Cov khoom tseem ceeb
Cov yam ntxwv tseem ceeb ntawm Stainless Steel-Qib 347 yog tabulated hauv qab no.
Table 1.Cov khoom tseem ceeb
| Cov khoom hluav taws xob | |
|---|---|
| Hluav taws xob tiv taus (µOhm.cm) | 70-73 |
| Mechanical Properties | |
| Elongation ntawm tawg (%) | <60 |
| Hardness - Brinell | 160-190 |
| Izod cuam tshuam lub zog (Jm-1 ) | 20-136 |
| Modulus ntawm elasticity (GPa) | 190-210 |
| Tensile zog (MPa) | 520-1100 |
| Lub cev muaj zog | |
| Qhov ceev (g.cm-3 ) | 7.93 |
| Melting point (° C) | 1400-1425 |
| Thermal Properties | |
| Coefficient ntawm thermal expansion (x10-6 K-1 ) | 16-18 @ 20-100 ° C |
| Kev siv siab tshaj plaws hauv huab cua (°C) | 800 |