| Hom | Stainless hlau Sheet |
| Qib | 200 Series: 201/202 |
| 300 Series: 301/302/303/304/304 L/304 N/309/309 S/310/316/316 L/321/347 | |
| 400 Series: 403/408/409/410/416/420/430/431/440/440A/440B/440C/439/443/444 | |
| 600 Series: 610/620/630 | |
| 900 Series: 904L | |
| Thickness | 0.3-100 hli |
| Dav | 600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, thiab lwm yam |
| Ntev | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, thiab lwm yam |
| Nto | BA/2B/NO.1/NO.4/8K/HL |
| Kev xeem zoo | Peb tuaj yeem muab MTC, ISO, SGS, BV, thiab lwm yam |
| Cov nqe lus them nqi | L / CT / T (30% Deposit) |
| Tshuag los tsis | Txaus txaus |
| Qauv | Qauv dawb |
| Daim ntawv thov | Kev lag luam tshuaj, Tshuaj kho mob, khoom siv tsim kho, Kho kom zoo nkauj, Chav ua mov, Khoom noj khoom haus, thiab lwm yam |
| Lub sij hawm xa tuaj | Hauv 7-15 hnub |
Qib sib npaug ntawm A240 Stainless Hlau 316L Cov Ntawv & Phaj
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| SWB 316L | 1.4404/1.4435 | S31603 | SUS 316L | 316S11/316S13 | 03Ch17N14M3 / 03Ch17N14M2 | Z3CND17-11-02 / Z3CND18-14-03 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 |
Stainless hlau 316L Daim Ntawv & Phaj Cov Khoom Siv Tshuaj
| Qib | C | Mn | Si | P | S | Cr | Mo | Ni | N |
| SWB 316L | 0.035 max | 2.0 max | max 1.00 Nws | 0.045 max | 0.030 max | 16 – 18 | 2 – 3 | 10 – 14 | 68,89m ua |
SS 316L Sheets & Phaj Mechanical Properties
| Qhov ntom | Melting Point | Tensile zog | Yield zog (0.2% Offset) | Elongation |
| 8.0 g / cm3 | 1399℃(2550℃F) | Psi - 75000, MPa - 515 | Psi - 30000, MPa - 205 | 35 % |