ASTM A312 Austenitic Stainless Hlau Yeeb Nkab: Cov Ntawv Thov thiab Cov Kev Xav Tau
Apr 09, 2025
Tso lus
Scope ntawm ASTM A312 / A312M
ASTM A312 / A312M yog ASTM International specification rau seamless, ncaj- seam welded thiab hnyav hnyav ua haujlwm welded austenitic stainless hlau yeeb nkab npaj rau siab - kub thiab kev pabcuam corrosive. Tam sim no tsab A312 / A312M-24b tau tshaj tawm thaum Lub Kaum Hli 2024 thiab txuas ntxiv txheeb xyuas cov khoom siv, kev tsim khoom, kev kho cua sov, kev tshuaj xyuas thiab kev sim rau cov qib yeeb nkab siv thoob plaws cov tshuaj, roj av, zaub mov, tshuaj thiab marine engineering sectors.
Vim hais tias cov lus qhia tshwj xeeb tau sau rau ob qho tib si ambient thiab elevated - qhov kev pabcuam kub, nws tswj tsis tau tsuas yog cov khoom xa tuaj thiab cov khoom siv kho tshuab, tab sis kuj yog cov xwm txheej ntawm cov vuam, kev kho cua sov siv tom qab tsim, thiab cov kev sim tsis zoo thiab kev puas tsuaj uas yuav tsum tau ua ua ntej cov yeeb nkab tso tawm.
Cov khoom siv thiab kev tsim khoom
Cov khoom siv suav nrog cov qib austenitic xws li TP304, TP304L, TP316, TP316L, TP321H thiab TP347H, tag nrho cov uas cia siab rau chromium, npib tsib xee thiab, qhov cuam tshuam, molybdenum rau corrosion kuj thiab siab - kub lub zog. Siab dua -alloy super- qib austenitic xws li UNS S31254, 6% molybdenum cov ntaub ntawv, yog siv qhov twg halide- bearing acid media yuav tua cov pa 316L yeeb nkab.
Seamless yeeb nkab:ua los ntawm kub dov los yog txias daim duab, uas muab ib tug homogeneous phab ntsa thiab siab qhov tseeb tsis muaj ib tug weld seam.
Welded yeeb nkab:tsim los ntawm sawb lossis phaj thiab koom nrog tsis siv neeg tungsten inert gas lossis hlau inert roj vuam. Lub vuam feem ntau yog radiographed thaum daim ntawv xaj xaj lossis kev xa mus rau kev tsim kho code yuav tsum tau, thiab kev ntsuam xyuas kev sib xyaw ua ke ntawm ASTM A262 Practice E yog siv los xyuas kom meej tias cov cua sov- thaj tsam cuam tshuam tsis tau sensited.
Kev kho cua sov yuav tsum tau
Austenitic yeeb nkab yuav tsum tau tov annealed thiab sai txias kom rov qab corrosion kuj. Rau cov qauv qib no txhais tau hais tias tuav ntawm kwv yees li 1040 txog 1100 degrees Celsius thiab quenching lossis ceev cua txias kom cov chromium carbides rov qab mus rau hauv cov tshuaj.
Cov qib stabilized nrog titanium, xws li TP321H, los yog nrog niobium, xws li TP347H, tau txais kev kho kom ruaj khov ntxiv kom cov pa roj carbon yog khi li ruaj khov carbide thiab intergranular corrosion kuj yog khaws cia tom qab ntev raug ntawm qhov kub siab. Cov yeeb nkab tau muab rau hauv qhov cua sov- kho mob; field dabtsi yog khoov los yog vuam tsim ib qho kev mob hauv zos tshiab uas yuav tsum tau xav txog hauv cov txheej txheem fabrication.
Dimension Tolerances
| Khoom | Feature | Hom kam rau ua |
|---|---|---|
| Lub cev txias txias | Sab nraud txoj kab uas hla mus txog 25.4 mm | ntxiv los yog rho tawm 0.10 mm |
| Lub cev txias txias | Sab nraud txoj kab uas hla mus txog 88.9 mm | ntxiv los yog rho tawm 0.25 mm |
| Kub dov yeeb nkab | Sab nraud txoj kab uas hla mus txog 127 mm | ntxiv los yog rho tawm 1.6 mm |
| Lub cev txias txias | Phab ntsa thickness mus txog 3 hli | ntxiv 20% / rho tawm 0% |
| Lub cev txias txias | Phab ntsa thickness siab tshaj 3 hli | ntxiv 22% / rho tawm 0% |
Cov xwm txheej saum npoo yog tswj thiab. Cov yeeb nkab rau kev pabcuam tu cev yog cov neeg kho tshuab polished rau sab hauv thiab sab nraud kom muaj qhov ntxhib ntawm li 0.8 micrometer Ra lossis zoo dua, thaum cov yeeb nkab muaj feem ntau yog pickled lossis passivated kom tshem tawm cov nplai thiab rov ua cov zaj duab xis passive oxide tom qab kev kho cua sov.
H Qib thiab siab -Tsub Ua Haujlwm
Cov qib nqa H suffix, xws li TP316H thiab TP347H, yog npaj rau kev nce siab - qhov kub thiab txias. Lawv cov ntsiab lus carbon siab dua, los yog lawv cov niobium thiab titanium ntxiv, ua rau lub zog creep rupture kom cov yeeb nkab tuaj yeem nqa cov khoom ntawm qhov kub uas tus qauv qis - carbon qib yuav deform zuj zus.
TP347H yog dav siv rau superheater thiab reheater tubing nyob rau hauv loj boilers, qhov twg nws tuav oxidation thiab corrosion kuj ntawm hlau kub ntawm roughly 750 degrees Celsius thiab tshaj, nrog rau cov kev tso cai tso cai ntau yam kev ntxhov siab ncua mus txog 870 degrees Celsius nyob ntawm tus tsim code. Tshaj li qib ntawd, lossis qhov chaw oxidation ua rau qhov kev txwv, siab dua - qib alloy xws li S31254 tsev neeg lossis lwm yam 6% molybdenum cov ntaub ntawv raug txiav txim siab.
Kev Tshuaj Xyuas, Kev Ntsuas thiab Kev Tswj Xyuas Zoo
Kev kuaj Hydrostatic:Cov txheej txheem siab siab yog mus txog 19 MPa rau cov yeeb nkab nrog sab nraud txoj kab uas hla mus txog 88.9 hli, thiab mus txog 31 MPa rau cov kab loj dua.
Eddy tam sim no kuaj:performed to ASTM E426 to detect surface and near-surface discontinuities on the pipe body.
Intergranular corrosion xeem:ASTM A262 Practice E yog siv los xyuas kom meej tias cov khoom tsis tau rhiab heev los ntawm vuam los yog kev kho cua sov.
Kev kuaj hluav taws xob:tau teev tseg rau welded yeeb nkab qhov twg cov referencing siv code, xws li ASME B31.3 rau txheej txheem piping, yuav tsum tau kuaj weld.
Mechanical xeem:tensile, flattening thiab khoov kuaj xyuas lub zog, ductility thiab weld soundness.
Kev lag luam kev siv
ASTM A312 yeeb nkab tau teev rau cov txheej txheem piping nyob rau hauv cov tshuaj thiab petrochemical cov nroj tsuag, refinery thiab roj ua kab, zaub mov thiab tshuaj hloov chaw, thiab marine los yog offshore seawater piping. Kev xaiv ntawm cov qib los mus rau hom corrosive tam sim no, tus qauv tsim kub thiab cov txheej txheem tsim: 304L rau kev pabcuam me me corrosive ambient, 316L qhov twg chlorides lossis organic acids tshwm sim, thiab cov qib H stabilized qhov twg nkag los tiv thaiv cov phab ntsa tuab.
Cov lus nug nquag
Q: Qhov txawv ntawm ASTM A312 thiab ASME SA312 yog dab tsi?
Cov kev xav tau ntawm chemistry, mechanical thiab testing yog tib yam. ASME SA312 yog tus qauv siv rau hauv ASME code, uas yog ib tsab hais txog kev tsim cov kav dej siab.
Q: Thaum twg TP316L yuav tsum xaiv dua TP304L?
Thaum cov txheej txheem kwj muaj chlorides, organic acids los yog txhoj puab heev tshuaj ntxuav. Qhov sib ntxiv ntawm molybdenum hauv TP316L txhim kho pitting thiab crevice corrosion kuj, txawm tias qis -carbon chemistry ntawm ob qib txwv carbide nag lossis daus tom qab vuam.
Q: Vim li cas cov tshuaj annealing xav tau?
Kub ua hauj lwm thiab vuam cuam tshuam lub microstructure thiab tuaj yeem precipitate chromium carbides. Annealing ntawm 1040 txog 1100 degrees Celsius ua raws li cov cua txias sai yaj cov carbides thiab rov ua kom cov corrosion kuj ntawm austenitic matrix.
Q: Cov qib H siv rau dab tsi?
Kev kub siab - qhov kev pab cuam kub qhov twg creep rupture zog tswj tus tsim, xws li boiler superheater thiab reheater tubing thiab kub txheej txheem kab.
Q: Yuav ua li cas welded yeeb nkab weld zoo xyuas?
Los ntawm kev ntsuam xyuas hluav taws xob thaum xav tau los ntawm kev xaj xaj lossis kev tsim kho, ua ke nrog kev ntsuas kev sib xyaw ua ke ntawm ASTM A262 Practice E thiab, rau cov kev pabcuam tseem ceeb, kev sib tw flattening uas qhib lub vuam rau kev tshuaj xyuas.
Q: Puas yog A312 npog duplex stainless hlau yeeb nkab?
A312 nws tus kheej yog austenitic specification. Qhov twg duplex lossis super- qib austenitic cov cuab yeej xav tau, qhov tsim nyog duplex lossis siab- alloy specification yuav tsum tau hais, txawm tias qib xws li UNS S31254 feem ntau tham nrog A312 yeeb nkab hauv kev pabcuam corrosive.