1.4301 vs . 1.4306 Stainless hlau: Qhov txawv ntawm qhov tseem ceeb

Nov 04, 2025

Tso lus

Yog tias koj xaiv ntawm EN 1.4301 thiab EN 1.4306 stainless hlau, nkag siab txog lawv cov tshuaj muaj pes tsawg leeg, kev tiv thaiv corrosion, thiab daim ntawv thov tsim nyog yog qhov tseem ceeb rau kev txiav txim siab yuav khoom. Ob qib muaj nyob rau hauv austenitic 18/8 stainless hlau tsev neeg, sib npaug rau AISI 304 thiab AISI 304L, tab sis lawv txawv feem ntau ntawm cov ntsiab lus carbon thiab weldability kev ua tau zoo.1.4306 muaj cov ntsiab lus qis dua (0.03% max) dua li 1.4301 (0.07% corrosion kuj thiab max.)

 

X5CrNi18-10, 1.4301, AISI 304 yog dab tsi?
1.4301 stainless hlau yog sib npaug rau AISI 304 (tseem hu ua UNS S30400). Raws li European qauv, nws tseem hu ua X5CrNi18-10. Vim nws cov nominal muaj pes tsawg leeg ntawm 18% chromium thiab 8% npib tsib xee, qee zaum nws raug xa mus los ntawm nws lub npe laus, 18/8. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau cov phaj, coils, kav, tuav, thiab xaim.

 

1.4306 X2CrNi19-11 yog dab tsi?
Acid resistant stainless hlau nrog ntxiv ntawm nitrogen, txo cov ntsiab lus carbon thiab nce chromium 18-20% thiab npib tsib xee 10-12%. Txwv tsis pub, qhov kev txhim kho ntawm qib 1.4307 / AISI 304L. Siv qhov twg ib txwm 304 lossis 304L cov khoom tsis txaus thiab yuav tsum muaj kev tiv thaiv corrosion ntxiv.

 

1.4301 puas tuaj yeem siv 1.4306?
Yog lawm, tab sis yog tias vuam koom nrog lossis cov khoom siv yuav ua haujlwm nyob rau hauv ib puag ncig corrosive (tshwj xeeb tshaj yog cov tshuaj chloride lossis acid raug), 1.4306 raug pom zoo.

 

1.4301 vs . 1.4306 Stainless hlau: Tshuaj lom neeg (EN 10088-1 Standard)

Element EN 1.4301 (AISI 304) EN 1.4306 (AISI 304L)
C (Carbon) Tsawg dua lossis sib npaug li 0.07% Tsawg dua lossis sib npaug li 0.030%
Si (Silicon) Tsawg dua lossis sib npaug li 1.00% Tsawg dua lossis sib npaug li 1.00%
Manganese (Mn) Tsawg dua lossis sib npaug li 2.00% Tsawg dua lossis sib npaug li 2.00%
P (phosphorus) Tsawg dua lossis sib npaug li 0.045% Tsawg dua lossis sib npaug li 0.045%
S (Sulfur) Tsawg dua lossis sib npaug li 0.015% Tsawg dua lossis sib npaug li 0.015%
Cr (Chromium) 17.5–19.5% 17.5–19.5%
Ni (Nickel) 8.0–10.5% 10.0–12.0%
N (Nitrogen) Tsawg dua lossis sib npaug li 0.11% Tsawg dua lossis sib npaug li 0.11%

1.4301 vs . 1.4306 Stainless Steel: Mechanical Properties

Khoom TS EN 1.4301 TS EN 1.4306
Qhov ntom 7.93 g/m² 7.93 g/m²
Tensile zog (MPa) Ntau dua lossis sib npaug li 520 Ntau dua lossis sib npaug li 500
Yield zog (MPa) Ntau dua lossis sib npaug li 210 Ntau dua lossis sib npaug rau 190
Elongation (%) Ntau dua lossis sib npaug li 45 Ntau dua lossis sib npaug li 45
Hardness (HB) Tsawg dua lossis sib npaug li 215 Tsawg dua los yog sib npaug li 200
Max Service Kub 870 degree 870 degree

 

1.4301 thiab 1.4306 Stainless Hlau: Weldability

1.4301 (X5CrNi18-10) muaj qhov zoo weldability, tab sis cov cua sov- thaj tsam cuam tshuam yog qhov ua rau muaj kev kub ntxhov thaum vuam, uas txo nws cov corrosion tsis kam. 1.4306 (X2CrNi19-11), raws li qhov sib txawv ntawm cov pa roj carbon tsawg (3 los yog sib npaug), tsawg dua li 0. txhim kho weldability los ntawm kev txo qis carbide tsim, ua rau nws yog qhov kev xaiv zoo tshaj plaws rau kev siv vuam tseem ceeb uas yuav tsum tau muaj siab heev tom qab vuam corrosion kuj.


1.4301 thiab 1.4306 Stainless Hlau: Corrosion Resistance

1.4301 pom zoo corrosion kuj nyob rau hauv ib puag ncig me me (piv txwv li, huab cua, dej tshiab), tab sis nws cov ntsiab lus carbon siab (tsawg dua lossis sib npaug li 0.07%) tuaj yeem ua rau muaj kev xeb hauv zos (xws li, intergranular corrosion) tom qab vuam los yog ntev raug rau cov xov xwm corrosive. 1.4306 stainless hlau muaj ib qho ultra-tsawg dua cov ntsiab lus ntawm 0.07% (Less). thiab cov ntsiab lus npib tsib xee ntau dua me ntsis, yog li nthuav tawm zoo heev tiv thaiv intergranular corrosion thiab pitting corrosion, ua rau nws tshwj xeeb tshaj yog haum rau welded pob qij txha los yog chemically corrosive ib puag ncig.

 

1.4301 vs . 1.4306 Stainless hlau: Daim ntawv thov

1.4301 stainless hlau yog dav siv nyob rau hauv dav siv xws li cov khoom siv hauv chav ua noj, kho kom zoo nkauj hauv tsev, thiab tsis yog - cov kav dej tseem ceeb, qhov uas yuav tsum tau muaj kev tiv thaiv corrosion tsis siab . 1.4306 stainless hlau yog qhov tsim nyog rau siab -precision los yog corrosion- cov ntaub ntawv rhiab heev, xws li cov cuab yeej siv tshuaj, khoom noj khoom haus, thiab cov khoom siv hauv cov tshuaj lom neeg. corrosive ib puag ncig.

 

1.4306 stainless hlau nqi ib kg
Tus 1.4301 stainless hlau nqi ib kg yog feem ntau nyob ib ncig ntawm US $ 2.4-US $ 3.2, thaum 1.4306 stainless hlau ranges ntawm US $ 2.6-US $ 3.5, nyob ntawm seb cov khoom hom, thickness, thiab nto tiav (2B, BA, No.4, los yog iav). Tej kev txiav txim los yog CIF tus me nyuam quotes yuav customized raws li qhov chaw nres nkoj.

 

Yog tias koj muaj ib qhov project xav tau rau 304 lossis 304L stainless hlau, thov koj xav tso qhov kev txiav txim. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Peb tuaj yeem ua lawv rau hauv ntau hom khoom siv, nrog rau cov phaj, coils, kav, tuav, thiab xaim. Rau cov ncauj lus kom ntxaws tshuaj muaj pes tsawg leeg thiab kuaj dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.

1.4301 Stainless Steel Plate
1.4301 stainless hlau phaj
1.4306 Stainless Steel  Pipe
1.4306 stainless hlau yeeb nkab

Xa kev nug