310 Stainless Hlau Tus Nqi & Tus nqi sib piv

Jan 28, 2026

Tso lus

Vim li cas 310 Tus Nqi Ntau Tshaj 304 thiab 316

310 (UNS S31000, EN 1.4845) yog ib qho austenitic stainless hlau nrog txog 24-26% chromium thiab 19-22% npib tsib xee, kwv yees li ob npaug ntawm cov npib tsib xee thiab siab dua chromium tshaj 316. Vim tias npib tsib xee yog cov khoom kim tshaj plaws alloying, tus nqi ntawm 313-4 zaug yog . lub sij hawm ntawm 316, nyob ntawm kev ua lag luam. Tus nqi alloy yog tus tsav tsheb ncaj qha ntawm tus nqi.

Tus nqi sib piv ntawm ib nrais muag

Kev sib piv Yam piv txwv
310 vs 304 ib txog 3-4 zaug
310 vs 316 ib txog 1.5-2 zaug
310 vs nickel{1}}raws li alloy (UNS N06601 chav kawm) qis dua

Kev Ntsuas Tus Nqi: Tag Nrho Tus Nqi Ntawm Cov Tswv Cuab

Hauv siab - qhov kev pabcuam kub, tus nqi ntawm 310 yog los ntawm kev pabcuam lub neej. Nws cov ntsiab lus siab chromium thiab silicon muab cov oxidation zoo heev, thiab cov ntsiab lus nickel siab stabilizes austenitic qauv tiv thaiv thermal qaug zog. Qhov twg cov khoom siv tsis tu ncua ntawm qhov kub siab, qhov hloov pauv ntev ntawm 310 feem ntau ua rau nws cov nqi tag nrho ntawm cov tswv cuab qis dua cov qib pheej yig dua uas yuav tsum tau hloov ntau zaus.

Sib piv 310 nrog Nickel-Based Alloys

Nickel-raws li cov alloys xws li UNS N06601 muab siab dua - qhov kub thiab txias zoo dua nyob rau hauv ib puag ncig hnyav tab sis raug nqi ntau dua 310. Rau ntau qhov chaw oxidizing thiab kev pabcuam kub kub txog li 1000-1100 degrees C, 310 muab kev sib piv ntawm tus nqi. Qhov twg yuav tsum tau txo cov huab cua, sulfur compounds los yog siab creep zog, yuav tsum tau ib tug nickel-raws li alloy tseem tsim nyog.

Nqis -Txuag lwm txoj kev

Rau kev pabcuam kub txog li 900 degrees C, 309S (UNS S30908, EN 1.4833) yog ib qho qis dua -tus nqi hloov nrog oxidation zoo. Qhov twg yuav tsum tau vuam, qhov qis -carbon 310S (UNS S31008) zam carbide nag lossis daus thiab feem ntau nyiam. Xaiv cov qib zoo rau qhov ntsuas kub ua haujlwm, tsis yog tshaj- qhia, yog txoj hauv kev zoo tshaj plaws los tswj tus nqi.

Kev xav txog kev yuav khoom

Kev txiav txim kom muaj nuj nqis cuam tshuam rau nqi tsev: kev txiav txim ntau txo nqi tsev los ntawm kev lag luam ntawm nplai hauv zeb ntau lawm thiab logistics. Txiav- rau- phaj loj thiab daim ntawv txo cov seem rau tus neeg yuav khoom. Yuav tsum tau daim ntawv pov thawj zeb kuaj thiab lees paub tus qauv tswj hwm, piv txwv li ASTM A240 rau phaj, ASTM A312 rau cov yeeb nkab thiab ASTM A276 rau bar.

FAQ

1. Tus nqi ntawm 310 piv nrog 304 thiab 316 li cas?

Feem ntau hais txog 3-4 npaug ntawm tus nqi ntawm 304 thiab 1.5-2 npaug ntawm tus nqi ntawm 316, vim yog cov ntsiab lus chromium thiab nickel ntau dua.

2. Puas yog 310 pheej yig dua nickel-raws li alloys?

Yog lawm, pheej yig dua li npib tsib xee-raws li cov alloys xws li UNS N06601, thaum muab cov kev ua tau zoo sib xws hauv ntau cov oxidizing siab - cov kev pabcuam kub.

3. Puas yog tus nqi siab dua ntawm 310 them?

Rau kev ua haujlwm siab - qhov kub thiab txias tsis tu ncua, lub neej ua haujlwm ntev dua feem ntau txo tag nrho cov tswv cuab tus nqi piv nrog cov qib qis dua - alloy.

4. Puas muaj lwm txoj kev pheej yig dua rau 310?

309S (UNS S30908) yog qhov tsim nyog txog li 900 degrees C; Hauv qab no, 316L tuaj yeem tsim nyog.

5. Puas yog qhov kev txiav txim kom muaj nuj nqis cuam tshuam rau tus nqi tsev?

Yog, kev txiav txim ntau txo nqi tsev los ntawm kev lag luam ntawm nplai.

6. Qhov txawv ntawm 310 thiab 310S yog dab tsi?

310S yog qhov tsawg-carbon variant (carbon siab tshaj 0.08% piv rau 0.25%), muab cov weldability zoo dua thiab tsis kam rau carbide nag lossis daus.