316 vs 316L Stainless hlau qhov tseem ceeb sib txawv
Jan 29, 2026
Tso lus
1. Cov ntsiab lus ntawm 316 thiab 316L yog dab tsi? 316: Tsawg dua lossis sib npaug li 0.08%; 316L: Tsawg dua lossis sib npaug li 0.03%.
2. Uas muaj kev vuam zoo dua, 316 lossis 316L? 316L, raws li nws cov ntsiab lus carbon tsawg tiv thaiv rhiab heev thiab intergranular corrosion tom qab vuam.
3. Thaum twg kuv yuav tsum xaiv 316 tshaj 316L? Xaiv 316 rau cov ntawv thov uas xav tau siab dua - qhov kub thiab txias, vim 316L muaj zog tensile qis dua.
4. Puas yog 316L kim dua 316? Yog lawm, 316L qhov kev tswj hwm nruj dua ua rau nws cov nqi nce li ntawm 10-15%.
5. UNS code rau 316L yog dab tsi? UNS S31603.