ATM A 276 347 h polished stainless bar

ATM A 276 347 h polished stainless bar

Cov lus qhia tshwj xeeb: ASTM 276 347 h polished stainless bar
Qeb Kawm: 300 SERIES
Ntawv pov thawj: ISO, AISI, ASTM, GB, en, din, jis
Puab: Round
Cov txheej txheem: Rolled txias
Thickness: 2mm-300 hli
Dav: 1000mmm -2000 hli
Ntev: raws li koj qhov yuav tsum tau ua
Txoj kab uas hla tsis kam: H9, H11, H13, K9, K11, K13 thiab lwm yam
Qauv: Dawb Qauv
Nto: Tsis muaj, tev, polishing, ci, ci me me,
Pob Thauj: Ntoo Pob

Dab tsi yog ovm 276 347 h polished stainless bar?

 

347H Stainless Hlau Baryog cov roj carbon high roj carbon aus roj stainless hlau (raws li Astm A276 Txuj Ci, cov pa roj carbon monoxide ({} 0 {. 08%) . Lub ntsiab lus ntawm cov ntsiab lus ntawm "h":

 

 

Stainless hlau 347h polished round bar Tshuag

 

 Stainless Steel 347H Polished Round Bar Stock

Qhov Zoo ntawm 347H Stainless Hlau Polishing Bar

 

Cov khoom tawg ntawm 347h txias kos cov bar tuaj yeem ncav cuag ra tsawg dua los yog cov khoom siv impurity, thiab cov khoom siv tshuaj ntsuab)} nquag rau corrosion pib cov ntsiab lus).

Muaj feem cuam tshuam cov xwm txheej:
Precision Soj Ntsuam: Kev Ntsuas Cov Kab Mob, Ntsuas Cheebtsam Cheebtsam
Kev Kho Mob / Khoom Noj: Sterile Kav, phais cov twj
Cov Khoom Siv High-aus: Aerospace Fasteners

 

Vim li cas thiaj xaiv peb 347h polishing pas nrig?

Cov khoom lag luam ncaj qha los ntawm cov ntaub ntawv chaw tsim khoom: 18 xyoo ntawm stainless hlau bar tsim, txhawb nqa tag nrho}}}}}}
SOFT SOFT Kev Tshawb Nrhiav Kev Tshawb Xyuas Kev Nyeem Ntawv thiab Tensile Kuaj Tshuab, Daim Ntawv Tshaj Qhia Tiav Tshaj Tawm tuaj yeem muab tso rau hauv 48 teev
✅ Kev xaiv nto kev kho mob: Ntxiv rau cov kev kho sab saum toj: Ra tsawg dua lossis sib npaug nrog 0.8μm), kev tiv thaiv xeb thiab lwm yam kev xaiv tau muab
✅ Muab cov khoom lag luam sib txuas: 500 tons ntawm cov khoom ua tau muaj, xa tawm tsis pub dhau 3 hnub, export txhawb nqa cov khoom lag luam thiab kev lis kev cai tshaj tawm ib qho kev pabcuam ib zaug

 

 

Hu rau tam sim no

347h stainless hlau tuav specification:

ATM A 276 347 h ss puag ncig cov kabTshuaj lom neeg tshuaj lom neeg (Astm A276 Txuj Ci)

Lub ntsiab Cov ntsiab lus ntau (%)
C 0.04–0.10
Cr 17.0–19.0
Ni 9.0–12.0
Nb Ntau dua los yog sib npaug rau 10 × c
Mn / Si Tsawg dua los yog sib npaug rau 2.0 / tsawg dua lossis sib npaug rau 0.75

 347H puag ncig ci bar mecha yam ntxwv (chav sov)

Ntiag tug Tus nqi
Lub zog tensile Ntau dua los yog sib npaug rau 515 MPa
Paib lub zog Ntau dua los yog sib npaug rau 205 MPa
Elongation Ntau dua los yog sib npaug rau 40%
Kev nyuaj Tsawg dua los yog sib npaug rau 217 hb

Ss 347h puag ncig cov khoom xa khoom

product-800-600

Gnee ntim thiab xa khoom

347 Stainless Steel Bright Rod Round Bar

Cov qhua tuaj noj mov

Customer Visit 

Cim npe nrov: ASTM A 276 347 h polished stainless bar, Tuam Tshoj276 347 h polished stainless bar manortic, lwm tus neeg, Hoobkas

Xa kev nug