ASTM A269 thiab ASTM A270

ASTM A269 tus qauv siv rau seamless thiab welded stainless hlau thiab npib tsib xee alloy kav, feem ntau yog siv rau dav - lub hom phiaj piping systems, tshav kub exchangers, condensers, boilers, turbines thiab lwm yam kev siv. Tus qauv npog ntau yam ntaub ntawv, suav nrog 304, 304L, 316, 316L thiab lwm yam stainless hlau.

ASTM A270 tus qauv siv rau me me - txoj kab uas hla stainless hlau seamless thiab welded kav, feem ntau yog siv rau cov kav dej hauv cov khoom siv tu cev thiab cov khoom ua zaub mov. Cov qauv no muaj cov kev xav tau siab dua rau cov khoom siv purity thiab huv si, thiab feem ntau yog siv rau hauv lub sijhawm uas yuav tsum tau ua kom huv huv, xws li cov dej haus, cov khoom siv tshuaj, thiab lwm yam.

 

Dab tsi yog qhov txawv ntawm ASTM A269 thiab A270?

ASTM A269 yog rau kev dav dav -lub hom phiaj stainless hlau tubing, thaum ASTM A270 tshwj xeeb rau kev siv huv huv, yuav tsum tau ua kom nruj dua saum npoo, huv si, thiab cov khoom siv kho tshuab. Qhov sib txawv tseem ceeb suav nrog A270 tus qauv qhia txog kev ua kom lub ntsej muag zoo dua thiab huv si sab hauv kom tiv thaiv kev sib kis, thiab cov kev xav tau nruj dua rau kev ntim khoom thiab cov txheej txheem tsis zoo, qhov A269 yog tsim rau cov kev pabcuam tseem ceeb tsawg xws li cov khoom siv hluav taws xob.

 

ASTM 270 specification yog dab tsi?

ASTM A270 sanitary stainless yeeb nkab feem ntau yog hais txog cov yeeb nkab me me, feem ntau ntawm 1/2 "rau 2 1/2", thickness ntawm 0.049 hauv (1.24mm) txog 0.15 hauv (3.81mm). Qhov siab tshaj plaws sab nraud ntawm ASTM A270 tubing yog 12 nti (304.8 mm). ASTM A270 tubing siv nti - phaus raws li tus qauv ntsuas.

 

Dab tsi yog qhov ua tiav ntawm ASTM A270?
Dab tsi yog qhov ua tiav ntawm ASTM A270? Nto tiav yog 20 µ-in Ra (0.5 µm) ID siab tshaj plaws, 30 µ-in Ra (0.8 µm) OD qhov siab tshaj plaws ntawm qhov roughness ntsuas ib ASME / ANSI B46. 1 nrog rau qhov profileometer nyeem ntawm 90 degrees rau nteg.

 

Qhov txawv ntawm ASTM A269 thiab A270

Feature ASTM A 269 Cov khoom siv ASTM A270 1
Scope Npog seamless thiab welded austenitic stainless hlau tubing rau kev xeb dav dav - tiv taus thiab siab - kev siv kub. Npog stainless hlau tubing rau kev huv thiab huv, suav nrog zaub mov, dej haus, thiab kev siv tshuaj.
Daim ntawv thov Thaum tshav kub kub exchangers, condensers, boilers, tshuaj nroj tsuag. Sanitary piping systems, mis nyuj, breweries, khoom noj khoom haus, tshuaj kav dej.
Nto tiav Tej zaum yuav muaj xws li annealed, pickled, los yog txias - kos tiav. Yuav tsum tau ua kom du, polished nto kom tau raws li cov qauv kev tu cev; feem ntau 2B lossis ci ntsa iab.
Kev xeem yuav tsum tau Standard mechanical thiab flattening xeem. Xws li kev ntsuam xyuas hydrostatic nruj, qhov ntev kam rau ua, thiab xyuas qhov ua tiav.
Tolerance & Ncaj General industrial kam rau ua. Tight tolerances rau txoj kab uas hla, phab ntsa thickness, thiab straightness kom huv si ua raws.
Kev ntsuas siab Haum rau nruab nrab - cov ntawv thov siab nyob ntawm phab ntsa thickness. Kev sim tshwj xeeb rau siab - siab huv cov kav dej.

 

Dab tsi yog qhov txawv ntawm qhov ntsuas siab ntawm A269 thiab A270 raj?

Tsis muaj qhov sib txawv ntawm qhov ntsuas siab ntawm A269 thiab A270 raj, vim tias ob qho tib si tshwj xeeb npog cov raj siab rau kev xeb dav dav - kev pabcuam tiv thaiv. Kev ntsuas siab yog txiav txim siab los ntawm cov khoom siv (piv txwv li, qib, tensile lub zog) thiab lub raj qhov ntev (inch thiab phab ntsa thickness), tsis yog tus qauv ASTM nws tus kheej. Rau tib cov khoom thiab qhov ntev, qhov ntsuas siab yuav zoo ib yam rau ob qho kev qhia tshwj xeeb.

Xa kev nug