ASTM A213 TP321H Stainless Hlau Seamless Yeeb Nkab

Jan 27, 2026

Tso lus

ASTM A213 TP321H yog dab tsi?

ASTM A213 TP321H yog qhov siab -carbon titanium-stabilized austenitic stainless hlau seamless yeeb nkab, optimized rau siab -kub creep zog. Nws yog tshwj xeeb yog siv nyob rau hauv siab - kub, siab - kev nyuaj siab boiler raj thiab superheater Cheebtsam.

Qib sib npaug (Horizontal)

UNS: S32109|JIS: SUS321H|GB: 07Cr18Ni11Ti|EN: X7CrNiTi18-10|PIB: 1.4541

Chemical Composition (wt%, Kab rov tav)

C: 0.04-0.10|Si: Tsawg dua lossis sib npaug rau 1.00|Mn: Tsawg dua lossis sib npaug rau 2.00|P: Tsawg dua lossis sib npaug rau 0.045|S: Tsawg dua lossis sib npaug rau 0.030|Cr: 17.00-19.00 Nws Nws: 9.00-12.00|Ti: Ntau dua lossis sib npaug rau 5 × C|Fe: Sib npaug

Cov khoom tseem ceeb (20 degree, Annealed, Kab rov tav)

Qhov ceev: 7.93g / cm³|Melting Point: 1400-1450 degree|Tensile Strength: Ntau dua lossis sib npaug ntawm 515N / mm²|Yield Strength: Ntau dua lossis sib npaug rau 205N / mm²|Elongation: Ntau dua lossis sib npaug li 40%|Hardness: Tsawg dua los yog sib npaug rau 201HB

Cov yam ntxwv tseem ceeb

• Cov ntsiab lus ntawm cov pa roj carbon ntau txhim kho siab -kub creep lub zog, tswj kev ruaj ntseg hauv qab 600-870℃kev ntxhov siab • Titanium stabilization ua kom cov ncej zoo heev-weld intergranular corrosion kuj, sib piv siab -kub kev ua tau zoo • Yuav tsum tau ncej-weld annealing • Tsim nyog rau qhov siab tshaj 6} corrosion thiab kub siab high-temperature siab piping nyob rau hauv fais fab nroj tsuag thiab industrial boilers

TP321 vs TP321H kab rov tav

Cov ntsiab lus carbon: 321 (tsawg dua lossis sib npaug rau 0.08%)|321H (0.04-0.10%)|Creep Strength: 321 (Zoo)|321H (Zoo heev)|Annealing: 321 (Yeem)|321H (Yuav tsum tau)|Siab kub ntxhov siab: 321 (General)|321H (Resistant)

Qib C Mn Si P S Cr Mo Ni N Lwm yam
321 min.
max
-
0.08
2.00 0.75 0.045 0.030 17.0
19.0
- 9.0
12.0
0.10 Ti=5(C+N)
0.70
321H min.
max
0.04
0.10
2.00 0.75 0.045 0.030 17.0
19.0
- 9.0
12.0
- Ti=4(C+N)
0.70

 

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau cov phaj, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, lossis ntim raws li cov neeg siv khoom xav tau.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug