Txawm hais tias koj npaj tus nqi ua tiav lossis cov nqi thauj khoom, nkag siab qhov hnyav ntawm 316 stainless kav hlau yog qhov tseem ceeb. Hauv phau ntawv qhia no, peb muab cov ncauj lus kom ntxaws, kev xam cov txheej txheem, thiab cov lus qhia tswv yim los pab koj ua kom nrawm dua thiab muaj tseeb dua kev txiav txim siab.

316 stainless steel pipe weight chart

316 Stainless Hlau Yeeb Nkab Daim phiaj (metric thiab nti ntau thiab tsawg)

Txheej hauv lub taub (mm) Txheej hauv txoj kab uas hla (nti) Phab Ntsa Thickness (Mm) Nyhav (kg \/ m)
19.05 3/4" 1.65 0.77
25.4 1" 2.11 1.30
33.4 1-1/4" 2.77 2.21
42.16 1-1/2" 2.77 2.84
48.26 2" 2.77 3.27
60.33 2-1/2" 3.05 4.61
73.03 3" 3.05 5.65
88.9 3-1/2" 3.05 6.94
114.3 4-1/2" 3.05 9.04
141.3 5-1/2" 3.40 12.00
168.3 6-5/8" 4.78 20.00
219.1 8-5/8" 6.35 34.40
273.05 10-3/4" 7.11 51.60
323.85 12-3/4" 7.92 67.40
355.6 14" 9.53 97.30
406.4 16" 9.53 111.30

 

Vim li cas 316 Stainless hlau yeeb nkab yuag yog qhov tseem ceeb rau kev tshaj tawm?

Yog paub txog qhov hnyav ntawm316 stainless hlau kavPab koj:

Npaj thiab Nyiaj Siv Nyiaj Siv Tau Zoo

Xam cov nyiaj thauj khoom thiab cov nqi logistics

Kwv yees lub nra rau kev tsim kho thiab tshuab tshuab

Zam kev ua haujlwm qeeb los ntawm cov khoom siv tsis txaus lossis oversupply

Xaiv txoj cai316 lossis 316L stainless hlau yeeb nkabKuj ua kom paub meej qhov ruaj khov thiab corrosion tsis kam, tshwj xeeb yog rau cov tub rog, tshuaj lom neeg, thiab kev siv tshuaj.

 

Yuav xam li cas 316 stainless hlau yeeb nkab hnyav?

Tus qauv misula los laij qhov hnyav ntawm 316 stainless hlau yeeb nkab yog:
HeWeight (Kg \/ m) {{{0}}} (txheej thickness dickness × 0.02491
O🔹outer Txoj Inter (OD) thiab Phab Ntsa Thickness (WT) yog ntsuas hauv millimeters (hli)
{0. 02491 yog qhov ntom tsis tu ncua rau cov hlau tsis muaj hlau (kg \/ mm³)