420 vs 304 Stainless hlau hauv tsheb kauj vab chains thiab ntas
Jun 26, 2025
Tso lus
Ob Tsev Neeg Stainless ntawm Ib Lub Tsheb kauj vab
Stainless hlau tshwm nyob rau hauv lub tsheb kauj vab nyob rau hauv ob lub luag hauj lwm sib txawv, thiab ob qib kev koom tes yog sib txawv metallurgical tsev neeg. Hom 420 yog martensitic: nws tuaj yeem ua kom tawv tawv los ntawm kev kho cua sov, nws muaj zog sib nqus, thiab nws yog siv rau qhov chaw uas yuav tsum tiv thaiv kev puas tsuaj, xws li chains, sprockets, disc nres rotors thiab qee qhov fasteners. Hom 304 yog austenitic: nws tsis tuaj yeem hardened los ntawm kev kho cua sov, nws yog qhov tseem ceeb uas tsis yog-sib nqus tom qab annealing, thiab nws yog xaiv qhov twg corrosion kuj thiab cov tsos tseem ceeb tshaj hardness.
Tsis meej pem ob yog qhov chaw ntawm kev yuav khoom tsis zoo thiab kev txiav txim siab saib xyuas tsis zoo. Ib feem 304 yuav tsis raug ua rau hauv cov saw tawv tawv, thiab 420 thav duab raj yuav xeb sai dua li nws tus tswv xav tau.
Vim li cas Chains, Sprockets thiab Rotors Siv 420
Lub saw tsis ua haujlwm los ntawm kev hnav, tsis yog los ntawm kev ua haujlwm dhau. Pins, rollers thiab phaj qhov rub nyob rau hauv load hauv grit thiab dej, thiab thaum lub suab elongates cov saw noj cov cassette thiab chainrings nrog nws. Hom 420 muaj kwv yees li 12 txog 14% chromium nrog 0.15 txog 0.40% carbon, uas tso cai rau cov khoom kom quenched thiab tempered mus txog 50 HRC. Qhov kev nyuaj ntawd yog vim li cas cov saw tawv tawv yuav siv sij hawm ntau zaus ntev dua li qhov annealed austenitic nyob rau hauv tib lub sijhawm.
Kev lag luam tawm yog corrosion kuj. Nrog qis chromium dua li 304 thiab martensitic microstructure, 420 yuav ua rau xeb yog tias nws khaws cia ntub. Yog li ntawd, lubrication thiab drying teeb meem ntau npaum li cov khoom xaiv:
So cov saw hlau kom qhuav tom qab txhua lub caij ntub dej lossis ntug hiav txwv, tom qab ntawd rov ua dua -lubricate thaum cov kev sib txuas tseem sov me ntsis los ntawm kev siv.
Siv cov roj nplua nyeem nyob rau hauv qhuav, plua plav tej yam kev mob vim nws tsis tuav grit, thiab ib tug hnyav roj nyob rau hauv tsis tu ncua los nag.
Degrease thiab re-lubricate ua ntej pom cov xeb liab tshwm ntawm cov chais; nto xeb ntawm ib tug saw yog pib ntawm ceev tus pin hnav.
Hloov cov saw hlau rusted es tsis ntxuav nws. Elongation feem ntau tau pib, thiab cov saw hnav tsoos lub tsheb ciav hlau.
Qhov twg 304 Belongs on a Bike
Hom 304 tsis muaj txoj hauv kev kho cua sov mus rau qhov nyuaj siab, thiab nws qhov kev ua haujlwm qaug zog hauv cov ntu nyias yog qis dua ntawm cov tawv tawv thiab tempered carbon steels xws li 4130. Nws qhov txiaj ntsig tiag tiag yog tias nws tsis xeb hauv kev siv ib txwm, uas ua rau nws cov khoom siv zoo rau cov khoom siv uas raug, nyias thiab maj mam thauj khoom:
Lub raj mis cage bolts, khib thiab av nkos fasteners, thiab me me spacers
Fender nyob twj ywm, saw guards, kickstand daim hlau thiab trim npog
Cruiser thiab lub nroog thav ntawv los yog thav duab panels qhov twg zoo li thiab huab cua tsis kam tswj
Tsis tseem ceeb brackets thiab mounting hardware ntawm commuter tsheb kauj vab
Rau cov kabmob thauj khoom ntawm cov tsheb kauj vab kev ua tau zoo, cov neeg tsim khoom siv cov cua sov kho chromium molybdenum steel, aluminium lossis titanium, vim tias cov ntaub ntawv no muab lub zog ntau dua rau qhov hnyav dua li annealed austenitic stainless. A 304 thav duab yog ib qho kev xaiv tsim nyog rau lub tsheb kauj vab hauv nroog qis, tab sis qhov kev thov tias nws sib tw rau lub zog steel thav duab hauv kev nruj thiab qaug zog lub neej tsis tau txais kev txhawb nqa.
Qib sib piv
| Khoom | 420 stainless hlau (UNS S42000) | 304 stainless hlau (UNS S30400) |
|---|---|---|
| Tsev neeg | Martensitic | Austenitic |
| Chromium | 12.00 - 14.00% | 18.00 - 20.00% |
| Cov pa roj carbon | 0.15 - 0.40% | 0.07% max |
| Nickel | tsis tau teev tseg | 8.00 - 10.50% |
| Hardening txoj kev | Quench thiab npau taws, txog li 50 HRC | Txias ua hauj lwm nkaus xwb, tsis muaj hardening los ntawm kev kho cua sov |
| Sib nqus teb | Muaj zog sib nqus | Qhov tseem ceeb tsis yog-sib nqus thaum annealed, tsis muaj zog hlau nplaum tom qab ua haujlwm txias heev |
| Corrosion kuj | Nruab nrab, zoo tshaj plaws nrog polished los yog passivated nto | High atmospheric thiab dej tshiab raug |
| Kev siv tsheb kauj vab | Chains, sprockets, rotors, qee qhov bolts | Trim, tawb, fasteners, teeb lub luag haujlwm thav duab |
Fasteners, Counterfeits thiab Road ntsev
Kev ntsuam xyuas cov hlau nplaum paub tsuas yog cov lus qhia ntxhib xwb. Ib feem 420 yog ib txwm nyiam, tab sis 304 fasteners nrog dov threads thiab hnyav tsim lub taub hau tuaj yeem pom cov lus teb sib nqus me ntsis vim tias ua haujlwm txias ib nrab hloov cov austenite. Ntsuam xyuas ob peb fasteners ntawm tib batch ntawm tib lub hauv paus thiab kho lub zog, zoo ib yam rub raws li kev ceeb toom es tsis yog kev txiav txim. Liab xeb tom qab ib lub lim tiam ntawm kev caij ntub dej yog lub teeb liab txhim khu kev qha uas lub fastener yog ib qho qis nickel imitation lossis plated carbon steel.
Lub caij ntuj no txoj kev ntsev thiab cov tshuaj tsuag ntug dej hiav txwv yog qhov hnyav tshaj plaws uas lub tsheb kauj vab ntsib, thiab ob qho tib si tawm tsam stainless hlau los ntawm cov tshuaj dawb chloride:
Yaug cov thav duab, saw thiab fasteners nrog dej tshiab tom qab ib qho kev caij tsheb ntawm txoj kev ntsev los yog ntug hiav txwv.
Qhuav lub saw tam sim ntawd, ces lubricate nws, yog li dej tsis tuav tawm tsam tus pins.
Tsis txhob khaws lub tsheb kauj vab ntub dej, thiab tsis txhob tso ib txoj hlua khi ntsev thaum hmo ntuj.
Hloov cov ntsia liaj qhov rooj uas muaj xeb es tsis kho qhov chaw; cov corrosion twb txo cov seem.
Cov lus nug nquag
Q: Vim li cas cov hlua tsheb kauj vab feem ntau ua los ntawm 420 stainless hlau?
Vim tias 420 yog martensitic thiab tuaj yeem hardened txog li 50 HRC, uas muab cov pins thiab rollers qhov kev puas tsuaj rau cov saw hlau xav tau. Nws cov corrosion kuj tsuas yog nruab nrab, yog li niaj zaus lubrication thiab ziab yog qhov tseem ceeb.
Q: Puas yog 304 yog cov khoom siv rau lub tsheb kauj vab?
Rau lub luag hauj lwm lub teeb lub nroog thiab cruiser thav ntawv thiab rau trim Cheebtsam, yog. Rau kev ua haujlwm siab thav duab, kho cua sov chromium molybdenum steel, aluminium lossis titanium yog siv los hloov, vim annealed 304 tsis tuaj yeem phim lawv lub zog rau qhov hnyav piv lossis lub neej qaug zog.
Q: Kuv tuaj yeem pom cov bolts fake?
Ib qho hlau nplaum tsuas yog qhia tau hais tias: 420 yog ib txwm sib nqus, thaum ua haujlwm hnyav 304 tuaj yeem ua kom tsis muaj zog hlau nplaum. Saib es tsis txhob xeb liab tom qab siv ntub dej, thiab qhov chaw fasteners nrog cov qib teev tseg es tsis yog cov khoom tsis muaj npe.
Q: Cov 420 thiab 304 puas tuaj yeem siv ua ke?
Yog lawm, lawv feem ntau siv ib sab, piv txwv li 420 saw nrog 304 bolts. Qhov twg ob qho tib si kov cov hlau tsis tshua muaj txiaj ntsig hauv cov dej ntub dej, tshuaj xyuas ib ntus rau galvanic corrosion thiab ua kom cov pob qij txha qhuav thiab greased.
Q: Dab tsi yog qhov kev saib xyuas zoo tshaj plaws tom qab caij kev ntsev?
Yaug nrog dej tshiab, qhuav cov saw thiab tsav tsheb, tom qab ntawd siv cov roj nplua nyeem. Tsis txhob khaws cov tsheb kauj vab ntub dej, thiab xyuas cov thav duab fasteners rau xeb me ntsis tib lub sijhawm.
Q: Puas yog kev kho dua tshiab rau titanium tsim nyog rau lub tsheb kauj vab?
Tsuas yog rau cov neeg caij tsheb taug kev qhov hnyav tsawg kawg nkaus. Stainless hlau Cheebtsam xa cov feem ntau ntawm kev ua tau zoo ntawm ib feem ntawm tus nqi rau kev siv txhua hnub thiab kev ua si.