347 Stainless Hlau: Niobium-Stabilized Siab-Tub Kub Weldable Qib

Dec 22, 2025

Tso lus

347 stainless hlau yog niobium (Nb) -stabilized austenitic stainless hlau. Nws siv niobium (10 × C% - 1.0%) los hloov titanium hauv 321 rau stabilization. Niobium ua ke nrog cov pa roj carbon monoxide tsim NbC, uas tseem tiv thaiv kev cuam tshuam ntawm intergranular. Piv nrog rau 321, nws muaj qhov zoo dua siab - qhov kub thiab txias thiab kev ua haujlwm vuam, thiab yog qhov tsim nyog rau cov khoom uas yuav tsum tau siv vuam ntau zaus.

info-750-750

Core Parameters

Chemical Composition (wt%): C Tsawg dua lossis sib npaug rau 0.08, Si Less dua lossis sib npaug rau 1.00, Mn Tsawg dua lossis sib npaug rau 2.00, P Tsawg dua lossis sib npaug rau 0.045, S Less dua lossis sib npaug rau 0.030, Cr=17.00-19.00, Ni=9.00-13.00, Nb{{7}, Nb,

Mechanical Properties (Annealed): Tensile Strength Ntau dua los yog sib npaug rau 520MPa, Yield Strength Ntau dua lossis sib npaug rau 205MPa, Elongation Ntau dua lossis sib npaug li 40%, Brinell Hardness Tsawg dua lossis sib npaug rau 201HB

Kev Pabcuam Kub: 400℃txog 870℃(kev pabcuam txuas ntxiv), mus txog 925℃rau luv-lub sijhawm pabcuam

Qib sib npaug: SUS347 (JIS), EN 1.4550 (EN), UNS S34700 (ASTM)

Kev Ua Haujlwm Zoo: Niobium stabilization muaj zog siab dua - kub stability dua titanium, muaj zog creep ntau dua 321 saum 600 degree; niobium tsis yooj yim rau hlawv tawm thaum lub sij hawm vuam, thiab cov weld corrosion kuj thiab lub zog yog ruaj khov dua; corrosion kuj zoo heev rau oxidizing acids (nitric acid, acetic acid); tsis muaj kev tshaj tawm -weld kev kho cua sov yuav tsum tau ua, uas ua kom yooj yim rau kev tsim khoom.

Tej kev siv: High-kub rauv cov raj thiab cov khoom siv hluav taws xob sib txuas, txuas txuas ntxiv ntawm siab- cov kav dej kub, nuclear fais fab nroj tsuag sab hauv (nrog rau cov hluav taws xob zoo o tuaj yeem tiv thaiv), aircraft cav tso cov kav dej, thiab nitric acid cia tanks.

info-750-750

Tswv yim Q&A

Q1: Dab tsi yog qhov txawv ntawm 347 thiab 321 stainless hlau? A1: 347 siv niobium rau stabilization, thaum 321 siv titanium. 347 welding kev ua tau zoo (niobium tsis yooj yim rau hlawv tawm) thiab siab dua - kub zog; 321 muaj tus nqi qis dua. Xaiv 347 rau cov khoom uas yuav tsum tau siv vuam ntau zaus thiab ntev - lub sij hawm siab - qhov kub thiab txias kev pab cuam, thiab 321 rau dav dav - kub los tiv thaiv - intergranular corrosion scenarios.

Q2: Dab tsi yuav tsum tau sau tseg hauv kev ua kom sov ntawm 347? A2: Kub ua hauj lwm kub yuav tsum tau tswj ntawm 1150-1260 degree, thiab ntev nyob rau hauv lub 700-900℃ntau yam yuav tsum tau zam los tiv thaiv sigma theem los nag thiab embrittlement; intermediate annealing (1050-1120 degree, txias ceev) yuav tsum tau thaum lub sij hawm txias ua hauj lwm kom rov qab toughness.

Q3: Puas yog 347 haum rau cov khoom siv hluav taws xob nuclear? A3: Yog. Nws muaj cov hluav taws xob zoo o tuaj yeem tiv taus thiab kev cuam tshuam ntawm intergranular corrosion, thiab tuaj yeem siv los ua cov khoom siv hluav taws xob hauv cov hluav taws xob nuclear reactors thiab cov tshuab hluav taws xob. Nws ua tau raws li cov qauv ntawm cov khoom siv nuclear (xws li ASME SA-213), thiab nws cov khoom siv kho tshuab thiab kev tiv thaiv corrosion yog ruaj khov tom qab irradiation.

info-750-750

Q4: Cov khoom siv vuam zoo li cas rau 347? A4: ER347 vuam hlau los yog E347-16 electrode yuav tsum tau xaiv, uas muaj tib yam niobium cov ntsiab lus raws li lub hauv paus hlau, kom ntseeg tau tias cov weld muaj tib yam stabilization nyhuv thiab high-temperature ua hauj lwm raws li lub hauv paus hlau. Tsis txhob siv cov khoom siv vuam yam tsis muaj niobium, uas yuav ua rau muaj kev cuam tshuam ntawm kev sib tsoo ntawm cov vuam.

Q5: Yuav ua li cas paub qhov txawv ntawm 347 thiab 321 stainless hlau los ntawm txoj kev yooj yim? A5: Kev tshuaj xyuas cov tshuaj muaj pes tsawg leeg yog qhov tseeb tshaj plaws-347 muaj 0.80-1.20% niobium, thaum 321 muaj 0.10-0.30% titanium. Nyob rau hauv cov nqe lus ntawm vuam kev ua tau zoo, 347 muaj tsawg weld porosity thiab zoo weld tsim dua 321 nyob rau hauv tib txoj kev vuam, thiab niobium tsis yooj yim rau hlawv tawm.

Xa kev nug