309 vs 310 Stainless Hlau: Siab-} kub hnyav
Jul 28, 2025
Tso lus



Ua li cas lawv cov tshuaj lom neeg sib txawv sib txawv?
309 muaj 22 {{{- 24% chromium, thiab 0.2%) thiab 0.2% 50 oxidation ntau dua thiab ruaj khov.
Qhov twg ua tau zoo dua ntawm huab cua sov heev?
310 vam meej nyob rau hauv kev siv tas mus li 1150 ° C, outperforming 309, uas yog qhov tsim nyog rau ntawm huab cua sov, ua rau nws zoo tagnrho rau cov cub tawg thiab kiln tib yam.
Yuav ua li cas lawv sib piv hauv corrosion tsis kam?
Ob qho kev ua tau zoo rau oxidation thiab carburization ntawm qhov kub thiab txias {{} {} {} ua tau zoo dua nyob rau hauv tsawg tsawg hauv tshav kub.
Yuav ua li cas hais txog lawv cov ntaub thaiv thiab vuam cov khoom?
Ob qho tib si yog weldable nrog cov qauv kev kawm, Txawm hais tias muaj 310 yuav xav tau kev saib xyuas kom tsis txhob muaj kev sib cog lus hauv vuam thaum vuam thiab tej zaum yuav xav tau annealing rau kev ua haujlwm txias.
309 thiab 310 feem ntau siv?
309 siv nyob rau hauv cov chaw ua cua sov, kev hloov pauv cua sov, thiab cov khoom siv kub thiab cov khoom siv kub, thiab cov khoom siv boiler, thiab cov khoom siv boiler, thiab cov khoom siv ua kom sov.