321 Stainless Hlau: Titanium-Stabilized Alloy rau siab-Tsuas siv Welded

Apr 14, 2026

Tso lus

Txheej txheem cej luam: 321 stainless hlau yog titanium-stabilized austenitic alloy, zoo ib yam li 304 tab sis nrog ntxiv titanium los tiv thaiv intergranular corrosion. Nws yog tsim los rau welded Cheebtsam thiab siab -kub kev pab cuam, tshem tawm qhov yuav tsum tau rau post-weld annealing.

Chemical Composition (wt%)Chromium (Cr): 17.0-19.0; Nickel (Ni): 9.0-12.0; Titanium (Ti): 5 × C rau 0.70; Carbon (C): Tsawg dua lossis sib npaug rau 0.08; Manganese (Mn): Tsawg dua lossis sib npaug li 2.00; Silicon (Si): Tsawg dua lossis sib npaug rau 1.00; Phosphorus (P): Tsawg dua lossis sib npaug rau 0.045; Sulfur (S): Tsawg dua lossis sib npaug rau 0.030; Hlau (Fe): Sib npaug.

Tej yam cuab yeej cuab tam (Annealed Condition): Tensile Strength: Ntau dua lossis sib npaug ntawm 515 MPa; Yield zog: Ntau dua lossis sib npaug ntawm 205 MPa; Elongation: Ntau dua lossis sib npaug li 40%; Hardness (Brinell): Tsawg dua lossis sib npaug rau 201 HB.

Core Zoo: Zoo heev intergranular corrosion kuj (titanium-stabilized); zoo oxidation tsis kam (kev pabcuam txuas mus txog 925 degree, cuam tshuam txog 900 degree); tsis muaj ncej-weld annealing xav tau; zoo weldability thiab formability.

Daim ntawv thov: Cov khoom siv hluav taws xob hauv chaw nres tsheb, cov khoom siv ua zaub mov, cov cuab yeej ua yeeb yaj kiab thiab yees duab kev lag luam, siab -cov cua kub cua txias, cov khoom siv welded hauv kev lag luam tshuaj thiab petrochemical, thiab cov khoom siv dav hlau.

Qib sib npaug: UNS S32100; EN 1.4541; JIS SUS321; GB/T 06Cr18Ni11 Ti.

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.