ASTM A269 yeeb nkab Specification.pdf
Nov 12, 2025
Tso lus
ASTM A269 tus qauv yog dab tsi?
ASTM A269 yog tus qauv tshwj xeeb rau seamless thiab welded austenitic stainless hlau tubing siv rau kev pabcuam dav dav hauv qis lossis siab - qhov kub thiab txias. Nws suav nrog ntau qib, xws li TP304, TP304L, TP316, thiab TP316L, txhais lawv cov tshuaj muaj pes tsawg leeg thiab cov khoom siv kho tshuab xws li tensile lub zog, yield zog, thiab hardness. Cov txheej txheem no tseem tswj hwm cov kev ntsuas tshwj xeeb kom ntseeg tau tias cov tubing ua tau raws li qhov yuav tsum tau muaj rau kev tiv thaiv corrosion thiab lwm yam kev siv.
ASTM A269 sib npaug li cas?
ASTM A-269 thiab nws qhov sib npaug ASME, DIN & EN Standard. 202, 304, 304L, 304H, 304LN, 309S, 310S, 316, 316L, 316H, 316Ti, 3216L, 316Ti, 316LN 347, 347H, 904L, SMO 254, ALLOY 254, 6MO, 6MOLY, UNS S31254 ETC.
ASTM A269 Tube Chemical Composition
| Stainless hlau Coil Tube | C | Mn | P | S | Si | Mo | Ni |
|---|---|---|---|---|---|---|---|
| TP 316 L | 0.035 | 2 | 0.045 | 0.03 | 1 | 2.0-3.0 | 10.0-14.0 |
| TIAB SA 304 | 0.08 | 2 | 0.045 | 0.03 | 1 | - | 8.0-11.0 |
| TIAB SA 316 | 0.08 | 2 | 0.045 | 0.03 | 1 | 2.0-3.0 | 11.0-14.0 |
| TP 304 L | 0.035 | 2 | 0.045 | 0.03 | 1 | - | 8.0-13.0 |
Lub zog ntawm ASTM A269 yog dab tsi?
Lub zog tawm los tau teev tseg hauv ASTM A269 txawv nyob ntawm qib tshwj xeeb. Cov qib sib xws xws li TP304 thiab TP316 muaj qhov tsawg kawg nkaus lub zog ntawm 30 ksi (205 MPa), thaum TP304L thiab TP316L muaj qhov tsawg kawg nkaus lub zog ntawm 25 ksi (170 MPa). ASTM A269 yog tus qauv rau stainless hlau tubing, yog li nws lub zog tawm los pes tsawg nyob ntawm cov khoom muaj pes tsawg leeg thiab cov txheej txheem kho cua sov.
| Khoom siv | Tensile zog | Yield zog | Elongation %, Min |
|---|---|---|---|
| Ksi (MPa), Min. | Ksi (MPa), Min. | ||
| TIAB SA 316 | 75(515) | 30(205) | 35 |
| TP 304 L | 70(485) | 25(170) | 35 |
| TP 316 L | 70(485) | 25(170) | 35 |
| TIAB SA 304 | 75(515) | 30(205) | 35 |
ASME SA269 SS Rhaub Tubes Nyhav Daim Ntawv Qhia
| Qhov hnyav / m (kg / m) | Loj (OD * WT) |
|---|---|
| 3.94 | 50.8 hli * 3mm |
| 2.21 | 38.1 hli * 2 hli |
| 0.77 | 19mm * 1mm |
| 1.37 | 25.4 hli * 1.5 hli |
| 0.103 | 6.35 hli * 0.25 hli |
| 0.32 | 12.7 hli * 0.5 hli |
| 0.27 | 10mm * 0.5 hli |
| 0.53 | 15.88mm * 0.75 hli |
ASTM A269 Kev Pom Zoo
| Kev kam rau siab% | NPS | |
|---|---|---|
| – | + | |
| 12.5 | 15.0 | 3~18,t/D>5% |
| 12.5 | 17.5 | Ntau tshaj los yog sib npaug rau 20, welded |
| 12.5 | 20.0 | 1/8-2 1 /2 |
| 12.5 | 22.5 | 3 ~ 18, t / D Tsawg dua lossis sib npaug li 5% |
| 12.5 | 15.0 | ≥ 20,smls,t/D>5% |
| 12.5 | 22.5 | Ntau dua lossis sib npaug li 20, smls, t / D Tsawg dua lossis sib npaug li 5% |
ASTM A269 Seamless Tube Thaum tshav kub kub kho
| Khoom siv | Kev kho cua sov | Qhov kub thiab txias º F (º C) |
|---|---|---|
| A269 316L | Kev daws | 1900(1040) |
| A269 304 | Kev daws | 1900 (1040) |
| A269 304L | Kev daws | 1900 (1040) |
| A269 316 | Kev daws | 1900(1040) |
ASTM A269 Kev ntsuas siab
ASTM A269 kev ntsuas siab tsis yog ib qho txiaj ntsig tab sis nyob ntawm cov khoom tshwj xeeb ntawm cov khoom siv yeeb nkab, xws li cov khoom siv qib (piv txwv li, 304L, 316), phab ntsa thickness, thiab sab nraud. Qhov siab tshaj plaws kev tso cai ua hauj lwm siab yog xam los ntawm cov mis P=2St/D, qhov twg St yog qhov tso cai kev nyuaj siab (xws li, 20,000 psi rau ntau qib ntawm chav tsev kub), t yog qhov tsawg kawg nkaus phab ntsa thickness, thiab D yog lub sab nraud txoj kab uas hla. Piv txwv li, ib qho kev ntsuas siab rau 304L stainless hlau yeeb nkab nrog ib txoj kab uas hla ntawm 3/4 nti thiab phab ntsa tuab ntawm 0.049 ntiv tes yog 2450 psi, nrog rau qhov kub ntawm -20 txog 100℃F.

Kev xeem rau ASTM A269 yog dab tsi?
Tubing yuav tsum raug kuaj los ntawm hydrostatic test los yog nondestructive electric test los kuaj xyuas cov dej xau los yog qhov tsis xws luag. Welded tubes yuav tsum tau tiv thaiv flanging yam tsis muaj cracking qhia weld kev ncaj ncees.
Dab tsi yog qhov txawv ntawm ASTM A269 thiab A249?
ASTM A249 yog rau welded austenitic steel raj siv nyob rau hauv cov ntawv thov tseem ceeb xws li boilers thiab tshav kub exchangers, yuav tsum tau ntau dua kev ntsuam xyuas thiab cov txheej txheem tsim tshwj xeeb. ASTM A269 npog ob qho tib si seamless thiab welded austenitic stainless hlau tubing rau kev pabcuam dav dav, yuav tsum muaj kev ntsuas kev siv tshuab tsawg dua.
Dab tsi yog qhov txawv ntawm ASTM A269 thiab A270?
Qhov sib txawv tseem ceeb yog tias ASTM A270 yog rau cov kav dej huv, tsom mus rau qhov zoo nkauj sab hauv ua tiav rau cov ntawv thov xws li cov khoom noj thiab tshuaj, thaum ASTM A269 yog rau kev siv dav hauv -lub hom phiaj, corrosion- tawm tsam tubing nrog tsawg dua qhov yuav tsum tau ua kom tiav.
Xa kev nug