304L stainless perforated sheet hlau

304L stainless perforated sheet hlau

Khoom npe: 304L stainless perforated sheet hlau
Nto Kho: Mekas
Qhov hnyav: Customization
Khoom siv: raws li koj qhov kev thov
Lub cev zoo: puag ncig, square, customized thiab lwm yam.
Kev Pab Cuam: khoov, vuam, txiav, xuas nrig ntaus
Hnub Xa Tawm: tsis pub dhau 7-14 hnub
Thickness: 0.1-12mm
Ntawv pov thawj: ISO9001
Qauv: Qauv Dawb
Pob Thauj: Pallet
Muaj Peev Xwm Ntau Lawm: 10000M / Lub Limtiam
Xa kev nug
Tsham tam sim no

SS 304L perforated nplooj ntawv xa khoom hauv Suav teb

 

Yog tias koj tab tom nrhiav rau lub stainless hlau perforated daim ntawv uas yog ntau yam kev tiv thaiv corrosion, 304l stainless hlau perforated hlau daim ntawv yuav yog koj thawj qhov kev xaiv. Gnee yog ib qho ntawm cov ua kom siab-} Zoo li qub 304L stainless hlau perforated shortr manufacturers. Cov ntawv tsis tseeb muaj cov ntawv muaj zog muaj zog, lub zog corrosion, durability, weldability thiab ntev kev pab cuam lub neej. Gnee txhawb kev tsim cov khoom siv tuab ntawm 0.5-10 hli thiab siab tshaj plaws ntawm 1220 × 2440mm, thiab tseem tuaj yeem kho tau raws li cov neeg siv khoom xav tau.

 

304l stainless perforated sheetated ntawv

 

Tsis yog 30403 ss perforated sheet screen zoo

Piv rau tus qauv 304, 304l stainless hlau perforated sheet hlauyog tsawg dua qub rau intergranular corrosion thiab ua yeeb yam ntseeg tau thiab muaj kuab acidic lossis alkaline ib puag ncig. Tom qab electrolytic polishing, nws cov npoo roughness tuaj yeem ncav cuag ra tsawg dua los yog sib luag rau cov ntxaij cov khoom siv mis nyuj hauv cov khoom noj muaj peev xwm ua kom muaj kev phom sij.

 

304l perforated stainless hlau panelsMuaj lub zog tensile ntawm ntau dua lossis sib npaug ntawm 485 MPa txiav, khoov, thiab muaj kev sib xyaw ua ke rau hauv cov kab ntau lawm rau kev ua. Nrog ib tug du, tsis {2} peem tob tob thiab muab cov khoom siv tu kom huv si, thiab lwm yam kev nyiam huv si, thiab lwm yam kev nyiam noj mov.

 

UNS 30403 SS Perforated Sheet Screen

Peb cov ntawv SS 304L nrog cov qhov muaj nyob nrog puag ncig, square, somiced lossis thaj chaw qhib tau tuaj yeem ua rau airflow, tso dej, pom kev lossis kev ua kom pom tseeb.

Hu rau tam sim no

Stainless hlau 304L perforated sheet specification

Txheem: Astm / ASME A240 / SA240

Qhov loj me: 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 hli x 24000 mm, 2000 mm x 2000 mm, 2000 mm

Thickness: 0.1mm txog 12 hli thk

Daim Ntawv: Kev Kho Kom Zoo Nkauj Round, Dimpled, Xwmfab Qhov, Kub iav Round Qhov, etched, cov xim sau qoob loo

Tiav: Kub Rolled phaj (HR), Khawb Cuav Txias (CR), 2D, 2D, Satin (Tau Nrog Cov Yas)

 

Tshuaj lom neeg muaj pes tsawg xyoo ntawm SS 304L kub dov perforated

Teem nqi C Mn Si P S Cr Ni N
304L 0.03max 2.0max 0.75max 0.45max 0.03max feeb: 18.0 max: 20.0 Min: 8.0 Max: 12.0 0.10 max

 

SS 304L Txias Yeem Cov Ntawv Sau Cov Khoom Siv Neeg Kho Tshuab

Teem nqi Tensile lub zog (mpa) min Yield zog 0.2% pov thawj (MPA) min Elongation (% hauv 50 hli) min
304L 485 170 40

 

SS 304L Perforated Sheet Nqe

Tus nqi ntawm SS 304L perforated phaj yog nyob ntawm cov tuab, qhov qauv thiab phaj loj. Rau qhov tseeb thiab kev sib tw tso tawm, hu rau tus neeg xa khoom uas ntseeg tau xws li GNEE stainless hlau ntawminfo@gneestainless.comNrog koj cov kev xav tau tshwj xeeb.

Hu rau tam sim no

Hu rau GNEE!

 

Gnee muaj 1,000 tons ntawm 304L substrate hauv Tshuag. Cov qauv qhov sib xyaw ua ke tuaj yeem raug kuaj tsis pub dhau 3 hnub, thiab cov xaj xaj tuaj yeem xa tau tsis pub dhau 15 hnub, uas yog 40% luv dua li kev lag luam nruab nrab. Gnee muab cov xim dawb qauv thiab pom zoo cov qauv kev ua haujlwm zoo ntawm cov neeg siv khoom noj khoom haus (xws li cov nqi ntawm cov neeg siv khoom noj), uas tuaj yeem txo ntau dua 30% ntawm kev saib xyuas tom ntej.

 

Ntxiv rau, peb tseem muab 304L perforated stainless hlau ntawv 4x8, uns und tsis s30403 polished cov ntawv sau ua ke, stainless hlau 304L dai kom zoo nkauj flodated

Hu rau tam sim no

ASTM A240 SS 304L Perforated Sheettsev tsim khoom

ss sheet with holes
steel perforated metal

Gnee ntim thiab xa khoom

perforated sheet ss
perforated sheet metal stainless

Cov qhua tuaj noj mov

stainless steel durbar plate

 

Cim npe nrov: 304L stainless perforated sheet hlau, Tuam Tshoj 304L stainless fulorated sheet hlau tuam ntxhab, lwm tus neeg, Hoobkas

Xa kev nug