ASTM A554 TP304 Stainless hlau Welded Mechanical Tubing
Oct 13, 2025
Tso lus
ASTM A554 TP304 yog welded stainless hlau txhua yam tubing ua los ntawm tiaj dov 304 sawb. Cov kev qhia tshwj xeeb npog cov tubing rau cov khoom siv kho tshuab, cov qauv tsim, cov khoom siv kho kom zoo nkauj thiab tso pa tawm, qhov chaw huv si, kev cia siab rau lub zog thiab ruaj khov corrosion kuj tseem ceeb dua li kev tswj hwm lub siab. TP304 yog tus qauv 18 feem pua chromium thiab 8 feem pua nickel austenitic qib, uas nyob ruaj khov ntawm qhov kub thiab txias, yooj yim rau kev tsim thiab vuam, thiab tiv thaiv kev tawm tsam hauv feem ntau ntawm cov huab cua thiab ib puag ncig hnyav.
ASTM A554 TP304 Tubing yog dab tsi?
Lub raj yog yob tsim los ntawm lub tiaj tus sawb thiab kaw nrog ib tug longitudinal weld ua tsis muaj muab tub lim hlau, ces annealed thiab tiav rau qhov kev txiav txim saum npoo. Vim tias tsis muaj qhov muab tub lim ntxiv, cov phab ntsa nyob twj ywm tsis tu ncua thiab lub qhov dej nyob twj ywm du, uas haum rau kev siv tshuab, vaj tsev thiab kev tu cev. Cov khoom muaj nyob rau hauv round, square, rectangular thiab tshwj xeeb duab. A554 / A554M yog cov qauv ntsuas ntawm tib qhov kev qhia tshwj xeeb, thiab nws tseem hais txog cov cai cim uas lub raj tiav yuav tsum nqa.
Tshuaj muaj pes tsawg leeg ntawm Qib 304
| Element | Kev xav tau,% |
|---|---|
| Cov pa roj carbon | 0.08 max |
| Manganese | max 2.00 Nws |
| Phosphorus | 0.045 max |
| Sulfur | 0.030 max |
| Silicon | max 1.00 Nws |
| Chromium | 18.0 - 20.0 |
| Nickel | 8.0 - 11.0 |
Mechanical Properties
| Khoom | Tus nqi |
|---|---|
| Kev kho cua sov | Cov tshuaj kho tau ntawm 1900℃F / 1040 degree |
| Yield zog | 205 MPa / 30 ksi yam tsawg kawg nkaus |
| Tensile zog | 515 MPa / 75 ksi yam tsawg kawg nkaus |
| Elongation | 35 feem pua yam tsawg kawg nkaus |
Lub cev muaj zog ntawm TP304 Tube
| Khoom | Tus nqi |
|---|---|
| Qhov ntom | 8000kg / m3 |
| Elastic modulus | 193 gp ua |
| Lub ntsiab lus coefficient ntawm thermal expansion, 0 txog 100 degree | 17.2 µm / m / degree |
| Lub ntsiab lus coefficient ntawm thermal expansion, 0 txog 315 degree | 17.8 µm / m / degree |
| Lub ntsiab lus coefficient ntawm thermal expansion, 0 txog 538 degree | 18.4 µm / m / degree |
| Thermal conductivity ntawm 100 degree | 16.2 W/m.K |
| Thermal conductivity ntawm 500 degree | 21.5 W/m.K |
| Cov cua kub tshwj xeeb, 0 txog 100 degree | 500 J/kg |
| Hluav taws xob resistivity | 720 nΩ.m |
Qib sib npaug rau TP304 Tubing
| Qhov system | Lub npe |
|---|---|
| ASTM / ASME Cov | A554 TSO 304 |
| Tus lej Euronorm | 1.4301 |
| Euronorm npe | X5CrNi18-10 |
| British Standard | 304S31 |
| Swedish txuj | 2332 |
| Japanese Industrial Standards | TIAB SA 304 |
| Suav txheem | 06Cr19Ni10 |
Cov duab, qhov ntau thiab tsawg
Round raj rau txhua yam, hydraulic thiab kub exchanger dej
Square raj rau thav duab, railings, rooj tog thiab kev ua haujlwm
Rectangular raj rau load bearing thav duab thiab cladding kev txhawb nqa
Dimensions hais los ntawm sab nraud txoj kab uas hla los yog sab ntev ua ke nrog phab ntsa thickness
Finishes: zeb tiav, ci annealed thiab daim iav polished
Muab nyob rau hauv ncaj lengths, nrog txiav lengths thiab sib sib zog nqus polishing ntawm kev thov
Kev Tswjhwm Zoo, Marking thiab Ntim
Raw coil raug tshuaj xyuas los ntawm kev txheeb xyuas cov khoom zoo ua ntej kev tsim, qhov ntev ntawm qhov vuam yog saib xyuas hauv cov txheej txheem los ntawm eddy tam sim no thiab kuaj ultrasonic, thiab cov raj tiav dhau qhov kev soj ntsuam tag nrho. Kev tshuaj xyuas cov ntaub ntawv thiab cov duab tau khaws cia kom txhua pawg nyob twj ywm traceable, thiab peb theem kev tswj xyuas zoo ua kom muaj pes tsawg leeg thiab kev ua haujlwm ntawm txhua tus xa khoom zoo ib yam, uas yooj yim rau kev soj ntsuam tuaj rau cov neeg xa khoom thiab cov neeg tsim khoom.
Tube tau ntim rau hauv bales lossis hauv cov ntoo laminated, qhwv hauv cov yas thiab tiv thaiv kom nws tuaj txog hauv seaworthy, los yog ntim rau hauv ib qho kev xav tau. Kev kos npe ua raws li A554/A554M thiab txheeb xyuas tus qauv, qib, qhov ntev, tus naj npawb ntawm cov cua sov thiab cov batch tooj, ua ke nrog seb lub raj puas kub tiav lossis txias tiav.
Tej kev siv
Khoom noj khoom haus ua khoom noj thiab tu cev conveying tshuab
Pharmaceutical cog piping thiab khoom thav ntawv
Kev siv tshuaj thiab kev siv tshuab dav dav
Roj thiab roj twj thiab cov twj siv hluav taws xob
Architecture thiab kev tsim kho, suav nrog balustrades thiab handrails
Marine fittings thiab ntug hiav txwv installation
Cov khoom siv cua sov, cua thiab cua txias
Cov chaw kho dej thiab cov khoom siv ua liaj ua teb
Cov lus nug nquag
Q: ASTM A554 TP304 tubing yog dab tsi?
Nws yog welded mechanical tubing rau structural, ornamental, mechanical and hygienic applications xws li handrails, thav ntawv, khoom noj khoom haus, HVAC units thiab dej kho cov rooj sib txoos.
Q: Puas yog A554 raj welded lossis seamless?
A554 raj yog welded los ntawm lub tiaj tus sawb nrog ib tug longitudinal seam ua tsis muaj muab tub lim hlau, yog li ntawd lub phab ntsa thickness thiab lub bore nyob twj ywm nyob rau hauv ntev.
Q: TP304 txhais li cas?
TP sawv cev rau cov khoom tubular thiab 304 yog qib austenitic, muaj 18.0 txog 20.0 feem pua chromium thiab 8.0 txog 11.0 feem pua nickel nrog carbon txwv rau 0.08 feem pua.
Q: Qhov txawv ntawm ASTM A554 thiab ASTM A312 yog dab tsi?
A554 npog welded mechanical tubing rau kev ua haujlwm thiab kho kom zoo nkauj yam tsis muaj qhov ntsuas siab, thaum A312 npog seamless thiab welded yeeb nkab npaj rau siab thiab kub kev pab cuam.
Q: Cov duab twg thiab qhov chaw tiav yog muaj?
Round, square thiab rectangular seem nyob rau hauv zeb tiav, kaj annealed tiav thiab daim iav polished tiav, nkag ncaj lengths los yog txiav kom txiav.
Q: Qib twg sib npaug rau A554 TP304 hauv lwm lub tshuab?
Nws sib haum rau 1.4301 thiab X5CrNi18-10 hauv Euronorm, 304S31 hauv British Standard, 2332 hauv Swedish system, SUS 304 hauv Japanese Cov Qauv Txuj Ci thiab 06Cr19Ni10 hauv Suav tus qauv.