ASTM A269 TP.36L POLISHED Stainless Hlau Welded Tube

Oct 11, 2025

Tso lus

ASTM A269 cov tseev kom muaj rau seamless thiab welded ustenitic stainless hlau yeeb nkab thiab feem ntau siv nyob rau hauv cov kav dej thiab kav dej caw.


Peb ASTM A269 TP316L yog qhov qis- cov roj hmab welded stainless hlau yeeb yam thiab siab {}} qhov kev thov kub. Nws muaj zoo heev corrosion tsis kam, tshwj xeeb hauv chloride ib puag ncig. Nws yog qhov haum rau kev siv hauv kev lag luam xws li tshuaj lom neeg, chaw muag tshuaj, thiab cov tubrog nkoj, tab sis yuav tsis muaj kev tiv thaiv zoo ib yam li cov yeeb nkab. POLISHING yog muaj los txhim kho kom zoo nkauj thiab tsos. Cov yeeb nkab yog polished sab hauv thiab / lossis sab nraud siv cov plua plav lossis txhuam kom ua tiav cov khoom noj, 2420g, 320g, 320g, 320g, 320g, uas yog cov khoom noj khoom haus, tshuaj ntsuab, thiab cov ntawv thov kho mob.

 

ASTM A269 TP316L Stainless Steel Tube Polish Finishing 320 Grit

 

Nto tas (Polish)

Qib polish yog qhov tseem ceeb thiab feem ntau yog teev los ntawm tus neeg siv. Nws yog ntsuas ntawm grit (piv txwv li, 180g) lossis los ntawm roughness nruab nrab (ra) hauv microinchches (μm) lossis micrometers (μm).

Grit tiav Raug RA Tus Nqi Daim ntawv thov
#4 / 180G < 0.8 µm / 32 µin Cov Ntawv Thov Huv Si, Architectural
#4L / 240G < 0.5 µm / 20 µin Mis nyuj, ua zaub mov noj, brewing
#7 / 320G < 0.4 µm / 15 µin Kws muag tshuaj, kom hniav zoo nkauj, siab - purity
# 8 daim iav < 0.3 µm / 10 µin Semiconductor, ultra - kev purity siab (UHP)


Tshuaj Muaj Tshuajntawm ASTM A269 TP316L Polished Stainless Hlau Welded Tube

Teem nqi C Mn Si P S Cr Mo Ni Zaum fe
Ss 316l 0.035 Max 2.0 max 1.0 max 0.045 Max 0.030 max 16.00 - 18.00 2.00 - 3.00 10.00 - 14.00 68.89 min

 

Cov Khoom Siv Lub Cevntawm ASTM A269 TP316L Polished Stainless Hlau Welded Tube


Teem nqi

Ceev
(kg / m3)

Elastic modulus
(GPA)
Lub ntsiab lus co - eff ntawm thermal expansion (μm / M / Degree) Thermal conductivity
(W/m.K)

Kev kub kub tshwj xeeb 0-100 degree
(J / KG.K)

Elec resistivity
(nΩ.m)
0-100 Qib 0-315 Qib 0-538 Qib Ntawm 100 degree Ntawm 500 degree
316/L/H 8000 193 15.9 16.2 17.5 16.3 21.5 500 740

 

Txawv los ntawm kev sib xws
TPP36L: piv rau ASTM A213, A213 npog Seamless Tubing feem ntau rau boiler, siab} kub, siab} siab} qhov kev pab kub). A269 yog npaj rau "cov kev pab dav dav," suav nrog kev pab cuam siab, tab sis kuj tsom rau corrosion tsis kam.
TPP36L: piv rau ASTM A249, A249 npog welded welded welded welded welded welded welded, thiab pauv kev hloov cua sov. Nws muaj cov kev ntsuam xyuas nruj dua rau Weld Kev Ncaj Ncees thiab High {{} kev pab cuam siab dua li A269.

 

Yog tias koj muaj lub phiaj xwm xav tau rau 316 stainless tus me nyuam ci analaled tubing, peb zoo siab txais tos koj daim ntawv xaj. Gnee muaj cov khoom lag luam loj ntawm cov khoom nrov rau koj xaiv los ntawm. Peb muab cov qauv khoom siv cov tswv yim zoo, suav nrog kev ua tsis taus thiab welded. Txhawm rau kom ntxaws tshuaj muaj pes tsawg leeg tshuaj thiab kuaj dawb, thov hu rau peb lub Hoobkas niaj hnub no. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev. Email:sales@gneestainless.com

316 stainless steel bright annealed tubing

 