316 - Molybdenum-Reinforced Austenitic Steel: Chloride Ib puag ncig Corrosion Fighter

Mar 31, 2026

Tso lus

Txheej txheem cej luam

316 yog tus hwm zoo austenitic stainless hlau, sib txawv los ntawm nws cov 2.00-3.00% molybdenum ntxiv uas ua rau muaj kev txhim kho pitting thiab crevice corrosion kuj nyob rau hauv chloride-muaj xov xwm. Ua los ntawm 16.00-18.00% chromium thiab 10.00-14.00% npib tsib xee, nws tsim lub ntsej muag ruaj khov-centered cubic austenitic qauv, ua kom cov khoom tsis sib nqus hauv lub xeev annealed. Qib no boasts zoo heev ductility, txias forming peev xwm, thiab weldability, yuav tsum tsis muaj complex preheating los yog tom qab-weld kev kho mob rau feem ntau daim ntaub ntawv. Piv nrog rau 304, nws muab kev ua tau zoo tshaj plaws hauv dej hiav txwv, ntsev pos huab, thiab ib puag ncig tshuaj lom neeg, dhau los ua cov khoom siv rau cov mob me me.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.08, Si Less dua lossis sib npaug rau 1.00, Mn Tsawg dua lossis sib npaug 2.00, P Tsawg dua lossis sib npaug 0.045, S Tsawg dua lossis sib npaug 0.030, Cr: 16.00-18.00, Ni: 10.00-14.00.

Tej yam cuab yeej cuab tam (Annealed Condition)

Tensile Strength (Rm): Ntau dua lossis sib npaug li 520 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 205 MPa; Elongation (A): Ntau dua lossis sib npaug li 40%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 187

Core Zoo

Molybdenum ntxiv ho txhim kho chloride corrosion kuj; non- sib nqus thiab ductile heev rau txoj kev sib sau; txhim khu kev qha weldability nrog tsawg kawg nkaus ncej- ua; balanced zog thiab corrosion kev ua tau zoo; ntau yam rau nruab nrab corrosive ib puag ncig.

Daim ntawv thov

Cov ntug dej hiav txwv architectural decorations, marine hardware, tshuaj siab hlab ntsha, khoom noj khoom haus thiab kws tshuaj, pulp thiab ntawv machinery, thiab dej kho tshuab.

Qib sib npaug

UNS S31600, STS316, SUS316, EN 1.4401, GB 06Cr17Ni12Mo2

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug