ASTM A240 Hom 410 Stainless Hlau Hlau Phaj
Daim ntawv pov thawj: ISO, RoHS, IBR
Kev kho deg: 2b, Ba, No.1, No.4, Hl, 8K, thiab lwm yam.
Txheej txheem: kub dov, txias dov
Thickness: 0.1mm-300mm los yog raws li xav tau
Dav: 3mm-2000mm los yog raws li xav tau
Lub sij hawm xa tuaj: 7-15 hnub
Kev Them Nyiaj: FOB / CIF / CFR
Kev thauj mus los ntim: cov ntawv tsis muaj dej tsis zoo thiab cov khoom siv steel.
Specifications: customized
PIB: 721921000
Peev xwm: 8000 tons / xyoo
410 Stainless Hlau Phaj Chaw tsim tshuaj paus, SS 410 Daim Ntawv Nqe
GNEE yog tus kws tshaj lij thiab cov chaw tsim khoom ntawm 410 thiab 410S stainless hlau daim hlau, xa tawm 5000 tons ntawm stainless hlau daim hlau txhua xyoo. Peb muab tag nrho cov lus qhia tshwj xeeb hauv Tshuag, kev hloov kho meej, thiab kev txhawb nqa kev tshaj lij, ua kom koj cov haujlwm ua haujlwm tau zoo nyob rau hauv siab - kub, corrosive, lossis dynamic ib puag ncig.
Lub 410 stainless hlau peb muab yog martensitic, featuring siab zog, kub tsis kam, thiab corrosion kuj, tsim rau hnyav tej yam kev mob. Nws tuaj yeem tswj kev ruaj ntseg ntawm qhov kub thiab txias mus txog 1500℃F (kwv yees li 815 degree). Los ntawm kev kho cua sov xws li hardening, tempering, thiab quenching, peb txhim kho hardness thiab tag nrho kev ua tau zoo. 410S stainless hlau phaj, tsom rau siab - daim ntawv thov kub, nyob ruaj khov thiab tiv taus kev puas tsuaj nyob rau lub sijhawm ntev - qhov kub thiab txias ib puag ncig.
Ob leeg 410 thiab 410S kub- dov stainless hlau daim hlau ua tau raws li ASTM, API, thiab ASME cov qauv, nrog cov tuab ntawm 4.0 txog 100 hli. Lub hardness tuaj yeem xaiv los ntawm cov tawv, mos, quarter- nyuaj, lossis caij nplooj ntoos hlav- xaiv nyuaj. Nto tiav suav nrog 2B / HR, thiab peb muab qhov ntau thiab tsawg los ua kom tau raws li cov kev xav tau tshwj xeeb ntawm kev lag luam xws li tshuaj lom neeg, petrochemicals, khoom siv kho cua sov, boilers, tshav kub exchangers, thiab siab -kub yam ntxwv Cheebtsam.

Tiv tauj peb tam sim no rau cov ncauj lus kom ntxaws, kev ua haujlwm tsis zoo, thiab tus nqi!
Specification
Kev qhia tshwj xeeb: ASTM A240 / ASME SA240
Txuj: ASTM, ASME thiab API
Thickness: 4.0mm-100mm
Loj: 1000 hli x 2000 hli, 1220 hli x 2440 hli, 1500 hli x 3000 hli, 2000 hli x 2000 hli, 2000 hli x 4000 hli
Tiav: Kub dov phaj (HR), Cold dov phaj (CR), 2B, 2D, BA NO (8), SATIN (Met with Plastic Coated)
Hardness: Mos, Hard, Ib nrab Hard, Quarter Hard, Spring Hard thiab lwm yam.
Chemical Properties Ntawm 410 Stainless Steel Sheet
| SS | Si | C | Mn | P | Cr | S | Mo | Ni | N |
| TIAB SA 410 | 1.0 max | .15 max | 1.0 max | 040 max | 11.5 – 13.5 | 030 max | – | 0.50 max | – |
SS 410 Sheets Mechanical Properties
| SS | Yield zog 0.2% offset ksi (MPa) Yam tsawg kawg nkaus |
Tensile zog ksi (MPa) Yam tsawg kawg nkaus |
Elongation (% hauv 50mm) Yam tsawg kawg nkaus |
Hardness (Brinell) Qhov siab tshaj plaws |
Hardness (Rockwell B) Qhov siab tshaj plaws |
| Qib 410 | 30 (205) | 65 (450) | 20 | 217 | 96 |
AISI 410 Stainless Hlau Sheet Nqe
| Product Description | Loj (mm) | Nqe (USD) |
|---|---|---|
| Stainless hlau xovxwm phaj, AISI 410 | 2460 x 1250 x 3 | $400.96 |
| Stainless Hlau Phaj - Qib 410 (Cold Rolled) | 0.040 hli x 36 hli x 120 hli | $577.93 |
Yog tias koj txaus siab rau peb cov khoom thiab cov kev pabcuam, thov koj xav tiv tauj kuv txhua lub sijhawm, peb pab neeg yuav npaj muab kev txhawb nqa thiab kev pabcuam rau koj!
Nyem kom tau txais tus nqi sib tw tshaj plaws.
Stainless Hlau 410 Daim Ntawv Tus Nqi Ntxiv Kev Pabcuam / Kev Ua Haujlwm
Kev lees paub zoo: 100% PMI kuaj, kuaj xyuas qhov tsis zoo, thiab kuaj cov khoom siv tshuab. Advanced annealing thiab leveling cov cuab yeej ua kom zoo ib yam flatness thiab precision.


Stainless hlau 904L Sheet Manufacturers
Factory Peev Xwm: Ntau tshaj 50,000 square metres ntawm thaj chaw tsim khoom, nruab nrog CNC txiav, slitting, thiab polishing ntau lawm kab, nrog rau txhua xyoo export ntim ntau tshaj 30,000 tons, tag nrho raws li ISO 9001, SGS, thiab BV ntawv pov thawj.


GNEE packaging thiab Shipping
Ntim: Txhua daim ntawv lossis kauj yog qhwv hauv cov dej noo- cov ntawv pov thawj, kab nrog cov yas zaj duab xis, thiab ruaj nrog cov hlua hlau. Cov txheej txheej sab nrauv yog tiv thaiv los ntawm cov ntoo pallets lossis crates kom muaj kev nyab xeeb thaum caij tsheb thauj mus los thoob ntiaj teb.
Labeling: Txhua pob suav nrog tus lej ntawm lub cub tawg, qib, qhov ntev, thiab cov ntaub ntawv txheem.
Lub sij hawm xa tuaj: Feem ntau hauv 7-15 hnub ua haujlwm tom qab tau txais cov nyiaj them ua ntej.


Cim npe nrov: Tuam Tshoj astm a240 hom 410 stainless hlau hlau phaj manufacturers, lwm tus neeg, Hoobkas