Tso lus
Raws li lub Ib Hlis Ntuj Tim 7, 2026, tus nqi ntawm qhov chaw txias - dov 409L stainless hlau los xij yog 7.35 RMB / kg (kwv yees li US $ 1.03 / kg). Tus nqi zoo rau kev txiav txim loj (tshaj 10 tons) thaj tsam ntawm 7.00-8.00 RMB / kg (kwv yees US $ 0.98-1.12 / kg), nrog rau cov nqi tshwj xeeb sib txawv nyob ntawm thickness (0.3-12 mm), dav (1000-2000 mm), nto tiav (2D / 2B / BA50), thiab AST400 (AST400).
409L Stainless hlau vs . 304: Tus nqi
409L stainless hlau muaj 30-40% tus nqi kom zoo dua piv rau 304 (tam sim no tus nqi ntawm 14.20 RMB / kg rau txias dov). Tus nqi yuav tsum nyob twj ywm hauv qhov nqaim ntawm 6.80-7.80 RMB / kg thaum lub quarter thib ib ntawm 2026, cuam tshuam los ntawm cov khoom siv xws li cov nqi raw khoom (chromium: US $ 8.5-9.0 / kg, titanium: US $ 35-38 / kg) thiab kev thov los ntawm kev lag luam tsheb (nws lub ntsiab daim ntawv thov 5, suav txog 6%).
Dab tsi yog409L Stainless Hlau Sheet?
409L stainless hlau yog ferritic qis -carbon stainless hlau nrog 10.5-11.5% chromium thiab Tsawg dua lossis sib npaug rau 0.03% carbon. Nws cov ntsiab lus carbon tsawg txo qis carbide nag lossis daus thaum lub vuam, ua rau nws zoo tagnrho rau cov tsheb siv hluav taws xob, kev lag luam ducting, thiab kev siv cov txheej txheem uas yuav tsum tau muaj kev tiv thaiv corrosion ntawm tus nqi - tus nqi zoo.
Cov yam ntxwv tseem ceeb:
Sib nqus ferritic qauv
Zoo weldability thiab formability
Nruab nrab corrosion kuj
Tus nqi -tshwj xeeb zoo rau 430 stainless hlau hauv qee daim ntawv thov.
409L Stainless Hlau Sheet Chemical Composition (%)
| Element | Cov ntsiab lus |
|---|---|
| Cov pa roj carbon (C) | Tsawg dua lossis sib npaug li 0.03 |
| Chromium (Cr) | 10.5 – 11.5 |
| Nickel (Ni) | Tsawg dua los yog sib npaug li 0.5 |
| Manganese (Mn) | Tsawg dua los yog sib npaug rau 1.0 |
| Silicon (Si) | Tsawg dua los yog sib npaug rau 1.0 |
| Phosphorus (P) | Tsawg dua los yog sib npaug li 0.04 |
| Sulfur (S) | Tsawg dua lossis sib npaug li 0.03 |
| Hlau (Fe) | Tshuav |
409L Stainless Hlau Mechanical Properties
| Khoom | Tus nqi |
|---|---|
| Tensile zog | 350-500 MPa |
| Yield zog | 205-275 MPa |
| Elongation | 20 – 30% |
| Hardness | Tsawg dua lossis sib npaug li 180 HB |
| Qhov ntom | 7.7-7.8g / cm3 |
Yuav ua li cas 409L piv nrog 430 stainless hlau nyob rau hauv corrosion kuj?
409L stainless hlau muaj kev tiv thaiv qis dua li 430 stainless hlau nyob rau hauv ib puag ncig, tab sis muab kev tiv thaiv txaus rau oxidation thiab me ntsis corrosion, ua rau nws tsim nyog rau kev siv tsheb tso tsheb.
Dab tsi thicknesses thiab dav muaj rau 409L ntawv?
409L stainless hlau nplooj ntawv feem ntau muaj nyob rau hauv thicknesses xws li 0.4 hli mus rau 6 hli thiab txheem dav txog li 1,500 hli, nrog rau kev cai ntau thiab tsawg muaj raws li thov.
409L stainless hlau ntawv puas tuaj yeem siv rau kev siv lub tshuab hluav taws xob?
Yog lawm, 409L stainless hlau los xij yog siv dav hauv cov tsheb siv hluav taws xob vim lawv qhov zoo siab -kub oxidation tsis kam, tus nqi- ua tau zoo, thiab muaj peev xwm tsim cov duab nyuaj.
Puas yog 409L stainless hlau sib nqus?
409L stainless hlau yog hlau nplaum vim nws yog ferritic stainless hlau, uas tso cai rau nws khaws cov khoom sib nqus txawm tias tom qab vuam lossis sib sau.
GNEE yog ib lub tuam txhab muaj kev lag luam tshwj xeeb hauv kev lag luam wholesale ntawm stainless hlau raw cov ntaub ntawv, kev sib koom ua lag luam, ua, warehousing, thiab kev thauj mus los. Peb cov khoom tseem ceeb muaj xws li 304L stainless hlau, 316L stainless hlau, 409L stainless hlau, thiab lwm yam stainless hlau daim hlau, coils, strips, thiab tiaj tus tuav. Peb khaws cov khoom lag luam tsis tu ncua ntawm ntau dua 1000 tons ntawm cov ntaub ntawv nrog ntau yam kev qhia tshwj xeeb thiab cov khoom siv txaus. Peb kuj muab ntau yam stainless hlau ua cov kev pabcuam raws li cov neeg siv khoom xav tau, suav nrog qib, slitting, hlau kos duab, daim iav polishing, roj sib tsoo, stamping, dabtsi yog khoov, ncaj, txiav, dov, thiab xuas nrig ntaus.

Cov khoom yog ntim rau hauv cov ntoo crates lossis ntawm pallets haum rau kev thauj khoom hiav txwv, nrog rau kev ntsuas los tiv thaiv ya raws, xeb, thiab ntug kev puas tsuaj. Cov xov tooj cua sov thiab qhov ntev yog qhia meej meej rau ntawm daim hlau. Peb lav kev xa khoom zoo: hauv - Tshuag alloy 409L daim hlau tuaj yeem xa tuaj tsis pub dhau 7-10 hnub, thiab qhov ntau thiab tsawg hauv 15-25 hnub.