1.4021 QT800 vs . 1.4021 QT700: Sib piv lub zog

Jul 16, 2025

Tso lus

Nkag siab 1.4021 thiab + QT Tsim

1.4021 yog EN 10088 tsim rau X20Cr13, martensitic stainless hlau nrog 12-14% chromium thiab 0.16-0.25% carbon. Nws yog sib npaug rau AISI 420, UNS S42000, DIN X20Cr13, ISO X20Cr13 thiab Suav qib 20Cr13. Cov lus kawg +QT700 thiab +QT800 piav qhia txog kev xa khoom: cov hlau yog quenched thiab tempered rau ib chav kawm muaj zog. Qhov tseem ceeb, tus lej tom qab + QT xaiv qhov tsawg kawg nkaus tensile lub zog Rm hauv megapascals, tsis yog lub zog tawm los: +QT700 lav Rm ntawm 700 MPa yam tsawg kawg nkaus, thiab + QT800 lav Rm ntawm 800 MPa yam tsawg kawg nkaus. Qhov no ua raws li EN 10088-3 / ISO 683-13 convention rau cov qib kub-kho martensitic.

Chemical Composition thiab sib npaug

Cov muaj pes tsawg leeg hauv qab no ua raws li EN 10088-3 rau 1.4021 bar; tib qhov kev txwv siv rau cov qib sib npaug hauv lwm lub tshuab.

Element 1.4021 (EN 10088-3)
Cov pa roj carbon (C) 0.16-0.25%
Silicon (Si) Tsawg dua lossis sib npaug li 1.00%
Manganese (Mn) Tsawg dua lossis sib npaug li 1.00%
Phosphorus (P) Tsawg dua lossis sib npaug li 0.040%
Sulfur (S) Tsawg dua lossis sib npaug li 0.030%
Chromium (Cr) 12.00-14.00%
Standard System Qib sib npaug
EN 1.4021 (X20Cr13)
AISI / UNS 420 / S42000
DIN X20Cr13
ISO X20Cr13+QT700 / +QT800
GB (Tuam Tshoj) 20 Cr13

Mechanical Properties: QT700 vs QT800

Kev lees paub qhov tseem ceeb hauv qab no ua raws EN 10088-3 rau ob chav kawm muaj zog. Cov hlau qub yog tempered ntawm qhov kub thiab txias kom ncav cuag txhua chav.

Khoom 1.4021 +QT700 1.4021 +QT800
Tensile zog Rm 700-850 MPa 800-950 MPa
0.2% pov thawj kev nyuaj siab Rp0.2 Ntau dua lossis sib npaug li 450 MPa Ntau tshaj lossis sib npaug li 600 MPa
Elongation A Ntau dua lossis sib npaug li 15% Ntau dua lossis sib npaug li 12%
Impact toughness Siab dua (softer temper) Lower (nyuaj siab)
Hnav tsis kam Nruab nrab Txhim kho

Nco ntsoov tias hardness tsis cais los ntawm EN 10088-3 rau cov chav kawm no; nws yog qhov tshwm sim ntawm kev xaiv npau taws. Hauv kev xyaum QT700 cov khoom ntsuas kwv yees li 200-230 HBW thiab QT800 kwv yees li 230-260 HBW, thiab cov nuj nqis no yuav tsum tau lees paub ntawm daim ntawv pov thawj zeb.

Kev kho cua sov thiab metallurgy

Ob chav kawm pib nrog austenitising ntawm 950-1000℃tom qab los ntawm roj lossis polymer quenching. Qhov txawv yog qhov kub thiab txias: qhov kub siab dua nyob ib puag ncig 650-700℃softens lub martensite kom ncav cuag QT700 chav kawm, thaum lub kub qis dua nyob ib ncig ntawm 600-650℃khaws ntau hardness thiab ncav cuag QT800. Thaum tempering 13% chromium martensitic steel, zam qhov sib txawv nruab nrab ntawm 450℃thiab 600℃qhov twg toughness yuav poob vim npau taws embrittlement. Rau siab tshaj plaws corrosion kuj, cov hlau yuav tsum tau hardened, tempered thiab ces tiav los ntawm kev sib tsoo los yog polishing, vim hais tias cov passive zaj duab xis yog zoo tshaj plaws nyob rau hauv ib tug huv si nto.

Daim ntawv thov thiab kev taw qhia kev xaiv

1.4021 +QT700 suits shafts, bolts, twj twj tso kua mis thiab lub tshuab qhov chaw uas ductility thiab toughness teeb meem thiab loads yog nruab nrab. 1.4021 +QT800 suits valve stems, turbine hniav, spindles thiab heev stressed qhov chaw uas siab zog thiab hnav tsis kam ua pov thawj qis ductility. Yog hais tias ib feem yog welded, nco ntsoov tias martensitic 13% chromium steel yuav tsum tau preheating thiab post-weld tempering; rau weld-heavy designs qis dua- carbon qib lossis lwm yam austenitic yuav tsum raug txiav txim siab. Yog hais tias ib puag ncig yog corrosive, 420-hom steel yog txwv rau cov mob me me thiab yuav tsum tau coated los yog zam kom haum rau qib austenitic.

FAQ

+QT800 txhais li cas ntawm 1.4021?

Nws txhais tau tias lub bar yog xa nyob rau hauv lub quenched thiab tempered mob nrog ib tug guaranteed yam tsawg kawg nkaus tensile zog Rm ntawm 800 MPa. Tus lej tom qab + QT yog chav kawm tensile lub zog, tsis yog lub zog tawm los.

Puas yog 1.4021 tib yam li AISI 420?

Yog. 1.4021 (X20Cr13) yog EN lub npe ntawm AISI 420; UNS tus lej yog S42000 thiab Suav sib npaug yog 20Cr13.

Qhov twg zoo dua: QT700 lossis QT800?

Tsis muaj qib zoo dua. QT700 muaj qhov zoo dua ductility thiab toughness; QT800 muaj zog dua, hardness thiab hnav tsis kam. Qhov kev xaiv nyob ntawm seb qhov ua tsis tiav los ntawm kev ua haujlwm dhau los lossis los ntawm kev hnav.

QT cov chav kawm puas tuaj yeem welded?

Tsuas yog nrog ceev faj. Preheat rau 200-300 degree, siv qis-hydrogen muab tub lim thiab npau taws tom qab vuam. Txawm li ntawd los, tshav kub- thaj tsam cuam tshuam yuav nyuaj thiab tawg-sensitive; rau cov rooj sib txoos welded xav txog qib qis-carbon martensitic lossis austenitic stainless hlau.

Qhov txawv ntawm 1.4021 thiab 1.4028 yog dab tsi?

1.4028 (X30Cr13) muaj 0.26-0.35% carbon, txog 0.10% siab dua 1.4021. Nws ncav cuag hardness siab dua tom qab hardening tab sis muaj qis toughness thiab weldability . 1.4021 yog lub hom phiaj ntau dua ntawm ob.

Puas yog hardness lav rau QT cov chav kawm?

TS EN 10088-3 Kev lees paub lub zog tensile rau QT chav kawm; hardness yog tshwm sim los ntawm kev npau taws thiab tau tshaj tawm ntawm daim ntawv pov thawj zeb. Yog hais tias lub qhov rais hardness yog ib qho tseem ceeb, qhia nws raws li ib qho kev xav tau ntxiv ntawm kev yuav khoom.