ASTM B466 C70600 Copper Nickel Alloy Seamless Yeeb Nkab
Nov 05, 2025
Tso lus
ASTM B466 tus qauv C70600 tooj liab-nickel alloy seamless yeeb nkab yog lub siab -kev ua tau zoo, corrosion- cov kav dej resistant ua los ntawm 90-10 tooj liab-nickel alloy (90% tooj liab, 10% npib tsib xee, nrog kev tswj cov hlau thiab manganese).
GNEE cov khoom siv ASTM B466 C70600 seamless kav tsim siv precision seamless extrusion los yog kos cov txheej txheem raws li ASTM B466 tus qauv. Lawv cov qauv microstructure tshem tawm cov vuam seams, txo cov ntsiab lus tsis ua hauj lwm thiab ua kom muaj kev ruaj ntseg siab tshaj plaws. Ua nrog nruj me ntsis kam rau ua (txoj kab uas hla ± 0.05-0.10mm, phab ntsa thickness ± 10%), C70600 seamless kav kom meej sib dhos thiab xau- kev sib txuas dawb, thiab muaj nyob rau hauv ob qho tib si qauv thiab kev cai ntau thiab tsawg kom tau raws li ntau yam kev xav tau.
90-10 tooj liab-nickel alloy kav dej muaj cov thermal conductivity zoo heev (kwv yees li 45–50 W/m·K), ua kom muaj cua sov hloov hauv cov condensers, cov khoom siv hluav taws xob, thiab cov tshuab cua txias. Lawv cov khoom siv tau zoo thiab lub zog nruab nrab (lub zog tensile ~ 380-450 MPa, elongation Ntau dua lossis sib npaug li 30%) ntxiv rau kev yooj yim ntawm fabrication thiab installation.

SpecificationsNtawmASTM B466 C70600 Cov Lus Qhia Tshwj Xeeb
| Qhov ntev | Tag nrho cov yeeb nkab yog tsim thiab tshuaj xyuas / kuaj rau cov qauv tsim xws li ASTM, ASME, thiab lwm yam. | ||||
| Qhov ntau thiab tsawg | 1/2 "TO 20" IN, DN15 txog DN500 | ||||
| OD Dia | 15mm txog 508mm | ||||
| Teem caij | SCH 40, SCH 80, SCH 160, SCH XS, SCH XXS, Tag nrho cov sij hawm | ||||
| Kev sim | Hardness Test/Chemical Analysis - Spectro Analysis/Flattening Test/Pitting Resistance Test/Flaring Test/IGCTest, thiab lwm yam. | ||||
| Ntev | Feem ntau 6meter lossis ntev ntev | ||||
| Phab ntsa Thickness | SCH10, SCH20, SCH30, STD, SCH40, SCH60, XS, SCH80, SCH100, SCH120, SCH140, SCH160, XXS DIN, JIS standard thickness | ||||
Chemical Composition ASTM B466 Chemical Composition 90/10 Seamless Yeeb thiab Tubes
| Cov ntsiab lus | ||
|---|---|---|
| UNS C70600 | UNS C71500 | |
| Copper incl Silver | Tseem tshuav | Tseem tshuav |
| Nickel suav nrog Cobalt | 9.0-11.0 Nws | 29.0-33.0 Nws |
| Lead, max | 0.05 | 0.05 |
| Hlau | 1.0 rau 1.8 | 0.40 rau 1.0 |
| Zinc, max | 1.0 | 1.0 |
| Manganese | 1.0 max | 1.0 max |
Lub cev muaj zog ASTM B466 Chemical Composition 90/10 Seamless Yeeb thiab Tubes
| Cov khoom | Metric | Imperial |
| Tensile zog, qhov kawg | 303-414 MPa | 43900-60000 psi |
| Tensile zog, tawm los (nyob ntawm npau taws) | 110-393 MPa | 16000-57000 psi |
| Elongation ntawm tawg (hauv 254 hli) | 42% | 42% |
| Machinability (UNS C36000 (dawb-txiav tooj dag)=100%) | 20% | 20% |
| Shear modulus | 52.0 GPA | 7 540 tzk |
| Poisson tus ratio | 0.34 | 0.34 |
| Elastic modulus | 140 GPa | 20 300 TZS |
ASTM B466 C70600 seamless steel kav yog dav siv nyob rau hauv marine engineering (nkoj pipelines, offshore platforms), lub zog tsim (txias tshuab), seawater desalination nroj tsuag, HVAC thiab tshuaj industries, thiab yog thawj xaiv rau daim ntawv thov uas yuav tsum tau zoo heev corrosion kuj, durability thiab ntev -lub sij hawm ua hauj lwm nyob rau hauv corrosive ib puag ncig.

Txhua lub raj ua tau raws li ASTM B466 / ASME SB466 cov qauv thiab tuaj nrog cov ntaub ntawv zoo, suav nrog Daim Ntawv Pov Thawj Cov Khoom Siv (MTC) (los txheeb xyuas cov alloy muaj pes tsawg leeg), daim ntawv qhia txog kev ntsuas hydrostatic (kom paub meej tias lub siab ncaj ncees), eddy tam sim no lossis ultrasonic tsis yog -kev kuaj kev puas tsuaj (NDT) kev xaiv), {3} kev ua haujlwm tsis pub dawb Cov txiaj ntsig ntawm intergranular corrosion.

1.Kev ntim khoom dav dav: daim ntawv tsis muaj dej + yam tsawg kawg yog peb txoj hlua khi.
2. Txheem export ntim: ntawv waterproof thiab yas + hlau ntawv overing + strapping yam tsawg kawg peb strapping siv

Xa kev nug