1.4462 duplex stainless hlau sib npaug

Jul 17, 2025

Tso lus

Dab tsi yog 1.4462 duplex stainless hlau sib npaug?

1.4462 duplex stainless hlau, tseem hu ua X2CrNiMoN22-5-3, yog qib siv dav rau nws lub zog siab thiab zoo heev corrosion kuj, tshwj xeeb tshaj yog nyob rau hauv ib puag ncig chloride nplua nuj.

Khoom siv: Duplex stainless hlau (ferritic{0}}austenitic)

Daim ntawv thov: Cov hlab ntsha siab, cov nroj tsuag desalination, offshore platforms, tshav kub exchangers, pipelines.

Txuj Qib sib npaug
UNS (ASTM / ASME) S31803 / S32205
AISI / SAE –
JIS (Nyiv) SUS329J3L
GB (Tuam Tshoj) 022Cr22Ni5Mo3N
GOST 08Х22Н5М3Л

 

S31803 vs S32205 vs 1.4462: Puas yog Lawv Ib Leeg?

Thaum UNS S31803 thiab 1.4462 feem ntau suav hais tias yog sib npaug, UNS S32205 muaj qhov ua tau zoo me ntsis nrog kev txhim kho corrosion. Ntau lub tuam txhab tau hloov ntawm S31803 mus rau S32205 kom ua tau raws li kev pabcuam nruj dua.

Cov lus qhia rau cov neeg yuav khoom:Yog tias kev xa khoom los ntawm Tebchaws Europe, koj tuaj yeem tau txais cov ntaub ntawv sau tias yog 1.4462 tab sis tau lees paub kom ua tau raws li S32205 kev ua haujlwm.

 

Tshuaj muaj pes tsawg leeg 1.4462

Qhov nyiaj tshuav tshuaj no muab PREN (Pitting Resistance Equivalent Number) ntawm ~ 34–35, ua rau nws tsim nyog rau cov tshuaj chloride- muaj ib puag ncig xws li dej hiav txwv lossis tshuaj brine.

Element Cov ntsiab lus (%)
Chromium (Cr) 21.0–23.0
Nickel (Ni) 4.5–6.5
Molybdenum (hli) 2.5–3.5
Nitrogen (N) 0.14–0.20
Manganese (Mn) Tsawg dua los yog sib npaug rau 2.0
Cov pa roj carbon (C) Tsawg dua lossis sib npaug li 0.03

 

Mechanical Propertiesntawm 1.4462 Duplex Stainless Hlau

Khoom Tus nqi
Yield zog (Rp0.2) Ntau dua lossis sib npaug li 450 MPa
Tensile zog (Rm) 620-880 MPa
Elongation Ntau dua lossis sib npaug li 25%
PREN (Pitting Resistance) 34-38 (zoo heev)
Kev Pabcuam Kub -50℃rau +250 degree

 

Dab tsi yog qhov ntom ntawm 1.4462 steel?

Qib: X2CrNiMoN22-5-3
Tus lej: 1.4462
Kev faib tawm: Austenitic -ferritic stainless hlau
Ceev: 7.8g / cm3
Txheem:
TS EN 10088-2: 2005 Stainless hlau Kev xa tawm cov xwm txheej rau daim ntawv / phaj thiab sawb ntawm corrosion resisting steels rau dav siv
EN 10088-3: 2005 Stainless hlau Kev xa tawm cov xwm txheej rau cov khoom lag luam ib nrab tiav, tuav, rods, hlau, ntu thiab cov khoom ci ci ntawm corrosion resisting steels rau lub hom phiaj dav

 

1.4462 Stainless Hlau Machinability & Weldability

Kev ua haujlwm nruab nrab-yuav tsum tau txiav qeeb qeeb thiab cov cuab yeej nruj piv rau qib austenitic.
Zoo weldability nrog cov hlau muab tub lim kom zoo (xws li ER2209 lossis E2209), tsis txhob muaj cua sov ntau dhau los tiv thaiv cov theem tsis sib xws.

Tshaj tawm -weld pickling thiab passivation pom zoo kom pom zoo corrosion kuj.

 

Thaum xaiv 1.4462 lossis nws qhov sib npaug, xav txog qhov chaw ua haujlwm, cov ntawv pov thawj xav tau, thiab qib corrosion kuj. Txawm hais tias koj tab tom nrhiav los ntawm EU, Asmeskas, lossis Asia, kev nkag siab sib npaug ua kom zoo thiab ua raws.

NtawmGNEE, peb muab ntawv pov thawj 1.4462 duplex stainless hlau kav, raj, thiab nplooj ntawv nrog tag nrhoEN 10204 3.1/3.2 MTC, txhawb kev sib npaug thoob ntiaj teb xws liS32205. Peb pab cov neeg siv txheeb xyuas cov qib zoo ib qhov project specs thiab cov qauv hauv zos.

Hu rau tam sim no

 

1.4462 Duplex Stainless Hlau hauv Tshuag

Daim ntawv khoom Size Range (Tswj) Cov qauv
Seamless Yeeb Nkab OD 6 - 610 mm, WT 1 - 50 mm ASTM A790, EN 10216-5, DIN 17456
Welded yeeb nkab OD 15 - 1219 mm, WT 1 - 40 mm ASTM A928, EN 10217-7
Seamless Tube OD 6 - 114 hli, WT 0.5 - 6 mm ASTM A789, EN 10216-5
Welded Tube OD 12-254 hli, WT 0.5-5 mm ASTM A249, EN 10217-7
Phaj / Ntawv Thickness 1.0-50 hli ASTM A240, EN 10088-2
Coil / Sawb Thickness 0.3-6.0 hli, Dav mus txog 1500 hli ASTM A240, EN 10088-2
Round Bar / Qws Dia. 6 - 300 mm ASTM A479, EN 10088-3

 

Nto tiav:2B, No.1, pickled, polished, los yog txhuam muaj nyob rau ntawm kev thov.

Delivery condition:Cov tshuaj annealed, pickled, thiab passivated.

Cov ntawv pov thawj:EN 10204 3.1 / 3.2, PED/AD 2000, NORSOK (yog muaj).