347 Kub Rolled Stainless Hlau H Beams
Ntawv pov thawj: ISO, CE
Daim Duab: H Hom
Cov txheej txheem: Kub Rolled
Nto Kho: No.1, BA, 2B, 2D, No.4 lossis Accial
Qauv: Muaj
Kev Pab Cuam: Vuam, xuas nrig ntaus, txiav, khoov, decoiling
Lub sij hawm xa tuaj: 7-15 hnub
Daim Ntawv Thov: Kev Tsim Kho, Kev Lag Luam Automotive, Tsev neeg
Cov Lus Qhia Tshwj Xeeb: Raws li cov neeg yuav tsum tau ua
Khoom Piav Qhia
347 Kub Rolled Stainless Hlau H Beamsyog engineered rau cov kev kub-ib puag ncig uas cov qauv stainless hlau zoo li 304 lossis 316 yuav swb. Txawm hais tias koj ua ib tsob nroj petrochemical, rauv nyiaj txhawb nqa, lossis chaw nres tsheb fais fab 347 h-nqaj muaj koj cov tshuab hluav taws xob zoo.
Cov Qauv Txheej Txheem:ASTM A276, A479
Cov qib siab sib npaug:UNRN UN34700, DIN 1.4550, Sus347

UNS UNL UNRT S34700 Cov Khoom Taw Qhia Baj Teeb
Dab tsi yog qhov txawv ntawm 316 thiab Astm 276 347 h nqaj?
Thaum 316 muaj kev tiv thaiv corrosion zoo heev, 347 ua yeeb yam zoo dua ntawm qhov kub thiab txias vim NiObium stabilization. Nws kuj tseem tiv thaiv weld lwj ntau dua nyob rau hauv cyclic tshav kub ib puag ncig.
Puas yog 347 stainless hlau h tws zoo rau vuam?
Yog lawm. Hom 347 yog qhia tshwj xeeb rau weldability thiab tiv taus intergranular corrosion tom qab vuam, tsis zoo li tsis muaj qib kawm.
Dab tsi yog qhov kev pab cuam siab tshaj plaws rau 347 stainless hect?
Kwv yees li 870 degree (1600 degree f) hauv kev pabcuam txuas ntxiv thiab nce mus txog 925 degree f) rau kev sib quas ntus.
347 stainless hlau h nqaj nqe ib kg?
Tus nqi ntawm 347 stainless hlau h-nqaj sib txawv raws li yam xws li loj npaum li cas, kom muaj nuj nqis, thiab khoom xa khoom. Tus nqi ntau yog kwv yees li $ 1.5 rau $ 4.5 rau ib phaus, uas yog sib npaug rau $ 1,500 rau $ 4,500 ib metric tuj.
347H Stainless Tus Qauv Kev Ncaj Ncees
Hom:Kub Rolled Stainless Hlau Qauv H Beooj
Daim Ntawv:H-BEWASE KHAU \/ NTIV FLEZE BEARE \/ I-PHAJ
Didensional (raug)
| Chaw ua uas tsis tau haus | Ntau Yam \/ Muaj |
|---|---|
| Web qhov siab (h) | 100 hli - 600 hli |
| Flarch Dav (B) | 100 hli - 300 hli |
| Web Thickness (Tw) | 5 hli - 20 hli |
| Flange Thickness (TF) | 7 hli - 25 hli |
| Qho ntev | 3 m - 12 m (kev cai txiav muaj) |
| Kev nyiaj tau | Raws li ANTM A484 \/ EN 10034 |
347 Cov Khoom Siv Hlau Stainless Cov Khoom Siv
| Ntiag tug | Tus nqi |
|---|---|
| Paib lub zog (0. 2%) | Ntau dua los yog sib npaug rau 205 MPa |
| Lub zog tensile | 515 - 750 MPa |
| Elongation (hauv 50 hli) | Ntau dua los yog sib npaug rau 35% |
| Kev nyuaj | Tsawg dua los yog sib npaug rau 217 hb (brinell) |
| Ceev | 7.96 g \/ cm³ |
Tshuaj lom neeg tshuaj ntsuab (% los ntawm qhov hnyav)
| Lub ntsiab | Cov ntsiab lus ntau |
|---|---|
| Carbon (c) | 0.04 – 0.10 |
| Chromium (cr) | 17.0 – 19.0 |
| Npib tsib caug (ni) | 9.0 – 13.0 |
| Manganese (mn) | Tsawg dua los yog sib npaug rau 2. 00 |
| Silicon (si) | Tsawg dua los yog sib npaug rau 1. 00 |
| Phosphorus (p) | Tsawg dua los yog sib npaug rau 0. 045 |
| Sulphur (s) | Tsawg dua los yog sib npaug rau 0. 030 |
| Niobium (NB + TA) | Ntau dua los yog sib npaug rau 1 0 × c (min 0.10%) |
Vim li cas thiaj xaiv GNEE
✅ Cov ntaub ntawv nruj me ntsis niaj zaus & MTC (en 10204 3. 1 \/ 3.2)
Kev cai txiav kev cai, kev sib tsoo, thiab cov kev pab kho kom zoo
In International xa nrog cov seasworthy ntim
Cov Sij Hawm Coj Cov Ntev Npaum Cov Sij Hawm Sib Tw
Tau txais cov lus hais hnub no
Xav tau txhim khu kev qha 347 Kub Rolled Stainless Hlau H Be tws rau koj txoj haujlwm siab tshaj plaws? Hu rau GNEE rau kev tsocai sai, kev ua haujlwm, thiab cov kws txhawb nqa kev txhawb nqa.
Qhov twg yuav 347 stainless hlau h tws

Stainless Hlau Hlawv Stockist

Gnee Cov Neeg Siv Khoom

Cim npe nrov: 347 Kub Rolled Stainless Hlau H Beams, Tuam Tshoj 347 Kub Rolled Stainless Hlau H Beams Cov Chaw Tsim Tshuaj, Chaw muag khoom, Hoobkas