310S Stainless Steel Chemical Composition piav qhia

Aug 12, 2025

Tso lus

Dab tsi 310S Stainless hlau muaj

310S, sau 06Cr25Ni20 hauv GB / T 20878 system thiab 1.4845 hauv DIN thiab EN systems, yog qis-carbon austenitic stainless hlau ua nyob ib ncig ntawm 25% chromium thiab 20% npib tsib xee sib npaug. Qhov muaj pes tsawg leeg yog vim li cas nws tuaj yeem siv tsis tu ncua ntawm 1150 degree, thiab nws kuj yog vim li cas qib tau teev tseg los ntawm chemistry es tsis yog los ntawm lub zog ib leeg.

Chemical Composition Table

Element Cov ntsiab lus (%) Muaj nuj nqi
Cov pa roj carbon (C) 0.08 max Tswj carbide nag lossis daus thiab weldability
Chromium (Cr) 24.0-26.0 Tsim cov txheej txheem tiv thaiv oxide
Nickel (Ni) 19.0-22.0 Stabilizes cov qauv austenitic
Silicon (Si) 1.50 max Txhim kho oxidation tsis kam
Manganese (Mn) max 2.00 Nws Deoxidation thiab nitrogen solubility
Phosphorus (P) 0.045 max Cov khoom seem, khaws cia qis
Sulfur (S) 0.030 max Cov khoom seem, khaws cia qis

Lub luag hauj lwm ntawm Txhua Yam

Chromium (24.0-26.0%)yog tus yuam sij rau siab -kev ua haujlwm kub. Tshaj li kwv yees li 20% chromium cov hlau alloy tsim ib qhov ntom ntom, nws tus kheej - kho chromium oxide txheej uas tiv taus scaling thiab oxidation mus txog 1150℃.

Nickel (19.0-22.0%)ua kom cov qauv ua tiav austenitic, uas tiv thaiv cov theem nkig uas tsim nyob rau hauv qis dua -nickel tshav kub- tiv thaiv cov hlau thiab ua rau cov pa roj carbon diffusion hauv carburizing atmospheres.

Cov pa roj carbon ntau (0.08%)txhob txwm tshaj tawm qis qis kom cov chromium carbides tsis tsim ntawm cov ciam teb thaum lub sij hawm vuam lossis nce siab - kev pabcuam kub.

Silicon (1.50%)ntxiv oxidation kuj; silicon ntau dua yuav txhim kho qhov kev tiv thaiv ntxiv tab sis yuav ua rau muaj kev puas tsuaj rau weldability thiab toughness.

Manganese (2.00% siab tshaj)pab deoxidation thaum melting thiab pab khaws cia nitrogen hauv cov kua.

Phosphorus thiab sulfuryog cov seem uas raug txwv vim ob qho tib si txo tus cwj pwm ua haujlwm kub thiab vuam zoo.

Qhov Zoo Tshaj Carbon Tsawg thiab Intergranular Corrosion

Qhov sib txawv tseem ceeb tshaj plaws ntawm 310 thiab 310S yog carbon. Standard 310 tso cai rau 0.25% carbon, whereas 310S txwv rau 0.08%. Thaum lub austenitic stainless hlau uas muaj cov pa roj carbon ntau dua nyob rau hauv 600-900℃ntau yam thaum lub sij hawm vuam los yog kev pab cuam, chromium ua ke nrog carbon los ua chromium- nplua nuj carbides xws li Cr23C6 raws li cov ciam teb. Cov hlau uas nyob ib sab yog sab laug depleted hauv chromium thiab tsis tuaj yeem tsim cov yeeb yaj kiab oxide tiv thaiv, yog li intergranular corrosion thiab tawg pib muaj. Vim tias 310S khaws cov pa roj carbon monoxide los yog qis dua 0.08%, uas tsis muaj nag lossis daus loj heev, vuam kub- cov cheeb tsam cuam tshuam nyob twj ywm, thiab kev kho cua sov tom qab vuam feem ntau tsis tsim nyog. Qhov twg muaj zog nkag siab ntawm qhov kub thiab txias yog qhov yuav tsum tau ua, qhov kev tswj hwm ntawm 310H (0.04-0.10% carbon) raug xaiv.

Siab -Coj Cwj Pwm

Lub 24-26% chromium thiab 19-22% npib tsib xee sib npaug muab 310S kev pabcuam txuas ntxiv mus rau 1150℃thiab kev pabcuam cuam tshuam txog li 1200 degree, nrog kev ua haujlwm zoo rau oxidation, scaling thiab carburization. Lub austenitic matrix tag nrho kuj tiv taus cov sigma{10}}theem embrittlement uas cuam tshuam qis dua -nickel qib tom qab raug ntev hauv 600-900℃band. Raws li nrog rau txhua qib kub-tiv taus, kev ua tau zoo degrades sai sai hauv kev txo cov huab cua-kev coj tus kheej, thiab 310S yuav tsum tsis txhob raug xaiv rau cov tshuaj chloride ntub dej lossis kev pabcuam tshuaj lom neeg, qhov twg molybdenum-bearing lossis duplex qib ua tau zoo dua.

Cov Khoom Muag Khoom thiab Cov Qauv Sib Xws

Cov muaj pes tsawg leeg saum toj no siv thoob plaws phaj, ntawv, sawb, bar, seamless raj thiab welded yeeb nkab, nrog rau cov khoom tsim kho qhov ntev thiab kam rau ua.

Phaj, ntawv thiab sawb: ASTM A240

Seamless boiler, superheater thiab kub exchanger raj: ASTM A213

Seamless thiab welded yeeb nkab: ASTM A312

Bar thiab duab: ASTM A276

Cov qauv sib npaug: GB / T 20878 06Cr25Ni20 thiab DIN/EN 1.4845

Cov lus nug nquag

Q: Cov ntsiab lus carbon ntawm 310S stainless hlau yog dab tsi?
Nws yog capped ntawm 0.08% siab tshaj plaws, uas yog qhov txawv ntawm 310S los ntawm qhov siab dua -carbon niam txiv qib 310 ntawm 0.25% siab tshaj.

Q: Vim li cas 310S xav tau 24-26% chromium?
That chromium level produces a dense, adherent oxide scale, giving continuous service capability up to 1150℃without rapid scaling.

Q: Puas yog 310S zoo ib yam li 06Cr25Ni20?
Yog. 06Cr25Ni20 yog GB/T 20878 tus qauv thiab 1.4845 yog DIN thiab EN kev xaiv rau tib 25% chromium, 20% npib tsib xee qis-carbon alloy.

Q: Puas muaj cov pa roj carbon tsawg tsawg?
Nws me ntsis txo qis siab -kub creep zog piv nrog 310H, uas yog vim li cas 310H nrog 0.04-0.10% carbon yog xaiv rau loaded Cheebtsam nyob rau hauv lub creep ntau yam.

Q: Dab tsi yog qhov txwv ntawm silicon thiab vim li cas nws tseem ceeb?
Silicon yog txwv rau 1.50% siab tshaj plaws: nws pab oxidation tsis kam, tab sis qib siab dua txo cov weldability thiab toughness.

Q: Yuav ua li cas 310S welded?
Siv cov cua sov sib xws- tiv thaiv cov khoom siv thiab tswj cov cua sov nkag; cov ntsiab lus carbon tsawg txhais tau tias tom qab -weld kev kho cua sov feem ntau tsis tas yuav tsum tau.