ASTM A312 TP904L Stainless hlau welded yeeb nkab

Feb 02, 2026

Tso lus

Yog tias koj tab tom nrhiav rau siab -kev ua tau zoo, corrosion- tiv taus welded stainless hlau kav rau kev thov tshuaj thiab kev siv tshuaj, peb tuaj yeem muab kev ntseeg siab ASTM A312 TP904L stainless hlau welded kav nrog kev xa khoom thoob ntiaj teb.


Peb ASTM A312 TP904L welded kav yog tsim los siv precision forming thiab tsis siv neeg TIG los yog SAW vuam txheej txheem, thiab undergo kev daws annealing, pickling, thiab passivation kev kho mob kom zoo zoo phab ntsa thickness, du nto, thiab siab qhov tseeb. TP904L welded kav feem ntau muaj lub zog tensile ntau dua los yog sib npaug ntawm 520 MPa thiab zoo heev elongation, sib txuas ua haujlwm ntev, corrosion kuj, thiab zoo weldability rau ntev - siv nyob rau hauv hnyav tshuaj ib puag ncig.


ASTM A312 TP904L stainless hlau kav kav dej yog dav siv nyob rau hauv tshuaj nroj tsuag, sulfuric acid khoom, tshav kub exchangers, seawater systems, thiab heev corrosive industrial piping networks.

 

ASTM A312 TP904L stainless steel welded pipe

🔹 Nyias Phab Ntsa AISI 904L Yeeb Nkab Specifications:

Qib TP 904 L
Specifications ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASTM A312 / ASME SA312)
Ntev Ib qho Random, Ob Chav Random, Txiav kom ntev
Xaus Screwed, Beveled, Threaded, Plain
Hom Welded|ERW|Seamless
Ntev 6 m los yog Customized
O.D. 1/2 "mus rau 18"
Teem caij Thickness SCH XS, SCH 40, SCH 80S, SCH 80, SCH XXS, SCH 160, SCH10, thiab lwm yam.
Kev Xa Khoom Annealed & Pickled, Polished, Bright & Annealed, thiab lwm yam.

 

🔹 Qib sib npaug:

STANDARD WERKSTOFF NR. UNS JIS KS BS AFNOR EN
TP 904 L 1.4539 N08904 SWB 904L TIAB SA 317J5L 904S13 Z2 NCUA 25-20 X1NiCrMoCu25-20-5

 

ASTM A312 TP904L Welded Yeeb Nkab Chemical Composition:

C Mn Si P S Cr Mo Ni Cu
0.02 max 2 max 1 max 0.04 max 0.03 max 19 – 23 4 – 5 23 – 28 1 – 2

 

🔹Cold Drawn SS 904L Pipe Mechanical Properties:

Qhov ntom Melting Point Tensile zog Yield zog (0.2% Offset) Elongation
7,95g 3 1350℃(2460℃F) Psi - 71000, MPa - 490 Psi - 32000, MPa - 220 35 %

 

🔹 Daim Ntawv Pom Zoo ntawm 904L Stainless Hlau Tube

Stainless hlau 904L yeeb nkab OD astm b677 tp 904l yeeb nkab kam rau ua
4 mus rau 35 millimeters +/- 0.08 milimeter mus
35-38 hli +/- 0.15 milimeter mus
38-60 hli +/- 0.20 milimeter mus
60 thiab siab dua +/- 0.25 milimeter mus

 

ASTM A312 TP 904L Seamless yeeb nkab thiab UNS N08904 Welded Tubes tsum

Rau qhov xav tau ceev, qhov zoo tshaj plaws yog qhov ntau thiab tsawg ntawm AISI 904L cov kav dej tau yooj yim muaj nyob hauv peb lub tsev khaws khoom suav. GNEE tuaj yeem muab cov ntaub ntawv sai sai rau Middle East thiab North African lub teb chaws, nrog tus nqi muag khoom muaj rau kev txiav txim ntau. Xav txog peb cov khoom xa tawm ntau tshaj 10 xyoo dhau los, GNEE yog ntawm kaum tus xa tawm sab saum toj ntawm SS 904L kav hauv Suav teb. Peb tsuas yog muab cov ntaub ntawv uas ua tau raws li EN 10204 Hom 3.1 MTC tus qauv.
Ntawm GNEE, cov neeg yuav khoom ntawm UNS S90400 cov kav dej tuaj yeem sib piv qhov ntau thiab tsawg, cov ntaub ntawv nplooj ntawv, thiab cov npe teev npe los ntawm cov ua lag luam Suav thiab European 904L stainless hlau yeeb nkab. Tau txais daim ntawv tsocai pub dawb hnub no!

 

 904L Stainless Steel Tube

Xa kev nug