347 Stainless Steel Yeeb Nkab & Tube: Niobium-Tantalum Stabilized High-Temp Corrosion Resistant Piping

Jan 30, 2026

Tso lus

Dab tsi yog 347 Stainless Hlau Yeeb & Tube?

347 yog niobium-tantalum stabilized austenitic stainless hlau yeeb nkab, muab superior siab - kub stability thiab post-weld corrosion kuj piv rau titanium- cov qib ruaj khov, zoo tagnrho rau siab - kawg kev lag luam scenarios.

Qib sib npaug (Horizontal)

UNS: S34700|JIS: SUS347|GB: 06Cr18Ni11Nb|EN: X6CrNiNb18-10|Nr.: 1.4550

Chemical Composition (wt%, Kab rov tav)

C: Tsawg dua lossis sib npaug rau 0.08|Si: Tsawg dua lossis sib npaug rau 1.00|Mn: Tsawg dua lossis sib npaug rau 2.00|P: Tsawg dua lossis sib npaug rau 0.045|S: Tsawg dua lossis sib npaug rau 0.030|Cr: 17.00-19.00 Nws NOS: 9.00-13.00 Nws Nb + Ta: Ntau dua lossis sib npaug ntawm 10 × C|Fe: Sib npaug

Cov khoom tseem ceeb (20 degree, Annealed, Kab rov tav)

Qhov ceev: 7.93g / cm³|Melting Point: 1400-1450 degree|Tensile Strength: Ntau dua lossis sib npaug ntawm 515N / mm²|Yield Strength: Ntau dua lossis sib npaug rau 205N / mm²|Elongation: Ntau dua lossis sib npaug li 40%|Hardness: Tsawg dua los yog sib npaug rau 201HB

Cov yam ntxwv tseem ceeb

• Niobium-tantalum stabilization: Ua kom zoo dua siab -kub stability thiab post-weld corrosion resistance dua titanium-stabilized qib • Zoo heev siab -kub creep resistance: Haum rau ntev -kev pab cuam ntawm mus txog 900℃• Peb muaj peev xwm ua tau zoo heev degradation tom qab vuam, hloov mus rau complex high -kawg kav kav • High-kawg scenario mob siab rau: Siv nyob rau hauv nuclear fais fab nroj tsuag, siab - kub rauv thiab cov txheej txheem tseem ceeb pipelines

UNS No Qib C Si Mn P S Cr Mo Ni N Lwm yam
S34700 347 0.08 0.75 2.00 0.045 0.030 17.00/19.00 – 9.00/13.00 – Cb:10xC1.00

 

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau cov phaj, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, lossis ntim raws li cov neeg siv khoom xav tau.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips