ASTM A790 UNS 31803 Duplex Steel Seamless Yeeb Nkab Rau Tubrog Nkoj Ib puag ncig
Jan 15, 2026
Tso lus
GNEE yog tus kws tshaj lij exporter ntawm siab - zoo duplex stainless hlau kav. Peb tau tshwj xeeb hauv kev xa tawm S31803 / S32205 (2205, EN 1.4462) series stainless hlau kav rau 19 xyoo thiab tau txais kev qhuas los ntawm peb cov neeg muas zaub tas li!
Peb muab siab - zoo ASTM A790 UNS 31803 seamless kav, uas ua tau zoo heev nyob rau hauv seawater ib puag ncig, nrog ib tug PREN ntawm 32-35. Tus nqi corrosion nyob rau hauv 3.5% NaCl tov (simulated seawater) yog ≤0.08 hli / xyoo, thiab nws cov pitting corrosion kuj yog 2-3 zaug siab dua 316L, thiab nws tsis kam rau marine atmospheric corrosion yog ntau tshaj 5 npaug zoo dua 304; Nws ua raws li NACE MR 0175 / ISO 15156 tus qauv thiab tiv taus cov crevice corrosion thiab chloride stress corrosion cracking nyob rau hauv tidal aav.
Customized solutions muaj · Thov ib daim ntawv tso cai pub dawb thiab tus nqi tshiab|Thov hu rau peb ntawm email.
Customized daws teeb meem muaj


Puas yog S31803 zoo ib yam li 2205?
UNS tus lej S31803 thiab S32205 sawv cev rau cov alloys nrog ntau tus yam ntxwv hauv ntau dua qhov sib txawv. Ua ntej, lawv yog ob qho tib si stainless hlau nrog cov ntsiab lus zoo sib xws. Ob leeg S31803 thiab S32205 belongs rau tsev neeg duplex 2205, uas txhais tau hais tias lawv suav nrog yuav luag sib npaug ntawm austenite thiab ferrite.
ASTM A790 UNS S3180 Cov khoom xyaw
| UNS No | AISI | C | Si | Mn | P | S | Cr | Mo | Ni | Lwm tus |
|---|---|---|---|---|---|---|---|---|---|---|
| S32205 | 2205 | 0.030 | 1.00 | 2.00 | 0.030 | 0.020 | 22.0/23.0 | 3.0/3.5 | 4.5/6.5 | N 0.14/0.20 |
Kev kho cua sov
Cov tshuaj kub yog nyob ib ncig ntawm 1100 ° C, thiab txias ceev.
| UNS npe | Kub | Quench |
|---|---|---|
| S31803 | 1870-2010 ° F [1020-1100 ° C] | Cia txias txias hauv huab cua lossis dej |
| S32205 | 1870-2010 ° F [1020-1100 ° C] | Cia txias txias hauv huab cua lossis dej |
Tensile Thiab Hardness Requirements
| Qib | Tensile zog, Min., Ksi [MPa] | Yield zog, Min., Ksi [MPa] | Elongation Hauv 2 Hauv., lossis 50mm, Min,% | Hardness, Max Brinell |
|---|---|---|---|---|
| S31803 | 90 [620] | 65 [450] | 25 | 290 |
| S32205 | 95 [655] | 70 [485] | 25 | 290 |
ASTM A790 UNS 31803 Duplex Steel Seamless Yeeb Nkab Daim Ntawv Thov
Offshore Roj & Gas: Platforms, pipelines, thiab cov khoom ua haujlwm raug dej hiav txwv.
Desalination Nroj Tsuag: Kuaj corrosive ntsev.
Kev Kho Dej: Seawater txias tshuab thiab twj tso kua mis.
Marine Vessels: Cheebtsam yuav tsum muaj kev tiv thaiv corrosion thiab lub zog.
Pulp & Ntawv: Digesters thiab cawv tanks.

Peb muab UNS 31803 stainless hlau txias- dov cov raj uas ua raws li ASTM A790 thiab ANSI B36.19 cov qauv, nrog rau sab nraud diameters xws li NPS 1/8 txog NPS 30, thiab phab ntsa thickness teem caij suav nrog Sch 5S, SCH10S, SCH40S, thiab SCH80S. Lwm qhov ntau thiab tsawg yog muaj raws li qhov kev thov. Qhov ntev ntev ntawm cov kav dej ASTM A790 yuav tsum ua raws li qhov yuav tsum tau muaj rau sab nraud txoj kab uas hla thiab phab ntsa tuab teev hauv ASTM A999. Cov kav dej yuav tsum tau khaws cia kom tshem tawm cov nplai. Yog hais tias ci annealing yog siv, pickling tsis tas yuav tsum tau.
Duplex steel S31803 hom
ASTM A790 Duplex steel S31803 yeeb nkab, ASTM A790 Duplex steel S32205 yeeb nkab, ASTM A790 Duplex steel S31500 yeeb nkab, ASTM A790 Duplex steel S32550 yeeb nkab, ASTM A790 Duplex steel S32750 yeeb nkab, ASTM A790 yeeb nkab, ASTM A790 Duplex steel yeeb nkab stainless-steel tube S31803, Duplex stainless-steel pipe S32205, Duplex stainless-steel pipe S31500, Duplex stainless-steel pipe S32550, Duplex stainless steel tube UNS S32750.

Xa kev nug