus (WT.%) |
|---|---|---|
| Pa roj carbon | C | Tsawg dua los yog sib npaug rau 0. 07 |
| Silicon | Si | Tsawg dua los yog sib npaug rau 1. 00 |
| Tus kws dai txiv manganese | Mn | Tsawg dua los yog sib npaug rau 2. 00 |
| Phosphorus | P | Tsawg dua los yog sib npaug rau 0. 045 |
| Leej mos | S | Tsawg dua los yog sib npaug rau 0. 015 |
| Yeebsab | Cr | 16.5 – 18.5 |
| Tus menyuam yaus | Ni | 10.0 – 13.0 |
| Molybdenum | Mo | 2.0 – 2.5 |
| Nitrogen | N | Tsawg dua los yog sib npaug rau 0. 11 |
| Liv | Zaum fe | Seem |
Cov yam ntxwv tseem ceeb ntawm 1.4401 stainless hlau
Zoo heev rau pitting thiab crevice corrosion ua tsaug rau lub xub ntiag ntawm Molybdenum (MO).
Haum rau high-humidity, saline, thiab tshuaj khia ib puag ncig me me.
Muaj cov Weldability zoo thiab muaj lub meej, ua rau nws zoo tagnrho rau cov khoom sib xyaw.
Feem ntau xaiv raws li cov khoom siv ntawm kev xaiv rau marine-qib stainless hlau ib cheebtsam.
1.4401 Cov Kev Siv Hlau Stainless
Kev sib hloov cua sov, cov hlab ntsha siab, thiab cov twj tso kua mis
Cov Khoom Noj thiab Dej Haus Ua
Tubrog Nkoj Rasteners Thiab Cov Txheej Txheem
Kws Tshuaj Thiab Khommetic Raug Cov Kab