Tso lus

Yog tias koj tab tom nrhiav stainless hlau tubing muaj peev xwm ua haujlwm txuas ntxiv ntawm 800℃F thiab 1650℃F (427-900 degree)-tsis tas yuav tsum tau tshaj tawm-weld tov annealing thiab nrog zoo heev tiv thaiv intergranular corrosion-AISI 347 seamless tubing yog qhov kev xaiv zoo tshaj plaws rau kev siv tshuab steel hlau xws li stabilizing tshuab. siab -kub tshuaj piping, thiab kub exchangers. Los ntawm dual stabilization nrog Niobium (Nb) thiab Tantalum (Ta), nws tshem tawm tag nrho cov kev pheej hmoo ntawm nplej- ciam teb carbide nag lossis daus nyob rau hauv chromium-carbide nag lossis daus ntau (800-1500℃F) thaum muab siab tshaj -kub creep 15} zog thiab kev nyuaj siab{3.

 

AMS 5571 yog dab tsi?

AMS 5571 yog cov khoom siv dav hlau dav hlau uas tau tshaj tawm los ntawm SAE International npog seamless, corrosion- thiab tshav kub-resistant Hom 347 stainless hlau tubing (UNS S34700) hauv kev daws cov cua sov- kho mob.

 

Dab tsi yog 347 aerospace - qib seamless stainless hlau tubing?

AISI 347 aerospace-qib seamless stainless hlau tubing (UNS S34700) yog niobium-tantalum stabilized austenitic stainless hlau khoom tsim los ntawm kev tho thiab txias- kos duab lossis txias- dov txheej txheem, kom ntseeg tau tias tsis muaj cov ntsiab lus tsis muaj zog 6.} Nws muaj pes tsawg leeg-featuring 17–19% Cr, 9–13% Ni, thiab Nb Ntau dua lossis sib npaug rau 10 × C%- ua kom nws tswj tau cov qauv kev ncaj ncees thiab ua haujlwm rau intergranular corrosion nyob rau hauv qhov siab -kub ntau ntawm 800-1650} xws li siv dav hauv F. tso pa tawm manifolds, turbine kub- cov pa roj ducts, tshuaj superheaters, thiab nuclear - qib kub exchangers.

AMS 5571 347 aerospace-grade Stainless Steel tubing
AMS 5571 347 aerospace- qib Stainless hlau tubing
347 aerospace-grade  tubing
347 aerospace - qib tubing

 

AMS 5571 TP347 Stainless Hlau Tube Specification

Yam khoom

Piv txwv Specification

Khoom Qib

AISI 347 / UNS S34700 (los yog 347H / S34709)

Siv tau Standard

TIAB SA 5571

Sab nraud Diameter (OD)

1/2 "(12.7mm) ± 0.05 hli

Phab ntsa Thickness

0.065 "(1.65 hli) ± 5%

Ntev

6 m (20 ft) / Kev cai

Kev Xa Khoom

Annealed (Kev daws teeb meem Annealed)

Nto tiav

2B / Bright Annealed / puab Polished

Hom kawg

Plain End + Caps tiv thaiv

Ntau

500 kg

Kev soj ntsuam yuav tsum tau

EN 10204 3.2 + PMI + Eddy Current Testing (ET)

Daim ntawv pov thawj

MTC + Tus Kheej Tube ET Daim Ntawv Qhia + PMI Daim Ntawv Qhia

Ntim

Ntoo Cases + Moisture -Cov ntaub ntawv pov thawj + Yas End Caps + Cov ntawv lo

Cov ntsiab lus ua lag luam

FOB Shanghai / CIF Long Beach

Lub Sijhawm Lead

25-35 Hnub

Cov Kev Cai Tshwj Xeeb

NADCAP Certification / AS9100 / Aerospace Khoom Pom Zoo

 

info-688-201​

Kev sib piv tshuaj lom neeg: TP347 vs TP347H

Cr (Chromium)

17.0–19.0%

17.0–19.0%

17.0–19.0%

18.0–20.0%

Ni (Nickel)

9.0–13.0%

9.0–13.0%

9.0–12.0%

8.0–11.0%

Manganese (Mn)

Tsawg dua lossis sib npaug li 2.00%

Tsawg dua lossis sib npaug li 2.00%

Tsawg dua lossis sib npaug li 2.00%

Tsawg dua lossis sib npaug li 2.00%

Si (Silicon)

Tsawg dua lossis sib npaug li 1.00%

Tsawg dua lossis sib npaug li 1.00%

Tsawg dua lossis sib npaug li 1.00%

Tsawg dua lossis sib npaug li 1.00%

P (phosphorus)

Tsawg dua lossis sib npaug li 0.045%

Tsawg dua lossis sib npaug li 0.045%

Tsawg dua lossis sib npaug li 0.045%

Tsawg dua lossis sib npaug li 0.045%

S (Sulfur)

Tsawg dua lossis sib npaug li 0.030%

Tsawg dua lossis sib npaug li 0.030%

Tsawg dua lossis sib npaug li 0.030%

Tsawg dua lossis sib npaug li 0.030%

Nb (Niobium / Cb)

Ntau dua lossis sib npaug li 10 × C% thiab Ntau dua lossis sib npaug rau 1.00%

Ntau dua lossis sib npaug li 8 × C% thiab Ntau dua lossis sib npaug rau 1.00%

-

-

Titanium (zeeg)

-

-

Ntau dua lossis sib npaug li 5 × C% thiab Ntau dua lossis sib npaug rau 0.70%

-

Molybdenum (zeeg)

-

-

-

-

 

Aerospace-Qib Mechanical Properties By Tube Diameter (AMS 5571)

Nominal Sab Nraud Diameter (OD)

Nominal Phab Ntsa Thickness

Tensile Strength UTS (ksi)

Yield zog YS (ksi)

Elongation

Tsawg dua los yog sib npaug li 0.188 "

Tsawg dua los yog sib npaug rau 0.016 "

75-120 max

-

35%

Tsawg dua los yog sib npaug li 0.188 "

> 0.016"

75-105 max

30 feeb

35%

> 0.188"–0.500"

Tsawg dua los yog sib npaug rau 0.010 "

75-115 max

30 feeb

35%

> 0.188"–0.500"

> 0.010"

75-105 max

-

35%

> 0.500"

Tag nrho cov phab ntsa thicknesses

75-100 max

30 feeb

35%

 

info-702-213​

info-15-15

info-707-203​

Yuav ua li cas koj xam lub siab - bearing muaj peev xwm ntawm 347 piping?

Siv cov qauv ASME B31.3 (los yog B31.1):

Pressure-Bearing Capacity Of 347 Piping

P=Tsim siab
D=Sab nraud txoj kab uas hla
S=Tso cai rau kev ntxhov siab (saib ASME Tshooj II Tshooj D; rau 347 ntawm 800℃F, S ≈ 18,000 psi)
E=Joint yam (seamless yeeb nkab=1.0)
Y=Coefficient (= 0.4)

 

 

AMS 5571 347 aerospace- qib Stainless Steel tubing Applications

Cheebtsam / Qhov chaw

Muaj nuj nqi

Hom Dimensions

Siv tau Standard

Turbine Exhaust Manifold (Header)

Directs siab -kub tso pa roj

OD 1"-4"; Phab ntsa 0.065 "-0.120"

TIAB SA 5571

Cav Kub-Gas Tube

Cua txias / cua txias

OD 1/4"-1"; Phab ntsa 0.028 "-0.065"

TIAB SA 5571

APU Exhaust

Auxiliary power unit tso tawm

OD 2"-6"

AMS 5571 / MIL -T-8808

Roj cua sov kab

Tsawg-kub roj cua sov

OD 1/2 "- 1"

TIAB SA 5571

Expansion Joint / Bellows

Thermal expansion them nyiaj

Kev cai

Cov neeg siv khoom -Specialized

 

347 aerospace-qib tubing Nqe ib kg

Yam khoom

Tus nqi ntau (USD / kg)

Lus hais

304 Seamless Yeeb Nkab (Benchmark)

$3.50–$5.50

Nyob ntawm specifications thiab phab ntsa thickness

347 Seamless yeeb nkab

$5.00–$8.00

+30%–50% vs . 304

347H Seamless yeeb nkab

$5.50–$9.00

Me ntsis siab dua 347

321 Seamless Yeeb Nkab (Sib piv)

$4.50–$7.00

10% -20% qis dua 347

347 Aerospace Qib (AMS 5571)

$8.00–$15.00+

suav nrog NADCAP ntawv pov thawj + batch-los ntawm -batch test

Txhawm rau muab cov lus qhia meej dua rau koj, koj puas tuaj yeem muab cov ntaub ntawv hauv qab no?
Yuav tsum tau sab nraud txoj kab uas hla (OD) thiab phab ntsa thickness?
Kwv yees kom muaj nuj nqis (hauv kilograms lossis ko taw)?
Puas muaj tej yam tshwj xeeb ntawm aerospace specifications lossis kev xeem (xws li, AMS cov qauv)?

Hu rau tam sim no

 

Dab tsi yog MOQ thiab Lub Sijhawm Lead rau 347 Stainless Hlau Tubes?

Yam khoom

Hom kab mob

MOQ (Kev Lag Luam Qib)

500 kg-1 tuj

MOQ (Aerospace Qib, AMS 5571)

100-500 kg

Lub Sijhawm Lead (Standard Sizes, In Stock)

7-15 hnub

Lub Sijhawm Lead (Custom Size)

25-45 hnub

Lub Sijhawm Lead (Aerospace Qib + Kev Ntsuas Tus Kheej Tube)

30-60 hnub

Kev pom zoo:Muab qhov kev txiav txim rau aerospace tej yaam num 3-4 lub hlis ua ntej, raws li ntau lawm muaj peev xwm rau AMS 5571 tubing yog txwv thiab ib tug neeg eddy-tam sim no xeem yog lub sij hawm-siv.

 

Peb muab cov qauv dawb (1-2 daim, Tsawg dua lossis sib npaug li 1 m) nrog cov khoom thauj.
Aerospace- cov qauv qib yuav tsum tau muab los ntawm cov ntawv pov thawj cua sov; cov khoom seem tsis tso cai.
Kev Tswj Xyuas Zoo:
PMI (kev txheeb xyuas cov ntsiab lus Nb)
Tensile xeem (UTS/YS/El)
Eddy tam sim no kuaj (sab hauv tsis xws luag)
Metallographic kuaj (tag nrho austenitic, tsis muaj delta ferrite)
Dimensional soj ntsuam (OD, phab ntsa thickness, ovality)

Flaring test
Flaring xeem
Eddy current testing
Eddy kev sim tam sim no
347 Pipe PMI
347 Pipa PMI
 

Ntim rau 347 Stainless Hlau Yeeb Nkab

Kev tiv thaiv dej noo: Desiccant thiab noo noo-cov ntaub ntawv pov thawj hauv cov thawv ntoo (tshwj xeeb tshaj yog rau cov khoom xa tuaj hauv hiav txwv tshaj 30 hnub)
Kev tiv thaiv deformation: yas tiv thaiv lub kaus mom ntawm cov yeeb nkab kawg kom tiv thaiv kev puas tsuaj
Kos npe: Txhua lub yeeb nkab / nras cim nrog: Khoom siv (347 / 347H); Txuj (AMS 5571); Batch No. / Kub No.; OD × Phab ntsa × Ntev; Quantity / Nyhav

Packaging For 347 Stainless Steel Pipe

 

FAQ

Qhov txawv ntawm 347 thiab 347H Stainless hlau yog dab tsi?

Cov tub ntxhais sib txawv ntawm 347 thiab 347H stainless hlau yog lawv cov ntsiab lus carbon. Tsab ntawv "H" sawv cev rau "High Carbon," thiab cov pa roj carbon ntau dua hauv 347H muab kev txhim kho siab - qhov kub thiab txias tsis kam, ua rau nws tsim nyog rau lub sijhawm ntev ntawm qhov kub siab.

Qhov tseem ceeb Parameter sib piv

Khoom / Parameter 347 AWS 34700 347H (UNS S34709) UA
Cov ntsiab lus carbon Qhov siab tshaj plaws 0.08% (tsawg dua lossis sib npaug rau 0.08%) 0.04–0.10%
Siab -Temperature Strength & Creep Resistance Haum rau kev ua haujlwm siab - kub Siab dua, tshwj xeeb tshaj yog siab dua 538℃(1000℃F)

 

Dab tsi yog qhov kev ua haujlwm kub ntawm 347 stainless hlau yeeb nkab?

Qhov xwm txheej Qhov kub thiab txias
Kev pabcuam txuas ntxiv (pom zoo) -425 ° F txog 1650 ° F (-250 ° txog 900 ° F)
Cov cua sov tsis sib xws Mus txog 1650℃F (900 degree)
ASME B31.1 pom zoo (347H) 347H yog nyiam tshaj 800℃F (427 degree)
Tshaj 900℃(1650℃F) Tsis pom zoo; xav txog 310S / Inconel 600
Tsawg-kev pabcuam kub (< -425°F / -250°C) Kev ntsuam xyuas cuam tshuam yog xav tau rau kev kuaj xyuas

 

347 puas tuaj yeem hloov 321?

Nws tuaj yeem siv los hloov pauv hauv qee qhov xwm txheej, tab sis lawv tsis tuaj yeem hloov pauv dawb. Qhov sib txawv tseem ceeb yog tias 347 muaj qhov zoo tshaj qhov siab tshaj -kub creep thiab kev ntxhov siab- tawg cov khoom piv rau 321; Hauv cov dej num hauv aerospace, txawm li cas los xij, 347 thiab 321 tsis hloov pauv tau, thiab cov kev qhia tshwj xeeb uas tau txib los ntawm OEM (tshwj xeeb yog AMS cov qauv) yuav tsum ua raws li nruj me ntsis.

Xa kev nug