304 Stainless Hlau: Universal Standard Austenitic Stainless Hlau

Dec 22, 2025

Tso lus

304 stainless hlau yog feem ntau siv austenitic stainless hlau, belongs rau classic "18-8" series (18% chromium + 8% nickel). Nws tsim cov ntaub ntawv ntom ntom chromium oxide passivation zaj duab xis rau ntawm qhov chaw, uas muab kev tiv thaiv corrosion zoo heev hauv qhov chaw me me. Nrog kev sib npaug ntawm cov khoom siv kho tshuab thiab tus nqi- kev ua tau zoo, nws tau dhau los ua tus qauv rau cov hom phiaj dav hlau stainless.

info-750-750

Core Parameters

Chemical Composition (wt%): C Tsawg dua lossis sib npaug rau 0.08, Si Less dua lossis sib npaug rau 1.00, Mn Tsawg dua lossis sib npaug rau 2.00, P Tsawg dua lossis sib npaug rau 0.045, S Tsawg dua lossis sib npaug rau 0.030, Cr=18.00-20.00, Ni=8.00-10.50}Balance

Mechanical Properties (Annealed): Tensile Strength Ntau dua los yog sib npaug rau 520MPa, Yield Strength Ntau dua lossis sib npaug rau 205MPa, Elongation Ntau dua lossis sib npaug li 40%, Brinell Hardness Tsawg dua lossis sib npaug rau 201HB

Kev Pabcuam Kub: -196℃txog 800℃(kev pabcuam txuas ntxiv; kev pabcuam ntev pom zoo Tsawg dua lossis sib npaug li 650 degree)

Qib sib npaug: SUS304 (JIS), EN 1.4301 (EN), UNS S30400 (ASTM)

Kev Ua Haujlwm Zoo: Zoo heev corrosion kuj nyob rau hauv atmospheric, dej tshiab, thiab qaug zog acid- puag ncig puag ncig; siab toughness txawm nyob rau hauv qis kub (-196 degree), tsis nkig puas; zoo txias sib sau thiab vuam kev ua tau zoo; tsis yog- sib nqus (cov hlau nplaum tsis muaj zog tuaj yeem tshwm sim tom qab ua haujlwm txias); tus nqi-zoo, haum rau kev siv ntau lawm.

Tej kev siv: Architectural decorations (curtain walls, handrails), food processing equipment (tanks, conveyors), cov khoom siv hauv tsev (sinks, qhov cub hauv phab ntsa), cov khoom siv kho mob (tsis yog{0}}implantable), cov kav dej dav dav, thiab cov khoom siv tshuaj lom neeg rau ib puag ncig corrosion me me.

info-750-750

Tswv yim Q&A

Q1: Vim li cas 304 stainless hlau xeb hauv ntug dej hiav txwv? A1: Lub ntug dej hiav txwv ntsev muaj cov tshuaj chloride ions siab, uas tuaj yeem nkag mus thiab ua rau cov yeeb yaj kiab passivation puas. Yog tsis muaj kev tu tsis tu ncua, lub zos pitting corrosion yuav tshwm sim. Rau kev siv ntug hiav txwv dej, nws raug nquahu kom nce qhov kev kho mob saum npoo av lossis ncaj qha xaiv 316 stainless hlau nrog cov tshuaj chloride ion zoo dua.

Q2: 304 stainless hlau puas tuaj yeem siv rau hauv siab - cov khoom siv kub? A2: Nws tuaj yeem siv tau ntawm qhov kub txog li 800℃rau lub sijhawm luv, tab sis ntev - kev pabcuam ntawm qhov kub siab tshaj 650℃yuav txo nws cov oxidation tsis kam thiab lub zog txhua yam. Rau siab - qhov kub thiab txias ib puag ncig siab tshaj 650℃, 304H lossis 309S nrog qhov siab zoo dua - qhov kub thiab txias yuav tsum tau xaiv.

Q3: Dab tsi cuam tshuam rau corrosion kuj ntawm 304 stainless hlau? A3: Lub hauv paus yog kev ncaj ncees ntawm cov yeeb yaj kiab passivation. Kev puas tsuaj rau lub cev (khib nyiab, kev sib tsoo), tshuaj yaig (muaj zog acids, siab -concentration chloride ions), thiab ntev- lub sij hawm tsub zuj zuj ntawm cov kab mob saum npoo tuaj yeem ua rau cov zaj duab xis passivation, ua rau txo qis corrosion. Kev tu thiab tu tsis tu ncua tuaj yeem ua rau nws lub neej ua haujlwm ntev.

info-750-750

Q4: Puas yog 304 stainless hlau haum rau kev ua haujlwm txias xws li stamping? A4: Yog. Nws muaj qhov txias txias formability, thiab tuaj yeem tiv taus qhov sib sib zog nqus nqus, stamping, khoov thiab lwm yam txheej txheem yam tsis muaj kev tawg. Nws yuav tsum tau muab sau tseg tias tom qab ua hauj lwm txias, cov khoom yuav ua hauj lwm - hardened, thiab yog hais tias yuav tsum tau ua ntxiv, intermediate annealing (1050-1100 degree, txias ceev) yuav tsum tau ua kom rov qab toughness.

Q5: Cov khoom siv vuam thiab cov txheej txheem dab tsi tau pom zoo rau 304 stainless hlau? A5: Qhov kev nyiam vuam hlau yog ER308L, thiab cov electrode yog E308L-16, uas tuaj yeem ua kom muaj kev tiv thaiv corrosion thiab toughness ntawm vuam. Rau TIG vuam, tam sim no yuav tsum tau tswj ntawm 80-120A, thiab argon ntshiab yuav tsum tau siv rau kev tiv thaiv; rau MIG vuam, qhov tam sim no yog 150-200A, thiab qhov vuam ceev yuav tsum ruaj khov kom tsis txhob muaj cua sov ntau dhau.