astm a351 cf8m cov khoom sib npaug

Sep 18, 2026

Tso lus

ASTM A351 CF8M yog dab tsi?

ASTM A351 CF8M yog austenitic stainless hlau casting qib tsim los rau siab- muaj cov khoom (xws li lub cev valve, twj tso kua mis, thiab cov yeeb nkab fittings).
CF=Corrosion-cov hlau tiv taus-chromium-nickel alloy
8=Nominal nickel cov ntsiab lus ntawm kwv yees li 8%
M=Muaj molybdenum (2.0–3.0%)
Nws yog cam khwb cia sib npaug ntawm wrought AISI 316 / UNS S31600 thiab muaj kev tiv thaiv zoo heev rau pitting thiab crevice corrosion nyob rau hauv chloride - muaj ib puag ncig.

 

Dab tsi yog cov khoom sib npaug rau ASTM A351 CF8M?

Qhov sib npaug ntawm CF8M yog AISI 316 / UNS S31600 (suav nrog ASTM A182 F316). Cov qib sib npaug European yog EN 1.4401, Japanese sib npaug yog SUS 316, thiab Chile sib npaug yog GOST 03CH17N14M3.

 

ASTM A351 CF8M khoom sib npaug

ASTM Qib AISI (US) UNS EN / DIN (EU) BS (UK) JIS (Nyiv) GOST (Kazakhstan)
ASTM A351 CF8M Txheem: 316 S31600 1.4401 316S17 TIAB SA 316 03Х17Н14М3
ASTM A351 CF8M Txheem: 316 S31600 1.4409 - - -
ASTM A351 CF3M 1 316L S31603 1.4404 316S12 SUS 316L 03Х17Н14М3
ASTM A351 CF8 304 S30400 1.4301 304S16 TIAB SA 304 08Х18Н10

Nco tseg:Qee cov ntaub ntawv sau npe EN 1.4409 raws li qhov sib npaug ntawm CF8M; Txawm li cas los xij, EN 1.4401 feem ntau suav hais tias yog qhov ze tshaj plaws European sib npaug rau ASTM A351 CF8M (cam khwb cia 316 stainless hlau). EN 1.4409 yog lwm hom 316-hom sib txawv nrog qhov sib txawv ntawm cov tshuaj lom neeg muaj pes tsawg leeg thiab daim ntawv thov. Rau kev yuav khoom, ib txwm txheeb xyuas cov tshuaj muaj pes tsawg leeg thiab cov khoom siv kho tshuab uas muaj nyob rau ntawm tus muag khoom MTC (Cov Khoom Siv Xeem Ntawv Pov Thawj).

 

CF8M vs . 316: Tshuaj muaj pes tsawg leeg

Qhov txawv tseem ceeb:Cov tshuaj muaj pes tsawg leeg ntawm cam khwb cia CF8M thiab wrought 316 txawv vim hais tias ntawm lub caij sib cais thaum lub sij hawm solidification txheej txheem thiab ferrite / austenite theem faib nyob rau hauv cam khwb cia lug. CF8M tso cai rau ntau dua chromium (txog 21%) piv nrog wrought 316 (18%) kom muaj kev tiv thaiv corrosion thiab kev ua haujlwm casting raws li ASTM A351 yuav tsum.

Element ASTM A351 CF8M (Ntaus) AISI 316 / F316 (Wrought)
C (max %) 0.08 0.08
Cr (%) 18.0 – 21.0 16.0 – 18.0
Tsis muaj (%) 9.0 – 12.0 10.0 – 14.0
Mo (%) 2.0 – 3.0 2.0 – 3.0
Feem ntau (%) 1.50 1.00
Mn (max%) 1.50 2.00
P (max%) 0.04 0.045
S (max %) 0.04 0.030

 

CF8M vs. CF3M: Mechanical Properties

Qhov txawv ntawm qhov tseem ceeb: CF8M feem ntau tso cai rau qhov kev pabcuam kub siab dua (txog li 538 degree) piv nrog CF3M (425 degree) vim tias CF3M cov ntsiab lus qis carbon hloov nws siab -kub carbide nag lossis daus tus cwj pwm thiab cuam tshuam rau nws qhov kev tso cai kub ntau hauv qee yam kev siv.

Mechanical Property CF8M (Kev daws teeb meem Annealed) CF3M (Kev daws teeb meem Annealed)
Tensile zog (min) 485 MPa / 70 ksi 485 MPa / 70 ksi
Yield zog (min) 205 MPa / 30 ksi 205 MPa / 30 ksi
Elongation (min) 30% 30%
Hardness (Tswj) 130-180 HWB 130-180 HWB
Kev Pab Cuam Kub Kub -254℃rau 538 degree -254℃rau 425 degree
Kev kho cua sov Kev daws annealing Ntau dua lossis sib npaug ntawm 1040 degree, ua raws li dej quenching Kev daws annealing Ntau dua lossis sib npaug ntawm 1040 degree, ua raws li dej quenching
Ferrite Cov ntsiab lus (Tswj) 5–20% 5–20%

 

Dab tsi yog qhov txawv ntawm CF8M thiab 316 stainless hlau?

Lawv qhia tib yam tshuaj muaj pes tsawg leeg, tab sis CF8M yog qib nrum (ASTM A351), thaum 316 yog qib wrought (ASTM A240 / A276). Qhov ntau ntawm chromium rau castings (18-21%) yog dav dua li cov khoom siv wrought (16-18%), thiab cov castings raug nruj dua NDT cov cai.

 

Qhov txawv ntawm CF8M thiab CF8 yog dab tsi?

CF8M muaj 2-3% molybdenum, whereas CF8 tsis muaj molybdenum (Mo Less tshaj los yog sib npaug rau 0.5%). CF8M muaj qhov zoo dua pitting corrosion kuj nyob rau hauv chloride-muaj ib puag ncig tshaj CF8. CF8M yog kwv yees sib npaug rau Qib 316, thiab CF8 rau Qib 304.

 

CF8M vs. CF8 vs. CF3M: Phau Ntawv Xaiv Cov Khoom

Kev sib piv Factor CF8 (≈304) CF8M (≈316) CF3M (≈316L)
Molybdenum Cov ntsiab lus ❌ Tsis muaj ✅ 2-3% Mo ✅ 2-3% Mo
Cov ntsiab lus carbon Tsawg dua lossis sib npaug li 0.08% Tsawg dua lossis sib npaug li 0.08% Tsawg dua lossis sib npaug li 0.03%
Pitting Corrosion Resistance (Cl⁻ Ib puag ncig) General Zoo heev Zoo heev
Vuam Sensitivity Nruab nrab Nruab nrab Tsawg (qis-carbon kom zoo)
Tej kev siv Cov dej tshiab, me me corrosive ib puag ncig Dej hiav txwv, kev ua tshuaj lom neeg, chloride- muaj cov xov xwm Welded Cheebtsam qhov twg tom qab-weld solution annealing tsis siv tau
Tus nqi txheeb ze Qib theem Puag +15–25% Puag +20–35%

 

Thaum twg yuav tsum xaiv CF3M es tsis yog CF8M?

CF3M (C Tsawg dua lossis sib npaug li 0.03%) yuav tsum raug xaiv thaum lub casting yuav tsis raug kev kho cua sov tom qab vuam, thiaj li yuav txo tau qhov kev pheej hmoo ntawm intergranular corrosion nyob rau hauv tshav kub - cuam tshuam cheeb tsam (HAZ). Yog tias cov kev kho mob tau ua tiav tom qab vuam, CF8M tau txais.

 

ASTM A351 vs ASTM A743 Txuj: Sib txawv

Kev sib piv Factor ASTM A 351 Cov Lus Qhia Tshwj Xeeb ASTM A743 Cov Lus Qhia Tshwj Xeeb
Scope ntawm daim ntawv thov Siab- muaj cov khoom pov thawj (valve, lub cev twj tso kua mis, cov khoom siv siab) General corrosion{0}}resistant castings (tsis yog- kev siv siab)
Kev soj ntsuam yuav tsum tau Cov kev cai nruj dua, suav nrog NDT thiab kev ntsuas siab thaum tau teev tseg Cov kev cai tshuaj ntsuam xyuas tsawg dua
Daim ntawv pov thawj yuav tsum tau Feem ntau xav tau ASME- cov chaw tsim nyog rau kev siv cov cuab yeej siv siab Tsis tas yuav tsum muaj daim ntawv pov thawj ASME
Tej kev siv Cov kav dej, cov hlab ntsha siab, li qub, twj tso kua mis, thiab lwm yam khoom siv siab- khaws cia Cov khoom sib xyaw ua ke, tsis yog -cov vaj tse siab, npog, thiab corrosion- cov khoom cam khwb cia

 

Tuam Tshoj ASTM A351 CF8M stainless hlau castings

GNEE tuaj yeem muab ASTM A351 CF8M stainless hlau castings (cam khwb cia sib npaug rau AISI 316) rau siab- muaj thiab corrosion- cov ntaub ntawv tiv thaiv, suav nrog lub cev valve, twj tso kua mis, impellers, yeeb nkab fittings, flanges, thiab cov khoom siv pov tseg. Cov khoom tuaj yeem tsim tau raws li cov neeg siv khoom kos duab nrog cov txheej txheem xws li peev casting, CNC machining, kev kho cua sov, thiab kev ua tiav. GNEE muab tag nrho cov ntaub ntawv traceability nrog EN 10204 3.1 MTC, tshuaj muaj pes tsawg leeg tsom xam, mechanical testing, dimensional soj ntsuam, PMI, thiab NDT cov ntaub ntawv los xyuas kom meej ua raws li ASTM A351 cov kev cai rau kev lag luam xav tau xws li marine, tshuaj ua, roj & roj, thiab muaj kua system.

 

ASTM A351 CF8M Stainless hlau rooj vag Valve

Khoom npe Stainless hlau Flange rooj vag Valve
1. Khoom siv SS304/316/304L/316L (CF8/CF8M/CF3/CF3M), thiab lwm yam.
2. Loj 1/2 ~ 12 nti (DN15 ~ DN300)
3. Kev sib txuas xaus Xov xaus / Flange kawg
4. Chaw nres nkoj Chaw nres nkoj puv
5. Ua haujlwm siab PN16-PN25 / 150LB-300LB / 10K-20K
6. Ua haujlwm Temp. -20 ~ 120ºC, lossis raws li cov neeg siv khoom xav tau rau kev lag luam sib txawv.
7. Haum Nruab Nrab Dej, Natural Gas, Roj thiab qee cov kua corrosive
8. Ua haujlwm Swing
9. Kev Tshawb Fawb & Kev Ntsuas API 598, EN12266
10. Lub Sijhawm xa tuaj 30 ~ 45 hnub
11.Package Standard Exporting Plywood Case

ASTM A351 CF8m Stainless Steel Gate Valve CAD

ASTM A351 CF8m Stainless Hlau Rooj vag Valve CAD
ASTM A351 CF8m Stainless Steel Gate Valve
ASTM A351 CF8m Stainless hlau rooj vag Valve

Tsis tas li ntawd, peb kuj muab cov khoom hauv qab no:

ASTM A351 CF8m Investment Cast Valve Disc
ASTM A351 CF8m Peev Cast Valve Disc
ASTM A351 CF8m Stainless Check Valves
ASTM A351 CF8m Stainless Hlau Kos Valve
ASTM A351 CF8m Ball Valves
ASTM A351 CF8m Pob Valve
ASTM A351 CF8m Stainless Steel Floating Ball Valves
ASTM A351 CF8m Stainless Hlau Floating Pob Valves

Txhawm rau pab tsim cov ntsiab lus tshwj xeeb lossis kev sim cov txheej txheem, koj puas tuaj yeem qhia meej:
Koj puas xav tau cov kev txwv tshwj xeeb rau cov tshuaj muaj pes tsawg leeg lossis yam tsawg kawg nkaus rau cov khoom siv tshuab?
Rau cov khoom tshwj xeeb lossis qhov chaw ua haujlwm (piv txwv li, qhov kub thiab txias, raug tshuaj lom neeg) yog koj tsim?

Hu rau tam sim no

FAQ

Q: Puas yog A351 CF8M thiab A743 CF8M hloov pauv tau?
A: Lawv tsis tuaj yeem hloov pauv ncaj qha. A351 siv rau siab- khaws cov khoom, xav tau ASME ntawv pov thawj thiab nruj NDT; A743 siv rau qhov tsis yog -siab- khaws cov khoom nyob rau hauv ib puag ncig corrosive. A743 daim ntawv pov thawj tsis tuaj yeem hloov pauv rau A351 yam tsis muaj tus tswv sau ntawv pom zoo.

 

Q: Qhov kev pabcuam siab tshaj plaws rau CF8M yog dab tsi?
A: Qhov kev pabcuam kub kub rau kev daws teeb meem -annealed CF8M yog −254℃txog 538℃(−425℃F txog 1000℃F). Cov teeb meem creep thiab oxidation yuav tsum raug txiav txim siab rau qhov kub siab tshaj 538 degree.

 

Q: Vim li cas nws thiaj li tsim nyog los tswj cov ntsiab lus ferrite hauv CF8M castings?
A: Ferrite (5–20%) helps inhibit hot cracking during casting, but excessive ferrite (>25%) txo corrosion kuj. Qhov feem pua ​​​​ferrite tiag tiag yuav tsum tau teev nyob rau hauv MTC (Cov Khoom Siv Xeem Ntawv Pov Thawj).

 

Q: Dab tsi vuam consumables siv rau CF8M?
A: ER316L/E316L (AWS A5.9/A5.4) electrodes lossis filler wires feem ntau yog siv. Yog hais tias lub hauv paus hlau yog CF8M, carbon enrichment tej zaum yuav tshwm sim nyob rau hauv lub tshav kub - cuam tshuam cheeb tsam (HAZ); yog li ntawd, post-weld tov annealing los yog hloov mus rau CF3M puag hlau yog pom zoo.