904L vs . 316L Stainless Hlau Tubes: Daim ntawv thov
Thaum 316L txaus rau kev siv dej hiav txwv dav dav thiab kev pabcuam tshuaj lom neeg, 904L yuav tsum tau thaum cov cuab yeej ntsib kev ua phem kom txo cov kua qaub los yog ntev -lub sij hawm ruaj khov hauv kub, chloride- cov xov xwm nplua nuj, ua pov thawj nws cov nqi pib siab dua los ntawm kev ncua lub neej thiab txo kev txij nkawm.

Dab tsi yog cov ntawv thov rau 904L stainless hlau kav?
Kev Lag Luam Kev Lag Luam: Siv rau hauv ib puag ncig uas xav tau cov kua qaub siab (xws li sulfuric acid, phosphoric acid, acetic acid), nrog rau kev tsim cov khoom siv tshuaj.
Kev Lag Luam Roj thiab Roj: Siv rau hauv cov kav dej hauv qab dej hiav txwv thiab cov khoom siv hluav taws xob hauv qab.
Marine thiab Seawater Environments: Siv nyob rau hauv seawater txias systems, desalination nroj tsuag, thiab tshav kub exchangers.
Kev Tiv Thaiv Kev Ua Phem: Siv rau hauv Flue Gas Desulfurization (FGD) systems.
Pulp thiab Ntawv Kev Lag Luam: Siv rau hauv cov khoom siv tshuaj dawb thiab cov tank cia.
316 stainless hlau kav siv nyob qhov twg?
Marine and Coastal Environments: Feem ntau siv rau marine fittings, seawater piping, thiab structural Cheebtsam nyob rau hauv offshore cheeb tsam.
Chemical thiab Petrochemical Processing: Siv nyob rau hauv cov hlab ntsha siab, tshav kub exchangers, thiab tshuaj cia tank.
Khoom noj khoom haus, dej haus, thiab tshuaj: nquag siv nyob rau hauv cov kav dej huv si, khoom noj khoom haus, thiab brewing ntau lawm kab.
Kev Kho Mob thiab Pharmaceutical Sectors: Siv rau hauv tsev kho mob piping infrastructure, cov khoom siv tshuaj, thiab cov chaw tsim khoom.
Kev Kho Dej thiab Pulp & Paper Industries: Siv nyob rau hauv ntau lub tshuab lim thiab cov chaw kho dej khib nyiab.

904L vs . 316L Stainless Hlau Tubes: Kev sib piv tshuaj lom neeg (%)
| Element | 316L (UAS S31603) | 904 L (UNS N08904) NPE |
| Chromium (Cr) | 16.0 – 18.0 | 19.0 – 23.0 |
| Nickel (Ni) | 10.0 – 14.0 | 23.0 – 28.0 |
| Molybdenum (hli) | 2.0 – 3.0 | 4.0 – 5.0 |
| Copper (Cu) | - | 1.0 – 2.0 |
| Cov pa roj carbon (C) | Tsawg dua lossis sib npaug li 0.030 | Tsawg dua lossis sib npaug li 0.020 |
| Nitrogen (N) | Tsawg dua lossis sib npaug li 0.10 | Tsawg dua lossis sib npaug li 0.10 |

904L vs . 316L Stainless Hlau Tubes: Mechanical & Physical Properties
| Khoom | 316L Stainless hlau | 904L Stainless hlau |
| Tensile zog (min) | 485 MPa (70 ksi) | 490 MPa (71 ksi) |
| Yield zog (min) | 170 MPa (25 ksi) | 220 MPa (31 ksi) |
| Elongation (min) | 40% | 35% |
| Hardness (max) | 95 PAB | 90 PAB |
| PREN (Pitting Resistance) | 24-26 (Nyob nruab nrab) | 34-36 (siab) |
| Magnetism | Tsis yog-magnetic (Standard) | Tsis yog -magnetic (Highly Stable) |
| Qhov ntom | 8.0 g / cm³ | 7.95 g / cm³ |
904L vs . 316L Stainless Hlau Tubes: Corrosion Resistance
Muab piv rau 316L stainless hlau, 904L stainless hlau tubing nthuav tawm cov kev tiv thaiv corrosion zoo tshaj - qhov zoo tshaj plaws los ntawm nws cov molybdenum siab dua (4%–5%) thiab cov ntsiab lus tooj liab-tshwj xeeb tshaj yog nyob rau hauv cov kua qaub uas muaj zog (xws li sulfuric acid) thiab chloride- thaj chaw nplua nuj (seawater). Thaum 316L yog qhov tsim nyog rau kev siv dej hiav txwv lossis tshuaj lom neeg, 904L-ua tsaug rau nws cov ntsiab lus nickel siab dua (nce txog 25%)- tiv thaiv pitting corrosion thiab kev ntxhov siab corrosion tawg hauv qhov hnyav, siab - kub, lossis acidic ua haujlwm ib puag ncig.

904L vs . 316L Stainless Hlau Tubes: Nqe
904L stainless hlau raj yog kim kim tshaj li 316L, feem ntau raug nqi 60% mus rau 80% ntau dua, lossis nruab nrab ntawm 1.5 mus rau 3 npaug ntawm tus nqi ib kg. Raws li thaum ntxov 2026, 904L tus nqi yog kwv yees li ntawm $ 11- $ 19 USD / kg, uas tau tsav los ntawm nickel siab (23-28%) thiab molybdenum (4-5%) cov ntsiab lus rau superior corrosion kuj.

| Lub hli | SS 904L Seamless | SS 904L welded yeeb nkab | SS 316L Seamless | SS 316L welded yeeb nkab | ||||
|---|---|---|---|---|---|---|---|---|
| USD/kg | CNY/kg | USD/kg | CNY/kg | USD/kg | CNY/kg | USD/kg | CNY/kg | |
| Peb Hlis 2026 | $8.50 | ¥61.20 | $6.20 | ¥44.64 | $3.20 | ¥23.04 | $2.60 | ¥18.72 |
| Peb 2026 | $8.80 | ¥63.36 | $6.40 | ¥46.08 | $3.30 | ¥23.76 | $2.65 | ¥19.08 |
| Peb Hlis 2026 | $9.20 | ¥66.24 | $6.70 | ¥48.24 | $3.40 | ¥24.48 | $2.75 | ¥19.80 |
| Plaub Hlis 2026 | $9.50 | ¥68.40 | $6.90 | ¥49.68 | $3.50 | ¥25.20 | $2.85 | ¥20.52 |
| Hloov | ↑ +$1.00 | ↑ +¥7.20 | ↑ +$0.70 | ↑ +¥5.04 | ↑ +$0.30 | ↑ +¥2.16 | ↑ +$0.25 | ↑ +¥1.80 |
Yog tias koj muaj qhov project-cov kev cai tshwj xeeb rau 316L lossis 904L stainless hlau raj, peb txais tos koj xaj. GNEE khaws cov ntaub ntawv tseem ceeb ntawm peb qhov zoo tshaj plaws - muag khoom rau koj xaiv. Cov ntaub ntawv no muaj nyob rau hauv ob qho tib si seamless thiab welded daim ntawv. Rau cov ncauj lus kom ntxaws chemical muaj pes tsawg leeg specifications lossis thov cov qauv dawb, thov hu rau peb lub Hoobkas tam sim. Peb muab cov nqi sib tw thiab kev pabcuam tshwj xeeb.
Peb cov khoom tau ntim khoom siv cov ntawv tsis muaj dej tsis zoo thiab cov hlua khi hlau, ua raws li cov txheej txheem ntim khoom xa tuaj rau kev thauj mus los thiab tsim nyog rau ntau txoj kev xa khoom; Hloov chaw, ntim tuaj yeem kho raws li cov neeg siv khoom tshwj xeeb.
Ntim
Txheem Export Ntim rau Stainless Hlau Phaj
1. Polished nto tiav; 2. Ntim ntim;
3. Ntoo crate ntim; Ntoo pallet ntim;
4. Thawv lossis bulk cargo shipping; 5. Customized raws li tus neeg yuav tsum tau muaj.


Xa kev nug