2205 Stainless hlau vs . 316: Qhov txawv tseem ceeb

Apr 27, 2026

Tso lus

 
2205 Stainless Steel

Dab tsi yog 2205 Stainless Hlau?

2205 stainless hlau yog nitrogen- txhim kho, 22% chromium duplex (ferritic-austenitic) alloy uas muaj kev tiv thaiv corrosion zoo dua thiab siab zog piv rau 316/316L. Cov alloy no ua rau muaj kev tiv thaiv zoo heev rau chloride-induced stress corrosion cracking and pitting. Kev siv dav hauv kev lag luam marine engineering, roj thiab roj, thiab cov khoom siv tshuaj lom neeg, 2205 muaj nyob rau hauv ntau hom khoom siv, nrog rau cov phaj, coils, raj, tuav, xov hlau, thiab lwm yam.

Dab tsi yog qhov sib npaug ntawm cov khoom siv SS 2205?

SS 2205 (Duplex 2205) feem ntau sib npaug rau UNS S32205 / S31803, EN 1.4462, thiab ASTM F51. Feem ntau siv nyob rau hauv marine thiab tshuaj ua, nws yog ib tug siab -lub zog, corrosion-resistant alloy, feem ntau suav hais tias yog ib tug nqi- zoo lwm txoj rau siab -nickel steels.

SS 2205 Material
Stainless Steel

Dab tsi yog qhov zoo ntawm 316 stainless hlau?

316 stainless hlau yog tus hwm, corrosion{1}} tiv taus austenitic alloy uas muaj hlau, chromium (16–18%), npib tsib xee (10–12%), thiab qhov tseem ceeb, molybdenum (2–3%). Qhov muaj pes tsawg leeg no muab kev tiv thaiv zoo tshaj rau cov tshuaj chlorides thiab cov kua qaub piv rau 304 stainless, ua rau nws xaiv tus qauv rau marine, tshuaj, thiab siab -chloride ib puag ncig.

Dab tsi yog cov khoom sib npaug rau 316 stainless hlau?

Cov sib npaug sib npaug rau 316 stainless hlau (UNS S31600) suav nrog EN 1.4401, DIN X5CrNiMo17-12-2, thiab JIS SUS316, feem ntau siv nyob rau hauv marine thiab tshuaj ib puag ncig. Rau kev txhim kho vuam, 316L (EN 1.4404, UNS S31603) yog siv. Cov kev xaiv zoo tshaj plaws muaj xws li 317L, 904L, lossis 2205 duplex, thaum 445M2 muab kev tiv thaiv corrosion ntau dua li kev xaiv ferritic.

316 Stainless Steel

2205 Stainless hlau vs . 316: Tshuaj muaj pes tsawg leeg

Tus nqi sawv cev qhov hnyav feem pua ​​(wt%) raws li ASTM A240 / A240M.

Element 316L (UAS S31603) 2205 Duplex (UNS S32205)
Chromium (Cr) 16.0 – 18.0 22.0 – 23.0
Nickel (Ni) 10.0 – 14.0 4.5 – 6.5
Molybdenum (hli) 2.0 – 3.0 3.0 – 3.5
Nitrogen (N) Tsawg dua lossis sib npaug li 0.10 0.14 – 0.20
Cov pa roj carbon (C) Tsawg dua lossis sib npaug li 0.03 Tsawg dua lossis sib npaug li 0.03
Manganese (Mn) Tsawg dua lossis sib npaug li 2.00 Tsawg dua lossis sib npaug li 2.00
Silicon (Si) Tsawg dua lossis sib npaug li 0.75 Tsawg dua lossis sib npaug li 1.00
Phosphorus (P) Tsawg dua lossis sib npaug li 0.045 Tsawg dua lossis sib npaug li 0.030
Sulfur (S) Tsawg dua lossis sib npaug li 0.030 Tsawg dua lossis sib npaug li 0.020
Hlau (Fe) Tshuav Tshuav
PREN Tus nqi* ~24 – 26 ~34 – 36

*PREN (Pitting Resistance Tus lej sib npaug)=%Cr + 3.3(%Mo) + 16(%N)

 

2205 Stainless hlau vs . 316: Mechanical Properties

Yam tsawg kawg nkaus nyob rau hauv chav tsev kub (20℃/ 68℃F) rau annealed phaj.

Khoom 316L (Austenitic) 2205 (Dubplex)
Yield zog (0.2% Offset) 170-205 MPa 450-485 MPa
Qhov kawg Tensile Strength (UTS) 485-515 MPa 620-680 MPa
Elongation (hauv 50mm) Ntau dua lossis sib npaug li 40% Ntau dua lossis sib npaug li 25%
Hardness (Brinell - HB) Tsawg dua lossis sib npaug li 217 Tsawg dua lossis sib npaug li 293
Hardness (Rockwell - HRC) Tsawg dua lossis sib npaug rau 95 (HRB) Tsawg dua lossis sib npaug rau 31 (HRC)
Impact Energy (Charpy V-Notch) Zoo heev mus rau -196 degree Zoo heev mus rau -50 degree

 

2205 Stainless hlau vs . 316: Lub cev muaj zog

Khoom Chav tsev 316/316L 2205 Duplex
Qhov ntom g/cm³ 8.00 7.80
Modulus ntawm Elasticity GPa 193 200
Thermal Expansion Coeff. µm / m·℃(0-100 degree) 16.0 13.0
Thermal conductivity W/m·K (100 degree) 16.3 19.0
Tshwj xeeb kub J/kg · K (0-100 degree) 500 450
Hluav taws xob Resistivity nΩ·m 740 800

 

2205 Stainless hlau vs . 316: Corrosion Resistance

Qhov kev tiv thaiv corrosion ntawm 2205 duplex stainless hlau yog qhov zoo dua li ntawm 316. Nws Pitting Resistance Equivalent Number (PREN) feem ntau ntau dua lossis sib npaug li 35, piv rau kwv yees li 24-26 rau 316. 2205 muab 2-3 npaug zoo dua rau cov tshuaj chloride -induced pitting, corrosion, crevice, seawater xaiv. desalination, thiab tshuaj ua haujlwm ib puag ncig, qhov twg 316 yuav maj mam ua tsis tau raws sijhawm.

 

2205 Stainless hlau vs . 316: Magnetism

Vim nws cov duplex (ferritic + austenitic) microstructure, 2205 stainless hlau nthuav tawm ib feem ntawm cov hlau nplaum, feem ntau qhia tsis muaj zog rau cov khoom sib nqus. Nyob rau hauv sib piv, 316 stainless hlau yog tag nrho austenitic thiab feem ntau tsis yog -magnetic nyob rau hauv lub annealed mob.

 

2205 Stainless hlau vs . 316: Daim ntawv thov

2205 yog dav siv nyob rau hauv ib puag ncig nruj heev xws li offshore roj platforms, seawater systems, desalination nroj tsuag, thiab flue gas desulfurization (FGD) units. Hauv kev sib piv, 316 feem ntau yog siv rau hauv kev ua zaub mov, tshuaj, kho vaj tse, thiab cov kav dej dav dav, qhov twg corrosion tsis tshua muaj zog thiab yooj yim ntawm fabrication feem ntau yog qhov tseem ceeb.


2205 Stainless hlau vs . 316: Tus nqi

Los ntawm tus nqi ntawm cov khoom siv, 2205 feem ntau yog 20% ​​-30% kim dua ib tuj tshaj 316 vim nws cov ntsiab lus alloy siab dua. Txawm li cas los xij, thaum ntsuas los ntawm tus nqi ntawm lub neej, siv 2205 tuaj yeem txo tag nrho cov nqi ntawm qhov project los ntawm 10% -25%. Yog li ntawd, nyob rau hauv cov tshuaj chloride- nplua nuj los yog corrosive ib puag ncig, 2205 feem ntau yog tus nqi ntau dua - kev xaiv zoo nyob rau lub sij hawm ntev.

 

Yog tias koj muaj qhov project-cov kev cai tshwj xeeb rau 316 lossis 2205 stainless hlau, peb caw koj tso qhov kev txiav txim. GNEE khaws cov khoom lag luam ntau ntawm cov khoom nrov rau koj xaiv. Cov ntaub ntawv no tuaj yeem ua tiav rau hauv ntau hom kev siv tswv yim-xws li cov phaj, coils, raj, tuav, xov hlau, thiab lwm yam. Yog xav paub ntxiv txog cov tshuaj muaj pes tsawg leeg lossis thov cov qauv dawb, thov hu rau peb lub Hoobkas tam sim. Peb muab cov nqi sib tw thiab kev pabcuam tshwj xeeb.

Hu rau tam sim no

ASTM A312 TP316 Stainless Steel Pipe 

ASTM A312 TP316 Stainless hlau yeeb nkab

 ASTM A240 316 Stainless Steel Plate

ASTM A 240 316 Stainless Hlau Phaj

ASTM A276 316 Stainless Steel Bar 

ASTM A 276 316 Stainless Hlau Bar

 316 Stainless Steel Coil

316 Stainless hlau kauj

ASTM A790 UNS 32205 Stainless Steel Pipe

ASTM A790 UNS 32205 Stainless hlau yeeb nkab
 

ASTM A240 2205 Stainless Steel Plate 

ASTM A 240 2205 Stainless Hlau Phaj

ASTM A276 2205 Stainless Steel Bar 

ASTM A 276 2205 Stainless Hlau Bar

2205 Stainless Steel Coil 

2205 Stainless hlau kauj

 

Cov khoom lag luam stainless hlau 316 thiab 2205 peb muab tag nrho ua raws li ASTM cov qauv, tuav ISO 9001, PED, thiab SGS ntawv pov thawj, thiab nrog EN 10204 3.1 Cov Khoom Siv Xeem Ntawv Pov Thawj (MTCs), ua kom tag nrho cov khoom traceability.

316 Stainless Steel Material Certificate
316 Stainless Hlau Khoom Certificate
2205 Stainless Steel Material Certificate
2205 Stainless Hlau Khoom Certificate

Xa kev nug