440C vs 440B Stainless Hlau: Siab - Hardness Martensitic qib

Aug 05, 2025

Tso lus

SS440CSS440CSS440C

 

Lawv cov khoom sib txawv li cas?

440B muaj 16-18% chromium, 0.75-0.95% carbon, thiab 0.4.6% molybdenum rau 0.4.7%, ua kom muaj kev nyuaj siab dua tom qab kev kho cua sov.

 

Qhov twg muaj cov hardness zoo dua thiab hnav tsis kam?

440C ncav cuag 58 {- 60 hrc tom qab kev kho cua sov, nyuaj tshaj 440b's 56 {{}} 58 hrc. Qhov no ua rau 440c ntau cov hnav-resistant, zoo tagnrho rau cov khoom siv ceev thiab txiav cov cuab yeej xav tau kom tswj cov npoo ntse.

 

Yuav ua li cas lawv sib piv hauv corrosion tsis kam?

Ob qho tib si muab cov kev ua kom zoo sib xws hauv cov chaw qhuav, nrog chromium tsim ib txheej oxide txheej. Lawv tiv thaiv xeb hauv cov chaw nyob sab hauv tab sis kuj corrode hauv noo noo los yog ntsev, uas tsis muaj qhov sib txawv ntawm lawv.

 

Dab tsi txog lawv cov khoom sib luag?

440B tau yooj yim me ntsis rau tshuab thiab txhuam dua 440C vim yog qis carbon. Ob qho tib si yuav tsum tau ua tib zoo saib xyuas kev ua kom sov (quenching thiab tempering) kom tsis txhob brittleness, nrog 440C xav tau kev tswj qhov kub thiab kub.

 

Muaj pes tsawg 440c thiab 440b feem ntau siv?

440B yog nyob rau hauv precision bearings thiab siab- zoo riam, thiab rooj zaum yuav tsum tau hnav tsis taus rau hauv kev sib txhuam.