Dab tsi yog 1.4401 2b Stainless Hlau Sheet?

Nov 27, 2025

Tso lus

1.4401 2B stainless hlau ntawv yog dab tsi?

1.4401 stainless hlau, tseem hu ua SUS316 / EN 1.4401, yog austenitic stainless hlau. Nws lub ntsiab alloy muaj pes tsawg leeg yog 16-18% chromium, 10-14% nickel, thiab 2-3% molybdenum. Nws tau txais kev kho 2B saum npoo, uas ua rau lub ntsej muag du, txias-dov, ci ntsa iab nrog lub ntsej muag roughness Ra tsawg dua lossis sib npaug li 0.5μm. Nws yog qhov tsim nyog rau kev lag luam thiab pom cov ntawv thov, suav nrog cov khoom siv tshuaj lom neeg, cov khoom siv ua zaub mov, cov khoom siv hauv hiav txwv, thiab cov khoom siv hluav taws xob.

 

Yog tias koj tab tom nrhiav rau 1.4401 2B stainless hlau ntawv, GNEE yog tus neeg muag khoom ntseeg siab. Peb muab cov ntawv zoo - cov ntawv zoo uas ua tau raws li cov qauv thoob ntiaj teb xws li ASTM A240, ASME SA240, thiab EN 10088-2. Peb cov nplooj ntawv muaj nyob rau hauv thickness ntawm 0.3 hli mus rau 8 hli thiab dav yog customizable, xws li 1000 hli, 1219 hli, thiab 1500 hli. Tag nrho cov nplooj ntawv muaj qhov zoo 2B tiav.

 

Peb muaj 316 cov ntawv kub-rolled, 316 txias-cov ntawv yob, 316 perforated nplooj ntawv, 316 polished nplooj ntawv, 316 welded nplooj ntawv, 316 seamless nplooj ntawv, 316 annealed nplooj, thiab 316 pickled nplooj ntawv. Peb muab cov kev cai ua kev xaiv xws li txiav, khoov, vuam, polishing, perforating, annealing, pickling, shearing, drilling, thiab laser txiav.

 

1.4401 2B stainless steel sheet,

 

1.4401 2B Stainless Hlau Sheet Specification

Yam khoom

Stainless hlau 316 phaj (kub dov, txias dov)

Specification

ASTM A240 / ASME SA240 / ASTM A240 / ASTM A240 / ASME SA240 / ASTM A240 / ASTM A240 / ASME SA240 / ASTM A240 / ASTM A240 / ASME SA240 / ASTM A240 / ASTM A240 / ASME SA240 / ASTM A240 / ASTM A240 / ASME SA240 / ASTM A240 / ASME SA240 / ASTM A240 / ASTM A240 / ASTM A240 / ASME SA240 / ASME SA240 / ASTM A240 / ASME SA240 / ASTM A240 / ASME SA240 / ASTM A240 / ASME SA240 / ASTM A240 / ASME SA240 / ASTM A240 / ASME SA240)

Txuj

EN10088-2-2005, ASTM A240, GB / T3280-2007, ASTM A167, JIS4304-2005 thiab lwm yam

Qib

ASTM A240 Qib 316
ASTM A240 Stainless Hlau 316 Phaj Ntev 2000mm txog 6000mm lossis kev cai ntev
SS UNS S31600 Phaj Dav 1000mm txog 3500mm los yog kev cai dav

Stainless hlau 316 Kub Rolled Phaj Thickness

0.01 ~ 200mm los yog kev cai thikness

Kub Rolled Ntawv Thickness

Qhov dav ntawm 3.0mm txog 20mm
Coils Thikness Ntau yam ntawm 0.3mm mus rau 10mm
Txias Rolled Sheets / Phaj Thickness Ntau yam ntawm 0.3mm mus rau 6mm
ASME SA240 Stainless hlau 316 phaj txheej txheem Kub / Cold Rolled

nto tiav

No.1, No. 2B, No.3,BA, No.6, No.4, No.7, 2D, 2B, Cov ntawv txias txias (CR), 1D, No.1 tag kub dov ASTM A240 Stainless hlau 316 Plate, No.4, 2B, 8K, BA,

Pob

Packed nyob rau hauv Standard export pob, Ntoo thawv los yog raws li ib tug neeg thov

Loj

40ft GP: 12032mm x 2352mm x 2393mm
  40ft HC: 12032mm x 2352mm x 2698mm

Tshwj xeeb

Lwm yam tshaj li qhov ntau thiab tsawg thiab Specifications tuaj yeem tsim los ntawm cov neeg thov

MTC

Mill Test Certificate, Muaj raws li EN 10204 3.1

 

 

SS 316 Plate Nyhav ib Chav


Qhov hnyav ntawm phaj ib kg

Loj hauv MM

Qhov hnyav ntawm phaj ib kg

Loj hauv MM

136.0

4000 x 2000 x 2.0

191.0

3000 x 1500 x 5.0

204.0

4000 x 2000 x 3.0

340.0

4000 x 2000 x 5.0

106.0

2500 x 1250 x 4.0

159.0

2500 x 1250 x 6.0

153.0

3000 x 1500 x 4.0

230.0

3000 x 1500 x 6.0

272.0

4000 x 2000 x 4.0

408.0

4000 x 2000 x 6.0

133.0

2500 x 1250 x 5.0

   

 

Qhov txawv ntawm 1.4401 2B thiab No.4 Finish Stainless Hlau Phaj yog dab tsi?

Qhov sib txawv tseem ceeb yog cov tsos: 1.4401 2B yog tus qauv, txias- dov tag nrog dull, me ntsis reflective grey nto, thaum Tsis yog . 4 yog ib tug mechanically polished, txhuam tiav nrog ib tug satin tsos thiab ib tug zoo, uniform, directional grain. 1.4401 yog hais txog cov austenitic stainless hlau khoom qib, thaum 2B thiab Tsis yog . 4 piav qhia txog qhov ua tiav ntawm qhov ua tiav rau nws.

 

Tsis tas li ntawd, peb muab ntau daim ntawv pov thawj, suav nrog ISO 9001, SGS, BV, thiab daim ntawv pov thawj ntawm lub Hoobkas (MTC 3.1), ua kom muaj kev ua raws li cov qauv thoob ntiaj teb. Cov neeg siv khoom tuaj yeem txaus siab rau cov qauv dawb, kev tiv thaiv corrosion zoo tshaj, zoo heev saum npoo, thiab kev siv dav hauv kev ua zaub mov, tshuaj, thiab kev tsim kho kev lag luam. GNEE 1.4401 2B daim ntawv yog qhov txhim khu kev qha, tus nqi- siv tau, thiab npaj tau-rau- siv cov tshuaj.

Hu rau tam sim no

1.4401 2B sheet