ASTM A312 TP304L Pickled thiab Annealed Stainless Hlau Yeeb Nkab
Sep 28, 2025
Tso lus
ASTM A312 SP304L Seamless Yeeb Nkab yog ib hom stainless hlau tsim rau high} kub thiab corrosive ib puag ncig. "AVTM A312" Tsim Cov Qauv Txheej Txheem rau Austenitic Stainless Hlau Yeeb Nkab (feem ntau hu ua 18/8 qhov ncauj lus chromium thiab 8% npib tsib xee). "Seamless" yog hais txog cov yeeb nkab tsis muaj welds thiab ib txwm tsim los ntawm kev rho tawm. Piv rau tus qauv 304 stainless hlau, nws muaj kev txhim kho weldability thiab corrosion tsis kam.
Gnee muajTPPPTHLED THIAB Annealed Stainless Hlau Yeeb NkabCov. Ib qho txheej txheem tswj qhov kub yog qhov ntsuas kub txhawb kev ua haujlwm ntxhov siab thiab ruaj khov cov qauv Austenic. Kev kho mob tom qab thiab kev kho mob passivation tsim cov yeeb yaj kiab, ntxuav cov yeeb yaj kiab passenty, ua rau muaj kev sib xws, du zoo nkauj lossis matte passive tiav.
Ib qho ntxiv, tsau ntev, ntau yam ntev, thiab random ntev, thiab ob zaug los yog ob zaug: Caj EN To end, threaded te xaus). Kev xaiv ntim ntim suav nrog noo noo {{}} Cov ntaub ntawv ntoo qhwv thiab ntoo crates, pallets, lossis worseive yas zaj duab xis.

AISI 304L kav cov kav dej tshwj xeeb
| Cov Qauv Qhia Tshwj Xeeb | ASTM A312 Tp34L ASME SA312 TPP04L |
| Phab Ntsa Thickness | 0.1 - 60 hli |
| Qhov loj | ½ rau 6 nti nominal bore |
| Teem Sij Hawm Yeeb Nkab Tickness | Teem Sij Hawm 60, xs, sij hawm 160, STD, Teem Sij Hawm 16, Sijhawm 140, Sijhawm 140, Sijhawm 10, Sijhawm 30, Chaw Muag Khoom hauv Mumbai |
| Qho ntev |
Ib leeg random ntev 5 mus rau 7 meter Ob chav random ntev 10 - 12 meter |
| Nto tas | Polished, ci, annealing, txias tiav, pickling |
| Lub hom phiaj | Din, JIS, ASTM, GB, ASME, AISI, AMS, en, GOST |
| Hom | Welded, Seamless, ERW, EFW Tus Neeg Muag Khoom thiab Chaw tsim tshuaj paus |
| Kev txawj | Cold Rolled Kub Rolled |
| Kev Tsim Kho Duab | Puag ncig, lub thawv ntawv, xwmfab, duab plaub |
| Raug Tshuab | Kub Txias tsim |
ASTM A312 TP304L Stainless Hlau Seamless Yeeb Nkab Yeeb Nkab Tshuaj Muaj Zog
| SS Qib | ASTM A312 Tshuaj Muaj Zog% Tshaj Plaws | ||||||||
|---|---|---|---|---|---|---|---|---|---|
| C | Mn | P | S | Si | Cr | Ni | Mo | Ti | |
| TPP3L | 0.035 | 2.00 | 0.045 | 0.030 | 1.00 | 18.0-20.0 | 8.0-13.0 | --- | --- |
ASTM A312 TP304L Stainless Hlau Seamless Yeeb Nkab Cov Khoom Siv
| SS Qib | Kev Kho Cua Sov | Lub zog tensile, Min Ksi [MPa] | Paib muaj zog, min ksi [MPA] |
|---|---|---|---|
| TPP3L | Lus teb | 70 [484] | 25 [170] |
Gnee muaj ze li ntawm 18 xyoo ntawm kev paub hauv seamless stainless hlau raj ntau lawm. Txhua lub raj raj undergoes sab, nto, PMI, EDDY tam sim no, thiab hydrostatic kev xeem. Tsuas yog siab - cov raj zoo tau ntim thiab xa mus rau cov neeg siv khoom thoob ntiaj teb. Peb cov raj cev npog npog ob qho Imperial thiab letric ntau thiab tsawg, nrog sab nraud diameters xws li ntawm 1.58 hli txog 108 hli. Qhov ntau tshwj xeeb yog muaj nyob rau thaum thov. Cov Qib: 304 / 304H, 316/36, 316, 31, 3423 / s32750, s3274, 904L
Cov lus qhia tshwj xeeb: ASTM A213, A270, A789, A790, GB / T13296, DIN17458, EN10216-5
Txheej Ntau Incuctions: 1.58mm - 108mm
Thickness: 0.38mm - 5.18mm
Ntev: Ntau 25mm (u - Khoov Khov)
Nto Kho: A & P, BA, EP
Tag nrho cov kav hlau stanbul tsis muaj kuab lom Lawv tau thauj nyob rau hauv cov qauv txheem lossis mob siab rau cov tsheb los xyuas kom meej meej txog kev ncaj ncees thiab kev nyab xeeb ntawm cov khoom thaum pib. Peb muab cov khoom xa mus thoob ntiaj teb, nrog cov thawj coj txhuas ntawm 7 -}}}}}} 15 hnub los ntawm kev tsim khoom los ntawm kev xa khoom, ua kom tau txais khoom xa mus rau peb cov neeg siv khoom.


Xa kev nug