ASTM A269 TP316 Stainless Hlau Pickled thiab Annealed Tube
May 19, 2026
Tso lus
GNEE yog tus kws tshaj lij ntawm ASTM A269 TP316 stainless hlau pickled thiab annealed hlab, nrog 18 xyoo ntawm kev xa tawm ua haujlwm rau ntau tshaj 70 lub teb chaws thoob ntiaj teb, tau ntawv pov thawj los ntawm ISO 9001, thiab muab Daim Ntawv Pov Thawj Mill Test (MTC) thiab 100% tsis yog -Tebchaws qhia txog kev puas tsuaj.
TP316 tubing muaj 2.0-3.0% molybdenum (Mo), txhim khu kev tiv thaiv chloride pitting thiab crevice corrosion. Tom qab cov tshuaj annealing kev kho mob (1040-1150℃dej quenching), kev ntxhov siab raug tshem tawm, cov qauv austenitic ruaj khov, thiab intergranular corrosion tiv thaiv, ua kom ntev - lub sij hawm seem stability thiab toughness thaum lub sij hawm kev pab cuam. Pickling tshem tawm cov nplai oxide nto thiab kub- ua haujlwm seem, tsim cov xim matte grey-dawb tiav, uas tsis tsuas yog txhim kho corrosion kuj tab sis kuj muab lub hauv paus zoo rau kev polishing tom ntej lossis txheej.


ASTM A269 TP316 stainless hlau pickled thiab annealed hlab muaj xws li ob leeg seamless thiab welded hlab. SS 316 seamless raj tuaj yeem tiv taus siab txog 42 MPa thiab ua haujlwm ntawm qhov kub ntawm -200℃txog 815 degree, ua rau lawv siv dav hauv siab -siab thiab siab -kub siv, nuclear fais fab, roj & roj systems, corrosive chemical pipelines, thiab high purity purity pipelines, high corrosive purity pipelines, thiab high-corrosive purity pipelines. TP316 stainless hlau welded raj tuaj yeem tiv taus siab txog li 16 MPa thiab tsim nyog rau lub sijhawm ntev - qhov kev pabcuam kub tsawg dua lossis sib npaug li 550℃. Lawv tuaj yeem tsim tau rau hauv loj- txoj kab uas hla nyias- phab ntsa tubing thiab dav siv nyob rau hauv lub plhaub- thiab - raj kub exchangers, zaub mov thiab kws tshuaj nruab nrab / qis-siab tsheb thauj mus los, ib puag ncig desulfurization cov khoom, thiab dav siv dej thauj mus los pipelines.
ASTM A269 TP316 Stainless hlau yeeb nkab Chemical Composition
| Qib | C | Mn | P | S | Si | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| 316 | 0.08 | 2.00 | 0.045 | 0.030 | 1.0 | 11-14 | 16-18 | 2-3 |
| 316L | 0.035 | 2.00 | 0.045 | 0.030 | 1.0 | 10-14 | 16-18 | 2-3 |
ASTM A269 TP316 round raj Mechanical Properties
| Qib | Tensile zog (Mpa) | Yield Point (Mpa) | Elongation (%) | Elongation (%) |
|---|---|---|---|---|
| 316L | 485 | 170 | 35 | 25 |
| 316 | 515 | 205 | 35 | 25 |
ASTM A269 TP316 Stainless Hlau Tubing Dimension Tolerances
| OD, hauv. [mm] | Phab ntsa thickness kam rau ua, hauv. [mm] | Phab ntsa thickness totlerance, nyob rau hauv. [mm] | Ntev, hauv. [mm] |
|---|---|---|---|
| Txog li 1⁄2 [13] | ±0.005 [0.13] | ±15 | Phab ntsa thickness kam rau ua, hauv. [mm] |
| 1⁄2–11⁄2 [13–38], excl | ±0.005 [0.13] | ±10 | +1⁄8 [3.2] |
| 11⁄2 txog 31⁄2 [38–89], excl | ±0.010 [0.25] | ±10 | +3⁄16 [4.8] |
| 31⁄2 txog 51⁄2 [89–140], excl | ±0.015 [0.38] | ±10 | +3⁄16 [4.8] |
| 51⁄2 txog 8 [140–203], excl | ±0.030 [0.76] | ±10 | +3⁄16 [4.8] |
| 8-12 [203-305], ib | ±0.040 [1.01] | ±10 | +3⁄16 [4.8] |
| 12-14 [305-356], ib | ±0.050 [1.26] | ±10 | +3⁄16 [4.8] |
Dab tsi yog qhov txawv ntawm TP316 thiab TP316L stainless hlau kav?
Cov tub ntxhais sib txawv ntawm TP316 thiab TP316L stainless hlau kav yog nyob rau hauv lawv cov ntsiab lus carbon thiab weldability. TP316 muaj cov ntsiab lus carbon tsawg dua lossis sib npaug li 0.08%, thaum TP316L muaj cov ntsiab lus carbon tsawg dua lossis sib npaug li 0.03%. Thaum welding 316 stainless hlau kav ntawm qhov kub siab (800℃F ~ 1575℃F), carbon yooj yim ua ke nrog chromium thiab precipitates, ua rau txo qis corrosion kuj ntawm weld ntug. Lub ultra- qis carbon TP316L txo qhov kev pheej hmoo no.
TP316 Stainless Hlau Pickled thiab Annealed Tube Daim Ntawv Thov
Tshuaj thiab Petrochemical Industries: Reactors, heat exchangers, thiab piping systems resistant to acids, alkalis, and high -temperature media.
Lub Zog Hluav Taws Xob: Lub siab tseem ceeb- cov khoom muaj nyob rau hauv boilers, nuclear fais fab nroj tsuag, thiab cov khoom siv roj flue desulfurization.
Environmental Engineering: Chlorine -cov kav dej tiv taus hauv dej hiav txwv desalination thiab cov dej khib nyiab.
Cov ntaub ntawv nug:
Txuj: ASTM A269
Khoom siv: TP316 (los yog 316L)
Hom: Seamless lossis Welded
Specifications: Outer Diameter (OD) x Phab Ntsa Thickness (WT) (xws li 1/2" x 0.049")
Nto tiav: Pickled & Annealed
Length: Tsau ntev lossis Random ntev
Ntau
Yog tias koj xav tau cov lus qhia txog kev tiv thaiv corrosion nyob rau hauv cov kev ntsuas tshwj xeeb lossis ib puag ncig tshwj xeeb, thov hu rau peb!
Kev xeem thiab kev ua tau zoo
Kev Ntsuas Hardness: Rockwell hardness (feem ntau yuav tsum tsawg dua lossis sib npaug rau 90 HRB lossis 192 HV).
Flaring Test: Ua kom cov yeeb nkab kawg tuaj yeem flared yam tsis muaj cracking.
Flattening Test: Txheeb xyuas cov khoom yas thiab vuam zoo (rau cov kav dej welded).
Hydrostatic Testing los yog Eddy Current Testing (NDT): 100% yuav tsum xeem dhau tsis yog -kev sim ua kom puas tsuaj kom ntseeg tau tias cov yeeb nkab phab ntsa tsis muaj dej los yog tawg.


High - ntim zoo
Standard 316 yeeb nkab qhov ntau thiab tsawg (piv txwv li, OD 6.35-25.4mm) muaj rau kev xa khoom tam sim hauv 3-7 hnub. Customized xaj feem ntau xav tau 25-45 hnub ua haujlwm. Ntim nruj me ntsis raws li cov qauv kev xa tawm: PE plua plav kaus mom raug ntxiv rau hauv cov yeeb nkab kawg, txhua lub yeeb nkab yog ib lub hnab ntim los tiv thaiv khawb, thiab txheej txheej txheej yog thickened, fumigation-free ntoo crate los yog hexagonal bundles reinforced nrog waterproof ntaub los xyuas kom meej xoom oxidation thiab xoom deformation ntawm cov ntaub ntawv thaum lub sij hawm ntev kev thauj mus los hauv hiav txwv.