321 Stainless Hlau Kub Ua Haujlwm Txheej Txheem
Jan 29, 2026
Tso lus
1. Qhov zoo tshaj plaws kub ua hauj lwm kub rau 321 yog dab tsi? 1100-1250 degree; zam qis dua 925℃kom tsis txhob kub luv.
2. 321 puas tuaj yeem kub -forged? Yog, rau kev tsim cov khoom loj xws li li qub thiab flanges.
3. Yuav ua li cas txias 321 tom qab ua haujlwm kub? Cua txias yog txaus rau feem ntau daim ntaub ntawv; dej quenching rau cov khoom tseem ceeb.
4. Puas ua haujlwm kub puas cuam tshuam rau 321's titanium stabilization? Tsis yog, kev ua haujlwm kub zoo khaws cia titanium carbide tsim.
5. Dab tsi yog qhov luv luv ntawm 321? Brittleness los ntawm kev sib cais ntawm leej faj, zam los ntawm nyob saum 925 degree.



Xa kev nug