Q1: Dab tsi yog qhov txawv ntawm cov tshuaj muaj pes tsawg leeg ntawm 347 thiab 347H stainless hlau?
A:Lub ntsiab txawv yogcov ntsiab lus carbon.
347 muaj cov qauv carbon ntau ntawm0.04–0.08%, stabilized nrog niobium (Nb=10 × C - 1.00%) thiab tantalum.
347H yog qhov siab - carbon variant nrog cov pa roj carbon ntau0.04–0.10%, kuj niobium-tantalum stabilized kom tsis txhob rhiab heev.
Q2: Yuav ua li cas lawv siab -kub txhua yam khoom sib piv?
A:347H nthuav tawm qhov ua tau zoo tshaj - qhov kub thiab txias.
347H ntau dua cov ntsiab lus carbon boostscreep thiab rupture zogntawm qhov kub siab tshaj 550 degree, ua kom ntev - kev pab cuam nyob rau hauv cov cua sov thiab thauj khoom.
347 muaj qhov zoo oxidation tsis kam tab sis qis cov qauv kev ruaj ntseg dua 347H thaum raug kub siab rau lub sijhawm ntev.
Q3: Puas yog 347 thiab 347H puas muaj qhov sib txawv intergranular corrosion tsis kam?
A:Yog lawm, ob qib sib qhia zoo heev intergranular corrosion kuj ntawm tib lub tshuab.
Niobium thiab tantalum nyob rau hauv ob qib reacts nrog carbon los tsim cov carbide ruaj khov, tiv thaiv chromium carbide nag lossis daus ntawm grain ciam teb thaum vuam los yog siab - kub raug.
Tsis muaj qib twg yuav tsum tau tom qab-weld kho cua sov kom muaj kev tiv thaiv corrosion.
Q4: Qib twg zoo dua rau kev siv siab -kub siab ntawm lub nkoj?
A: 347Hyog qhov kev xaiv zoo tshaj plaws rau cov ntawv thov no.
Nws qhov kev txhim kho siab - qhov kub thiab txias ua tau raws li cov qauv zoo li ASME rau cov hlab ntsha siab ua haujlwm ntawm qhov kub siab.
347 yog qhov zoo dua rau kev xeb dav dav - tiv taus siv ntawm qhov kub nruab nrab (hauv qab 550℃).
Q5: Yuav ua li cas xaiv ntawm 347 thiab 347H rau kev siv tshuab?
A:Xaiv raws li kev ua haujlwm kub thiab kev pabcuam thauj khoom:
Xaiv347rau chemical processing tanks, pa manifolds, thiab cryogenic khoom (prioritizing corrosion kuj ntawm nruab nrab kub).
Xaiv347Hrau chav boiler superheaters, roj turbine Cheebtsam, thiab siab -kub kub exchangers (prioritizing ntev - lub sij hawm creep zog).