ASTM A312 / A269 TP321 Pickled Thiab Annealed Stainless Hlau Seamless Yeeb Nkab

Nov 05, 2025

Tso lus

Yog tias koj tab tom nrhiav rau TP321 stainless hlau seamless yeeb nkab ua raws li ASTM A312 / A269 tus qauv, Gnee muaj siab -zoo pickled thiab annealed TP321 seamless yeeb nkab nrog zoo heev corrosion kuj thiab siab - kub stability. Tag nrho cov kav dej yog tsim los rau ASTM A312 thiab A269 cov qauv, kom ntseeg tau tias kev ua haujlwm zoo hauv kev siv tshuaj lom neeg, petrochemical, thiab cov khoom siv hluav taws xob.

 

ASTM A312 / A269 tus qauv TP321 stainless hlau seamless yeeb nkab yog dab tsi?

TP321 stainless hlau (UNS S32100 / EN 1.4541) yog titanium -stabilized austenitic stainless hlau. Qhov sib ntxiv ntawm titanium txhim kho nws cov kev tiv thaiv rau intergranular corrosion thiab txhim kho nws lub zog nyob rau hauv tas li siab - kub ua hauj lwm. Pickling thiab annealing kom huv si, du, thiab oxide-dawb yeeb nkab nto, ua rau nws haum rau huv si, siab -purity, thiab tshav kub exchange systems.

 

"Pickled thiab Annealed" txhais li cas?
"Pickled" yog hais txog kev kho cov kua qaub uas tshem tawm cov nplais oxide thiab impurities ntawm cov hlau nto. "Annealed" txhais tau hais tias cov yeeb nkab tau raug cua sov- kho los txhim kho nws cov khoom siv dag zog, ductility, thiab corrosion kuj.

TP321 Stainless Steel Seamless Pipe

 

ASTM A312 / A269 TP321 Pickled Thiab Annealed Seamless Yeeb Nkab hauv Tshuag

Khoom Specification
Txuj ASTM A312 / ASTM A269 Cov Lus Qhia
Qib TP321 (UNS S32100 / EN 1.4541)
Hom kev tsim khoom Seamless
Nto tiav Pickled & Annealed
Sab nraud Diameter (OD) 6mm-630 hli
Phab ntsa Thickness 0.5 hli-20mm
Ntev 5.8m, 6m, lossis kev cai
Tensile zog (MPa) 515 – 750
Yield zog (MPa) Ntau dua lossis sib npaug rau 205
Elongation (%) Ntau dua lossis sib npaug li 35
Hardness (HB) Tsawg dua lossis sib npaug li 217
Qhov ceev (g / cm³) 7.9
Max Service Kub (degree) 870℃nruam, 925℃intermittent
Hom kawg Plain, beveled, los yog threaded
Ntim Lub kaus mom yas + ntoo lub thawv / steel pallet

 

Dab tsi yog qhov txawv ntawm TP321 thiab TP304 stainless hlau?
TP321 muaj titanium, uas muab kev tiv thaiv zoo rau intergranular corrosion thiab siab kub zog tshaj TP304, tshwj xeeb tshaj yog nyob rau hauv welded los yog tsis tu ncua rhuab tej yam kev mob.

 

Puas yog TP321 haum rau thaj chaw marine lossis acidic?
TP321 ua tau zoo nyob rau hauv oxidizing thiab me me corrosive ib puag ncig. Rau cov dej qab ntsev ntau heev lossis chloride-nplua nuj tej yam kev mob, 316L lossis 316Ti yog qhov tsim nyog dua.

 

TP321 stainless hlau kav tau welded yooj yim?
Yog lawm, TP321 tuaj yeem welded siv TIG, MIG, lossis plasma vuam yam tsis muaj kev pheej hmoo ntawm carbide rhiab heev, ua tsaug rau titanium stabilization.

 

TP321 Stainless Hlau Seamless Yeeb Nkab Nqe ib kg
Tus nqi ntawm TP321 stainless hlau seamless yeeb nkab feem ntau yog li ntawm $ 6.50 txog $ 9.80 ib kilogram, nyob ntawm seb cov yeeb nkab txoj kab uas hla, phab ntsa thickness, kho deg, thiab keeb kwm. Piv txwv li, ib qho kev txiav txim ntau ntawm 2-inch SCH40 TP321 seamless yeeb nkab, tom qab annealing thiab pickling, nqi kwv yees li $7.20 ib kilogram. Polished los yog tuab-walled kav tej zaum yuav kim dua vim cov txheej txheem ntxiv thiab cov khoom siv ntau dua yuav tsum tau. Email:sales@gneestainless.com

 

Vim li cas thiaj xaiv Gnee rau TP321 Stainless hlau kav
Tshaj 18 xyoo ntawm stainless hlau export kev
Cov khoom lag luam loj ntawm ASTM A312 / A269 TP321 seamless kav
Kev cai txiav- mus rau-ntev, polishing, thiab kev pabcuam beveling
Cov ntawv pov thawj zoo: ISO 9001, SGS, BV, thiab MTC 3.1
Pab ntau tshaj 60 lub teb chaws thoob ntiaj teb
Muaj: Hauv Tshuag rau xa tam sim
MOQ: 1 tuj lossis ib qho kev txiav txim yuav tsum tau ua
Lub sij hawm xa tuaj: 7-15 hnub ua haujlwm
Cov ntsiab lus kev lag luam: EXW / FOB / CIF / CFR
Kev tshuaj xyuas: 100% kuaj nrog hydrostatic thiab eddy tam sim no kuaj
Daim ntawv pov thawj: EN 10204 3.1 / ISO / SGS / BV
Tag nrho cov kav TP321 muab los ntawm Gnee ua raws li ASTM A312 / ASME SA312 cov qauv thiab tau txais 100% qhov tseeb qhov tseeb, hydrostatic, thiab corrosion kev ua tau zoo los xyuas kom meej ruaj khov thiab txhim khu kev qha zoo thiab ua haujlwm ntev.