Dab tsi yog qib 316L stainless hlau?

Feb 25, 2026

Tso lus

Stainless Steel Grade 310S - Super Heat Resistant GradeUNS N08904 / EN 1.4539 Stainless Steel Sheet Data SheetASTM B673 Stainless Steel 904L Seamless Pipe

 

Mechanical Properties

Rooj 2.Mechanical zog ntawm 316L stainless hlau.

 

QibTensile Str (MPa) minYield Str 0.2% Pov thawj (MPa) minNtev (% hauv 50 mm) minHardness
Rockwell B (HR B) maxBrinell (HB) max
316L4851704095217

 

Lub cev muaj zog

Table 3.Cov khoom siv lub cev zoo rau 316-qib stainless hlau.

 

QibQhov ceev (kg / m3)Elastic Modulus (GPa)Txhais tau tias Co-eff ntawm Thermal Expansion (µm/m/°C)Thermal conductivity (W / mK)Cov cua kub tshwj xeeb 0-100 ° C (J / kg.K)Elec Resistivity (nΩ)
0-100 ° C0-315 ° C0-538 ° CNtawm 100 ° CNtawm 500 ° C
316/L/H800019315.916.217.516.321.5500740

 

 