430F Stainless Hlau: Tas Kom Xaj Pog
Jul 14, 2025
Tso lus



Muaj dab tsi tshwj xeeb txog 430F qhov muaj pes tsawg leeg?
Nws muaj 16-18 Chromium, zoo li 430, tab sis ntxiv cov pa roj hmab (0,2% max) tswj hwm nws cov qauv ferritic.
Nws ua dab tsi hauv machines?
Qhov ntxiv ntawm cov leej faj tsim cov ntaub ntawv sulfide uas ua rau cov chips, txo cov cuab yeej hnav {} nws yooj yim dua tshaj qhov precision seem .
Yuav ua li cas hais txog corrosion tsis kam?
Me ntsis qis dua 430 vim yog leej faj, tab sis tseem tawm tsam xeb hauv cov huab cua qhuav thiab ib qho chaw me me} Tsis txhob haum rau cov teeb meem lossis chaw ntub dej.
Dab tsi yog nws cov cuab yeej ua haujlwm?
Muaj lub zog nruab nrab thiab lub hardness, zoo ib yam li 430 tab sis nrog me ntsis qis dua kev sib ntxiv vim yog cov khoom noj uas tsis muaj kev ntxhov siab rau cov tub rog tsis yog-{4}
Qhov twg yog 430f feem ntau siv?
Siv nyob rau hauv fasteners, li qub, thiab tsheb qhov twg yooj yim tshuab machineme tau tshaj corrosion siab tshaj plaws .
Xa kev nug